Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-1.573 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.240 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.74 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToNa3Fe2(AsO4)3 + CO2 + Fe2O3 + O2 |
Band Gap0.099 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21 [4] |
HallP 2yb |
Point Group2 |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 252.5 |
LaAlO3 (mp-2920) | <1 1 1> | <0 1 0> | 252.1 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 252.5 |
LaAlO3 (mp-2920) | <1 0 0> | <0 0 1> | 72.1 |
LaAlO3 (mp-2920) | <1 0 1> | <1 0 0> | 312.4 |
LaAlO3 (mp-2920) | <1 1 0> | <1 0 0> | 125.0 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 108.2 |
AlN (mp-661) | <1 1 1> | <0 1 0> | 252.1 |
CeO2 (mp-20194) | <1 1 0> | <1 0 0> | 125.0 |
GaAs (mp-2534) | <1 1 0> | <1 0 0> | 187.5 |
AlN (mp-661) | <0 0 1> | <0 1 1> | 186.0 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 144.3 |
CeO2 (mp-20194) | <1 1 1> | <1 0 0> | 250.0 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 360.6 |
GaN (mp-804) | <0 0 1> | <1 1 1> | 89.2 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 288.5 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 180.3 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 108.2 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 216.4 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 -1> | 212.1 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 0> | 187.5 |
DyScO3 (mp-31120) | <1 1 0> | <0 1 0> | 302.5 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 324.6 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 144.3 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 216.4 |
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 108.2 |
CdS (mp-672) | <1 0 0> | <1 0 -1> | 141.4 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 216.4 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 144.3 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 360.6 |
ZnSe (mp-1190) | <1 1 0> | <1 0 0> | 187.5 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 0> | 302.5 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 187.5 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 250.0 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 187.5 |
Te2W (mp-22693) | <0 1 1> | <0 0 1> | 288.5 |
Te2W (mp-22693) | <0 0 1> | <0 1 0> | 151.3 |
Te2W (mp-22693) | <0 1 0> | <1 1 -1> | 260.5 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 180.3 |
TePb (mp-19717) | <1 1 0> | <1 0 0> | 62.5 |
Te2Mo (mp-602) | <0 0 1> | <0 1 1> | 186.0 |
Te2Mo (mp-602) | <1 0 0> | <1 1 -1> | 260.5 |
Te2Mo (mp-602) | <1 1 0> | <0 1 1> | 186.0 |
Ag (mp-124) | <1 0 0> | <0 1 0> | 302.5 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 1 1> | 186.0 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 180.3 |
BN (mp-984) | <0 0 1> | <0 1 0> | 201.7 |
BN (mp-984) | <1 1 0> | <0 1 1> | 310.0 |
BN (mp-984) | <1 0 0> | <1 1 -1> | 173.7 |
BN (mp-984) | <1 0 1> | <0 0 1> | 324.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Bi(BO2)3 (mp-23349) | 0.7014 | 0.001 | 3 |
Bi2B2O7 (mp-756526) | 0.6869 | 0.080 | 3 |
Bi(BO2)3 (mp-1079609) | 0.7184 | 0.006 | 3 |
Li2Mg11(WO4)12 (mp-853222) | 0.6705 | 0.120 | 4 |
Li3V(BO2)5 (mp-770344) | 0.6871 | 0.111 | 4 |
LiBiB2O5 (mp-768665) | 0.7113 | 0.091 | 4 |
Cr2B(PO4)3 (mp-565340) | 0.7010 | 0.124 | 4 |
MnZnPO5 (mvc-3247) | 0.6914 | 0.029 | 4 |
LiCePCO7 (mp-768198) | 0.3400 | 0.070 | 5 |
NaFePCO7 (mp-769633) | 0.2251 | 0.175 | 5 |
LiCuCSO7 (mp-768599) | 0.3287 | 0.060 | 5 |
NaBiAsCO7 (mp-768996) | 0.3307 | 0.070 | 5 |
NaCePCO7 (mp-767538) | 0.3649 | 0.029 | 5 |
KLiMnPCO7 (mp-764256) | 0.6258 | 0.000 | 6 |
NaLiMnPCO7 (mp-763833) | 0.5704 | 0.062 | 6 |
CdRe2H8C2(N2O5)2 (mp-733848) | 0.6545 | 0.016 | 6 |
KLi2MnPCO7 (mp-764310) | 0.7455 | 0.070 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesFe: 5.3 eV |
PseudopotentialsVASP PAW: Na_pv Fe_pv As C O |
Final Energy/Atom-6.1777 eV |
Corrected Energy-151.2080 eV
-151.2080 eV = -135.9099 eV (uncorrected energy) - 9.8321 eV (MP Anion Correction) - 5.4660 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)