Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-3.377 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.023 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.24 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLaBO3 + La4B14O27 |
Band Gap4.537 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/c [15] |
Hall-C 2yc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LiF (mp-1138) | <1 1 0> | <0 0 1> | 277.4 |
GaSe (mp-1943) | <1 0 1> | <0 0 1> | 277.4 |
BN (mp-984) | <0 0 1> | <1 0 1> | 223.3 |
BN (mp-984) | <1 0 0> | <0 0 1> | 332.9 |
Al (mp-134) | <1 1 0> | <0 0 1> | 277.4 |
TeO2 (mp-2125) | <0 1 0> | <0 0 1> | 277.4 |
TeO2 (mp-2125) | <0 1 1> | <1 0 -1> | 297.8 |
TeO2 (mp-2125) | <1 0 0> | <0 0 1> | 277.4 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 221.9 |
SiC (mp-7631) | <1 0 1> | <0 0 1> | 277.4 |
MgO (mp-1265) | <1 1 0> | <0 0 1> | 332.9 |
TiO2 (mp-2657) | <0 0 1> | <0 0 1> | 277.4 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 55.5 |
TiO2 (mp-2657) | <1 0 1> | <1 0 0> | 179.8 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 221.9 |
TiO2 (mp-2657) | <1 1 1> | <0 0 1> | 332.9 |
GdScO3 (mp-5690) | <1 1 1> | <0 0 1> | 221.9 |
Mg (mp-153) | <1 1 1> | <0 0 1> | 277.4 |
LaF3 (mp-905) | <1 1 0> | <0 0 1> | 277.4 |
GaP (mp-2490) | <1 1 0> | <1 0 -1> | 297.8 |
PbSe (mp-2201) | <1 0 0> | <1 0 -1> | 198.5 |
BaTiO3 (mp-5986) | <1 0 1> | <0 0 1> | 277.4 |
NdGaO3 (mp-3196) | <0 1 0> | <1 0 -1> | 297.8 |
NdGaO3 (mp-3196) | <1 0 0> | <1 0 -1> | 297.8 |
SiC (mp-11714) | <0 0 1> | <0 0 1> | 221.9 |
SiC (mp-11714) | <1 0 0> | <0 0 1> | 332.9 |
Ga2O3 (mp-886) | <1 0 -1> | <0 0 1> | 111.0 |
LaAlO3 (mp-2920) | <1 0 0> | <1 0 -1> | 297.8 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 269.7 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 332.9 |
CeO2 (mp-20194) | <1 1 0> | <1 0 -1> | 297.8 |
BaF2 (mp-1029) | <1 0 0> | <1 0 -1> | 198.5 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 277.4 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 277.4 |
TePb (mp-19717) | <1 1 0> | <1 0 0> | 179.8 |
TePb (mp-19717) | <1 1 1> | <0 0 1> | 221.9 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 221.9 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 277.4 |
Si (mp-149) | <1 1 0> | <1 0 -1> | 297.8 |
Au (mp-81) | <1 1 0> | <0 0 1> | 221.9 |
Au (mp-81) | <1 1 1> | <0 0 1> | 332.9 |
ZrO2 (mp-2858) | <1 1 -1> | <0 0 1> | 221.9 |
ZrO2 (mp-2858) | <1 1 0> | <1 0 0> | 269.7 |
YAlO3 (mp-3792) | <0 1 1> | <0 0 1> | 332.9 |
YAlO3 (mp-3792) | <1 0 1> | <0 0 1> | 332.9 |
YAlO3 (mp-3792) | <1 1 1> | <1 0 0> | 179.8 |
CdWO4 (mp-19387) | <1 0 1> | <0 0 1> | 277.4 |
MgF2 (mp-1249) | <1 1 0> | <0 0 1> | 166.4 |
MgF2 (mp-1249) | <1 1 1> | <0 0 1> | 332.9 |
ZnO (mp-2133) | <1 0 1> | <0 0 1> | 221.9 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ho4(B2O5)3 (mp-17714) | 0.2667 | 0.038 | 3 |
Dy4(B2O5)3 (mp-18108) | 0.2558 | 0.020 | 3 |
Tm4(B2O5)3 (mp-772919) | 0.2993 | 0.021 | 3 |
Er4(B2O5)3 (mp-772497) | 0.2741 | 0.041 | 3 |
Bi4(B2O5)3 (mp-768923) | 0.2195 | 0.005 | 3 |
LiBiP2O7 (mp-759122) | 0.5974 | 0.083 | 4 |
KBiP2S7 (mp-23572) | 0.7417 | 0.000 | 4 |
VAgTeO5 (mp-645743) | 0.6966 | 0.013 | 4 |
ZnSn2(PO4)2 (mvc-9630) | 0.7243 | 0.071 | 4 |
KVTeO5 (mp-19699) | 0.7018 | 0.000 | 4 |
TlZnSClO4 (mp-23146) | 0.7475 | 0.000 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: La B O |
Final Energy/Atom-8.3172 eV |
Corrected Energy-436.9308 eV
-436.9308 eV = -415.8621 eV (uncorrected energy) - 21.0687 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)