Final Magnetic Moment5.998 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.716 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.646 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density7.12 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToGd2W2O9 + WO3 |
Band Gap3.222 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/c [15] |
Hall-C 2yc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 272.5 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 134.2 |
GaAs (mp-2534) | <1 1 0> | <1 0 1> | 185.7 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 1> | 185.7 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 90.8 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 181.7 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 134.2 |
TePb (mp-19717) | <1 1 0> | <0 0 1> | 181.7 |
Te2Mo (mp-602) | <0 0 1> | <0 1 0> | 254.5 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 272.5 |
CeO2 (mp-20194) | <1 1 1> | <0 1 0> | 254.5 |
GaSe (mp-1943) | <0 0 1> | <0 1 0> | 254.5 |
BN (mp-984) | <0 0 1> | <1 1 0> | 158.7 |
Al (mp-134) | <1 1 0> | <1 0 1> | 185.7 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 134.2 |
ZnSe (mp-1190) | <1 1 0> | <1 0 1> | 185.7 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 1> | 185.7 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 1 0> | 84.8 |
GaSe (mp-1943) | <1 0 0> | <0 0 1> | 272.5 |
BN (mp-984) | <1 0 0> | <0 1 1> | 248.6 |
BN (mp-984) | <1 1 0> | <0 1 0> | 169.7 |
GdScO3 (mp-5690) | <1 0 0> | <0 0 1> | 90.8 |
CdTe (mp-406) | <1 1 0> | <1 0 1> | 185.7 |
TbScO3 (mp-31119) | <1 0 0> | <0 0 1> | 90.8 |
TbScO3 (mp-31119) | <1 1 0> | <0 0 1> | 181.7 |
InSb (mp-20012) | <1 1 0> | <1 0 1> | 185.7 |
BaTiO3 (mp-5986) | <0 0 1> | <0 1 0> | 254.5 |
NdGaO3 (mp-3196) | <1 1 0> | <0 0 1> | 181.7 |
Si (mp-149) | <1 1 1> | <0 1 0> | 254.5 |
C (mp-48) | <1 0 0> | <0 1 1> | 248.6 |
C (mp-48) | <1 1 0> | <0 1 0> | 169.7 |
BaTiO3 (mp-5986) | <1 0 1> | <1 0 1> | 185.7 |
NdGaO3 (mp-3196) | <1 1 1> | <0 0 1> | 272.5 |
SiC (mp-8062) | <1 1 0> | <0 1 1> | 248.6 |
CdWO4 (mp-19387) | <0 1 0> | <1 0 0> | 134.2 |
C (mp-48) | <1 0 1> | <1 1 0> | 158.7 |
CsI (mp-614603) | <1 0 0> | <0 0 1> | 181.7 |
MgF2 (mp-1249) | <1 0 0> | <0 0 1> | 272.5 |
MgF2 (mp-1249) | <1 1 0> | <1 0 1> | 185.7 |
NaCl (mp-22862) | <1 1 0> | <1 0 1> | 185.7 |
ZrO2 (mp-2858) | <0 0 1> | <0 0 1> | 272.5 |
MgAl2O4 (mp-3536) | <1 1 0> | <1 0 1> | 185.7 |
SrTiO3 (mp-4651) | <1 1 0> | <0 0 1> | 181.7 |
Ge (mp-32) | <1 1 0> | <1 0 1> | 185.7 |
ZnO (mp-2133) | <1 0 1> | <0 1 0> | 254.5 |
MgAl2O4 (mp-3536) | <1 0 0> | <1 0 0> | 134.2 |
SrTiO3 (mp-4651) | <1 1 1> | <0 0 1> | 272.5 |
Ge (mp-32) | <1 0 0> | <1 0 0> | 134.2 |
LiAlO2 (mp-3427) | <0 0 1> | <0 0 1> | 272.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Tb2(WO4)3 (mp-770351) | 0.0945 | 0.036 | 3 |
Er2(WO4)3 (mp-773513) | 0.1158 | 0.047 | 3 |
Sm2(WO4)3 (mp-773126) | 0.0328 | 0.024 | 3 |
Eu2(WO4)3 (mp-540684) | 0.0849 | 0.439 | 3 |
Ho2(WO4)3 (mp-772627) | 0.0906 | 0.043 | 3 |
EuMoO4F (mp-686947) | 0.6306 | 0.499 | 4 |
BiPPbO5 (mp-556878) | 0.6065 | 0.000 | 4 |
VBiPbO5 (mp-566459) | 0.6724 | 0.000 | 4 |
ErMoO4F (mp-565302) | 0.6789 | 0.000 | 4 |
HoMoO4F (mp-566496) | 0.6789 | 0.002 | 4 |
SrLaTl(AsO4)2 (mp-685195) | 0.7194 | 0.000 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesW: 6.2 eV |
PseudopotentialsVASP PAW: Gd W_pv O |
Final Energy/Atom-8.2645 eV |
Corrected Energy-324.1105 eV
Uncorrected energy = -280.9945 eV
Composition-based energy adjustment (-0.687 eV/atom x 24.0 atoms) = -16.4880 eV
Composition-based energy adjustment (-4.438 eV/atom x 6.0 atoms) = -26.6280 eV
Corrected energy = -324.1105 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)