Final Magnetic Moment4.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.128 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.051 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.53 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCO2 + Na2SO4 + Cr2O3 + C |
Band Gap2.378 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/m [11] |
Hall-P 2yb |
Point Group2/m |
Crystal Systemmonoclinic |
sign indicates spin ↑ ↓
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <1 0 1> | 296.8 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 336.3 |
GaAs (mp-2534) | <1 1 1> | <1 0 1> | 296.8 |
BaF2 (mp-1029) | <1 0 0> | <1 1 0> | 79.1 |
BaF2 (mp-1029) | <1 1 0> | <0 1 0> | 281.4 |
BaF2 (mp-1029) | <1 1 1> | <0 1 0> | 140.7 |
AlN (mp-661) | <1 0 0> | <1 1 1> | 263.4 |
AlN (mp-661) | <1 0 1> | <0 1 1> | 179.9 |
AlN (mp-661) | <1 1 1> | <1 0 1> | 222.6 |
GaN (mp-804) | <0 0 1> | <0 1 1> | 179.9 |
GaN (mp-804) | <1 1 0> | <0 1 1> | 60.0 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 254.6 |
SiO2 (mp-6930) | <1 1 0> | <1 1 0> | 237.2 |
GaN (mp-804) | <1 0 0> | <0 1 1> | 119.9 |
GaN (mp-804) | <1 0 1> | <0 1 0> | 328.3 |
SiO2 (mp-6930) | <1 0 1> | <1 0 0> | 254.6 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 261.6 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 336.3 |
InAs (mp-20305) | <1 1 0> | <0 1 0> | 281.4 |
KCl (mp-23193) | <1 0 0> | <1 1 0> | 79.1 |
KCl (mp-23193) | <1 1 0> | <0 1 0> | 234.5 |
KCl (mp-23193) | <1 1 1> | <0 1 0> | 140.7 |
DyScO3 (mp-31120) | <1 0 0> | <0 1 1> | 179.9 |
DyScO3 (mp-31120) | <1 1 0> | <1 1 0> | 316.3 |
InAs (mp-20305) | <1 0 0> | <1 1 0> | 79.1 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 336.3 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 336.3 |
ZnSe (mp-1190) | <1 1 1> | <1 0 1> | 296.8 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 261.6 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 1> | 179.9 |
CdS (mp-672) | <1 1 0> | <1 0 1> | 148.4 |
CdS (mp-672) | <1 1 1> | <1 0 0> | 254.6 |
LiF (mp-1138) | <1 0 0> | <0 1 0> | 328.3 |
Te2W (mp-22693) | <0 0 1> | <1 0 1> | 222.6 |
Te2W (mp-22693) | <1 1 0> | <0 0 1> | 112.1 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 254.6 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 112.1 |
Te2W (mp-22693) | <0 1 1> | <0 0 1> | 299.0 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 186.8 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 261.6 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 112.1 |
Te2Mo (mp-602) | <1 0 1> | <1 0 1> | 222.6 |
Ag (mp-124) | <1 0 0> | <1 1 0> | 158.1 |
Ag (mp-124) | <1 1 0> | <1 0 1> | 74.2 |
GaSe (mp-1943) | <0 0 1> | <0 1 1> | 299.9 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 1 0> | 140.7 |
BN (mp-984) | <0 0 1> | <0 1 0> | 140.7 |
BN (mp-984) | <1 0 1> | <0 0 1> | 261.6 |
BN (mp-984) | <1 1 1> | <0 1 0> | 140.7 |
BN (mp-984) | <1 0 0> | <0 1 0> | 234.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li3Fe(BO2)5 (mp-761304) | 0.6797 | 0.048 | 4 |
Li3V(BO2)5 (mp-770344) | 0.6862 | 0.061 | 4 |
Na3Ca(BO2)5 (mp-542719) | 0.6749 | 0.000 | 4 |
Li3Ni(BO2)5 (mp-771081) | 0.6746 | 0.062 | 4 |
MnZnPO5 (mvc-3247) | 0.6451 | 0.051 | 4 |
Na2LuPCO7 (mp-767562) | 0.2963 | 0.016 | 5 |
Na2FeCSO7 (mp-771482) | 0.2883 | 0.020 | 5 |
Na2InPCO7 (mp-767521) | 0.2771 | 0.000 | 5 |
Na2CoCSO7 (mp-773380) | 0.2347 | 0.037 | 5 |
Li2TiPCO7 (mp-25400) | 0.3006 | 0.131 | 5 |
Li12Mn3VP4(CO7)4 (mp-767666) | 0.5941 | 0.060 | 6 |
Na2LiMnPCO7 (mp-764273) | 0.5030 | 0.026 | 6 |
NaLi2CoPCO7 (mp-764251) | 0.6022 | 0.028 | 6 |
NaLiMnPCO7 (mp-763833) | 0.4873 | 0.001 | 6 |
Na2LiFePCO7 (mp-773705) | 0.6030 | 0.021 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesCr: 3.7 eV |
PseudopotentialsVASP PAW: Na_pv Cr_pv C S O |
Final Energy/Atom-6.5086 eV |
Corrected Energy-171.3912 eV
-171.3912 eV = -156.2062 eV (uncorrected energy) - 11.1590 eV (MP Anion Correction) - 4.0260 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)