Final Magnetic Moment0.208 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-1.530 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.078 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.60 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi(CoO2)2 + LiCuO2 + LiCoO2 |
Band Gap0.079 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/m [12] |
Hall-C 2y |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <0 0 1> | 126.0 |
AlN (mp-661) | <1 0 1> | <0 1 0> | 244.7 |
CeO2 (mp-20194) | <1 0 0> | <0 1 0> | 244.7 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 294.1 |
LaAlO3 (mp-2920) | <0 0 1> | <0 1 1> | 322.5 |
AlN (mp-661) | <0 0 1> | <0 1 0> | 195.8 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 210.1 |
GaAs (mp-2534) | <1 1 1> | <0 1 0> | 293.7 |
BaF2 (mp-1029) | <1 0 0> | <1 1 0> | 195.3 |
GaN (mp-804) | <1 1 0> | <1 0 1> | 284.9 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 210.1 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 84.0 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 210.1 |
SiO2 (mp-6930) | <1 1 0> | <1 0 1> | 95.0 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 210.1 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 0> | 253.5 |
DyScO3 (mp-31120) | <1 0 0> | <0 1 1> | 322.5 |
InAs (mp-20305) | <1 0 0> | <1 1 0> | 195.3 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 126.0 |
ZnSe (mp-1190) | <1 1 1> | <0 1 0> | 293.7 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 336.1 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 84.0 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 126.0 |
CdS (mp-672) | <1 0 0> | <1 0 1> | 284.9 |
YVO4 (mp-19133) | <1 0 1> | <1 1 0> | 293.0 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 336.1 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 210.1 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 294.1 |
Ag (mp-124) | <1 1 1> | <1 1 0> | 293.0 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 1 1> | 322.5 |
BN (mp-984) | <0 0 1> | <1 1 1> | 213.7 |
MoS2 (mp-1434) | <0 0 1> | <0 1 0> | 244.7 |
MoS2 (mp-1434) | <1 0 1> | <1 1 1> | 213.7 |
Al (mp-134) | <1 1 1> | <0 0 1> | 84.0 |
LiGaO2 (mp-5854) | <0 0 1> | <1 0 1> | 284.9 |
LiGaO2 (mp-5854) | <0 1 1> | <1 0 0> | 84.5 |
LiGaO2 (mp-5854) | <1 0 0> | <1 0 1> | 284.9 |
LiGaO2 (mp-5854) | <1 1 1> | <0 1 0> | 342.6 |
Fe3O4 (mp-19306) | <1 0 0> | <1 0 1> | 284.9 |
TiO2 (mp-2657) | <1 0 0> | <0 1 1> | 258.0 |
TiO2 (mp-2657) | <1 0 1> | <0 1 0> | 293.7 |
TiO2 (mp-2657) | <1 1 1> | <0 1 0> | 342.6 |
C (mp-66) | <1 0 0> | <0 0 1> | 126.0 |
GdScO3 (mp-5690) | <0 1 1> | <0 0 1> | 168.1 |
GdScO3 (mp-5690) | <1 0 1> | <0 0 1> | 168.1 |
GdScO3 (mp-5690) | <1 1 0> | <0 1 0> | 244.7 |
GdScO3 (mp-5690) | <1 1 1> | <0 0 1> | 294.1 |
Mg (mp-153) | <0 0 1> | <0 1 0> | 244.7 |
Mg (mp-153) | <1 1 0> | <1 0 1> | 284.9 |
Mg (mp-153) | <1 1 1> | <0 0 1> | 210.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li2Cr3O6 (mp-771534) | 0.2283 | 0.098 | 3 |
Li5Fe5O12 (mp-771687) | 0.2918 | 0.095 | 3 |
Li2Mn3O6 (mp-773276) | 0.3303 | 0.098 | 3 |
Li2(NiO2)3 (mp-773252) | 0.2200 | 0.062 | 3 |
TlIn5S7 (mp-562480) | 0.5233 | 0.000 | 3 |
Li4TiCo5O12 (mp-771514) | 0.1419 | 0.062 | 4 |
Li4CrCo5O12 (mp-771505) | 0.0732 | 0.066 | 4 |
Li2Cr(CoO3)2 (mp-761651) | 0.1274 | 0.078 | 4 |
Li2Fe(CoO3)2 (mp-761650) | 0.1452 | 0.081 | 4 |
Li4FeCo5O12 (mp-771206) | 0.0812 | 0.074 | 4 |
In6Se7 (mp-567596) | 0.5790 | 0.042 | 2 |
In6S7 (mp-555853) | 0.5281 | 0.008 | 2 |
Li4Ti4MnCr4O18 (mp-769442) | 0.6451 | 0.092 | 5 |
Li4Ti4V4CoO18 (mp-769478) | 0.6789 | 0.092 | 5 |
Li4Ti4Mn(Fe2O9)2 (mp-769443) | 0.6736 | 0.087 | 5 |
Li4Ti2V3Cr4O18 (mp-775447) | 0.6795 | 0.084 | 5 |
Li4Ti4VCr4O18 (mp-775391) | 0.6761 | 0.085 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesCo: 3.32 eV |
PseudopotentialsVASP PAW: Li_sv Co Cu_pv O |
Final Energy/Atom-5.5683 eV |
Corrected Energy-140.3011 eV
-140.3011 eV = -122.5036 eV (uncorrected energy) - 9.3700 eV (MP Advanced Correction) - 8.4275 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)