Final Magnetic Moment4.002 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.348 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.103 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.52 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiBO2 + Li2B4O7 + LiO8 + Co3(BO3)2 |
Band Gap1.162 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/c [15] |
Hall-C 2yc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <0 1 0> | 170.6 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 100.2 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 213.0 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 -1> | 204.3 |
CdS (mp-672) | <1 1 1> | <1 1 0> | 263.2 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 213.0 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 200.4 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 106.5 |
YVO4 (mp-19133) | <1 1 0> | <1 0 0> | 200.4 |
YVO4 (mp-19133) | <1 1 1> | <0 1 0> | 85.3 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 213.0 |
Ag (mp-124) | <1 1 1> | <1 0 1> | 179.8 |
MoS2 (mp-1434) | <1 0 0> | <1 0 0> | 200.4 |
Al (mp-134) | <1 0 0> | <0 0 1> | 213.0 |
Al (mp-134) | <1 1 0> | <1 0 -1> | 204.3 |
CdTe (mp-406) | <1 0 0> | <0 0 1> | 213.0 |
MgO (mp-1265) | <1 0 0> | <0 1 0> | 255.9 |
TiO2 (mp-2657) | <0 0 1> | <0 0 1> | 106.5 |
C (mp-66) | <1 0 0> | <1 0 -1> | 102.1 |
Mg (mp-153) | <1 0 0> | <1 0 0> | 100.2 |
Mg (mp-153) | <0 0 1> | <1 0 0> | 200.4 |
LaF3 (mp-905) | <1 0 1> | <0 1 1> | 136.5 |
InSb (mp-20012) | <1 0 0> | <0 0 1> | 213.0 |
NdGaO3 (mp-3196) | <0 1 1> | <1 1 0> | 263.2 |
MoSe2 (mp-1634) | <1 0 1> | <0 1 0> | 255.9 |
Ga2O3 (mp-886) | <1 1 1> | <1 1 0> | 263.2 |
Ge(Bi3O5)4 (mp-23352) | <1 0 0> | <0 0 1> | 106.5 |
Au (mp-81) | <1 1 1> | <1 0 1> | 179.8 |
TiO2 (mp-390) | <1 0 1> | <1 0 0> | 200.4 |
Cu (mp-30) | <1 1 1> | <1 0 1> | 179.8 |
CaCO3 (mp-3953) | <1 0 0> | <1 0 1> | 179.8 |
ZnO (mp-2133) | <1 1 0> | <1 0 1> | 179.8 |
LiAlO2 (mp-3427) | <1 1 1> | <1 1 0> | 263.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
LiB3O5 (mp-1020025) | 0.7131 | 0.044 | 3 |
LiVB2O5 (mp-773200) | 0.1414 | 0.068 | 4 |
LiAlB2O5 (mp-557104) | 0.1952 | 0.001 | 4 |
LiBiB2O5 (mp-768665) | 0.4565 | 0.091 | 4 |
LiCuC2O5 (mp-757669) | 0.3537 | 0.117 | 4 |
LiFeB2O5 (mp-774231) | 0.0671 | 0.042 | 4 |
Li2SiSnCO7 (mp-770647) | 0.7053 | 0.084 | 5 |
Li2CrAsCO7 (mp-773176) | 0.6991 | 0.026 | 5 |
Li2VAsCO7 (mp-772603) | 0.7110 | 0.039 | 5 |
Li2MnPCO7 (mp-769717) | 0.6779 | 0.009 | 5 |
BaNaLi3(BO2)6 (mp-1019555) | 0.6814 | 0.000 | 5 |
NaLiMnPCO7 (mp-763833) | 0.6811 | 0.000 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesCo: 3.32 eV |
PseudopotentialsVASP PAW: Li_sv Co B O |
Final Energy/Atom-6.9851 eV |
Corrected Energy-273.0054 eV
-273.0054 eV = -251.4636 eV (uncorrected energy) - 14.0458 eV (MP Anion Correction) - 7.4960 eV (MP Advanced Correction)
|