Final Magnetic Moment0.010 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.709 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.030 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.09 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToSrI2 + BaI2 |
Band Gap3.435 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/c [14] |
Hall-P 2ybc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
GaN (mp-804) | <1 0 1> | <0 0 1> | 281.6 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 211.2 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 211.2 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 140.8 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 281.6 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 140.8 |
Te2W (mp-22693) | <0 1 1> | <0 0 1> | 281.6 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 281.6 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 140.8 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 281.6 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 70.4 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 281.6 |
Al (mp-134) | <1 0 0> | <0 0 1> | 281.6 |
LiGaO2 (mp-5854) | <0 1 1> | <0 0 1> | 211.2 |
TeO2 (mp-2125) | <0 0 1> | <0 0 1> | 281.6 |
Fe3O4 (mp-19306) | <1 1 0> | <0 0 1> | 211.2 |
GdScO3 (mp-5690) | <0 0 1> | <0 0 1> | 281.6 |
Mg (mp-153) | <1 0 0> | <0 0 1> | 281.6 |
Mg (mp-153) | <1 1 1> | <0 0 1> | 281.6 |
TiO2 (mp-2657) | <0 0 1> | <0 0 1> | 281.6 |
PbS (mp-21276) | <1 0 0> | <0 0 1> | 70.4 |
TbScO3 (mp-31119) | <0 0 1> | <0 0 1> | 281.6 |
Ni (mp-23) | <1 1 1> | <0 0 1> | 211.2 |
Mg (mp-153) | <1 1 0> | <0 0 1> | 140.8 |
GaP (mp-2490) | <1 0 0> | <0 0 1> | 281.6 |
InP (mp-20351) | <1 0 0> | <0 0 1> | 70.4 |
C (mp-48) | <0 0 1> | <0 0 1> | 211.2 |
C (mp-48) | <1 0 0> | <0 0 1> | 211.2 |
NdGaO3 (mp-3196) | <0 0 1> | <0 0 1> | 281.6 |
NaCl (mp-22862) | <1 1 0> | <0 0 1> | 140.8 |
Au (mp-81) | <1 0 0> | <0 0 1> | 70.4 |
ZrO2 (mp-2858) | <1 0 0> | <0 0 1> | 140.8 |
ZrO2 (mp-2858) | <1 1 0> | <0 0 1> | 281.6 |
MgF2 (mp-1249) | <0 0 1> | <0 0 1> | 281.6 |
ZnO (mp-2133) | <0 0 1> | <0 0 1> | 140.8 |
YAlO3 (mp-3792) | <0 0 1> | <0 0 1> | 140.8 |
YAlO3 (mp-3792) | <1 1 0> | <0 0 1> | 281.6 |
ZnO (mp-2133) | <1 1 1> | <0 0 1> | 281.6 |
MgAl2O4 (mp-3536) | <1 1 0> | <0 0 1> | 281.6 |
Ge (mp-32) | <1 1 0> | <0 0 1> | 140.8 |
LiAlO2 (mp-3427) | <1 1 1> | <0 0 1> | 281.6 |
ZnTe (mp-2176) | <1 1 0> | <0 0 1> | 211.2 |
SrTiO3 (mp-4651) | <0 0 1> | <0 0 1> | 281.6 |
LiAlO2 (mp-3427) | <1 0 1> | <0 0 1> | 211.2 |
Al2O3 (mp-1143) | <1 1 0> | <0 0 1> | 211.2 |
CaF2 (mp-2741) | <1 0 0> | <0 0 1> | 281.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
LiVF4 (mp-779190) | 0.4634 | 0.054 | 3 |
Zr4MnO9 (mp-763464) | 0.4514 | 0.041 | 3 |
Ba2CaI6 (mp-766343) | 0.4651 | 0.038 | 3 |
NaGdCl4 (mp-28156) | 0.5002 | 0.000 | 3 |
Ba2SrI6 (mp-772878) | 0.3312 | 0.017 | 3 |
Li8Ni(O2F)2 (mp-861293) | 0.7318 | 0.112 | 4 |
Li3NbOF6 (mp-769384) | 0.7200 | 0.046 | 4 |
Li8Co(O2F)2 (mp-764104) | 0.7097 | 0.123 | 4 |
Li8Mn(O2F)2 (mp-763440) | 0.7336 | 0.067 | 4 |
Na3Li6Mn5O9 (mp-765723) | 0.6769 | 0.089 | 4 |
HfO2 (mp-352) | 0.6081 | 0.000 | 2 |
SnO2 (mp-560417) | 0.5824 | 0.134 | 2 |
K2O (mp-776016) | 0.6222 | 0.020 | 2 |
HfO2 (mp-1858) | 0.6074 | 0.024 | 2 |
CeSe2 (mp-1080301) | 0.5617 | 0.045 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ba_sv Sr_sv I |
Final Energy/Atom-3.3133 eV |
Corrected Energy-119.2780 eV
-119.2780 eV = -119.2780 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)