Final Magnetic Moment29.030 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.085 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom1.290 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.60 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCr2FeO4 + Li4CrFe3O8 + Fe + FeO |
Band Gap0.971 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2 [5] |
HallC 2y |
Point Group2 |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 1> | <0 1 1> | 268.0 |
GaAs (mp-2534) | <1 0 0> | <0 1 0> | 342.1 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 320.8 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 137.5 |
GaN (mp-804) | <0 0 1> | <0 1 0> | 244.4 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 183.3 |
GaN (mp-804) | <1 0 1> | <0 1 1> | 134.0 |
SiO2 (mp-6930) | <0 0 1> | <0 1 0> | 195.5 |
KCl (mp-23193) | <1 1 0> | <1 0 0> | 176.0 |
DyScO3 (mp-31120) | <1 0 1> | <0 1 0> | 293.2 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 229.2 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 137.5 |
ZnSe (mp-1190) | <1 0 0> | <0 1 0> | 342.1 |
ZnSe (mp-1190) | <1 1 1> | <0 1 0> | 342.1 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 0> | 342.1 |
CdS (mp-672) | <0 0 1> | <0 1 0> | 244.4 |
CdS (mp-672) | <1 0 1> | <0 1 0> | 97.7 |
Te2W (mp-22693) | <0 0 1> | <0 1 0> | 244.4 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 275.0 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 275.0 |
Ag (mp-124) | <1 0 0> | <0 1 0> | 244.4 |
Ag (mp-124) | <1 1 0> | <0 1 1> | 268.0 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 137.5 |
LiNbO3 (mp-3731) | <1 1 1> | <1 0 0> | 264.1 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 1 0> | 244.4 |
Al (mp-134) | <1 0 0> | <0 0 1> | 320.8 |
Al (mp-134) | <1 1 0> | <0 1 0> | 342.1 |
Al (mp-134) | <1 1 1> | <0 1 0> | 146.6 |
AlN (mp-661) | <0 0 1> | <0 1 0> | 293.2 |
AlN (mp-661) | <1 0 0> | <0 1 0> | 244.4 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 137.5 |
AlN (mp-661) | <1 1 1> | <0 1 0> | 342.1 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 229.2 |
GaN (mp-804) | <1 1 0> | <0 1 1> | 201.0 |
GaN (mp-804) | <1 1 1> | <0 1 0> | 342.1 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 137.5 |
SiO2 (mp-6930) | <1 0 1> | <0 1 0> | 342.1 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 320.8 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 137.5 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 0> | 264.1 |
DyScO3 (mp-31120) | <1 1 1> | <1 0 1> | 213.5 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 229.2 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 320.8 |
KTaO3 (mp-3614) | <1 1 1> | <0 1 0> | 146.6 |
CdS (mp-672) | <1 0 0> | <0 1 0> | 342.1 |
CdS (mp-672) | <1 1 0> | <0 1 1> | 201.0 |
LiF (mp-1138) | <1 0 0> | <0 1 0> | 342.1 |
LiF (mp-1138) | <1 1 1> | <0 1 0> | 146.6 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 91.7 |
GaSe (mp-1943) | <0 0 1> | <0 1 0> | 244.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li5Fe7O12 (mp-771531) | 0.1028 | 0.025 | 3 |
Li5V7O12 (mp-764746) | 0.1181 | 0.369 | 3 |
Li5Fe11O16 (mp-762692) | 0.1192 | 0.043 | 3 |
Li5Fe11O16 (mp-768075) | 0.1080 | 0.020 | 3 |
Li3Fe5O8 (mp-586092) | 0.1238 | 0.484 | 3 |
Li4AlCr3O8 (mp-770091) | 0.1125 | 0.013 | 4 |
Li4Cr3NiO8 (mp-770046) | 0.1087 | 0.017 | 4 |
Li5Fe5(CoO6)2 (mp-850359) | 0.1140 | 0.093 | 4 |
Li4Cr3NiO8 (mp-769743) | 0.1109 | 0.017 | 4 |
Li5Fe5(SbO6)2 (mp-771103) | 0.1115 | 0.055 | 4 |
LiTe3 (mp-27466) | 0.2484 | 0.009 | 2 |
Bi2Te3 (mp-568390) | 0.3132 | 0.248 | 2 |
In2Se3 (mp-1068548) | 0.3076 | 0.530 | 2 |
In2Se3 (mp-20830) | 0.3012 | 0.530 | 2 |
Sb2Te3 (mp-1080789) | 0.2671 | 0.129 | 2 |
Na6MnNi3(SbO6)2 (mp-1094109) | 0.5067 | 0.139 | 5 |
Hg (mp-982872) | 0.4671 | 0.020 | 1 |
Sb (mp-632286) | 0.4302 | 0.059 | 1 |
Te (mp-570459) | 0.4679 | 0.044 | 1 |
Te (mp-10654) | 0.5003 | 0.047 | 1 |
Te (mp-105) | 0.3916 | 0.047 | 1 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesCr: 3.7 eVFe: 5.3 eV |
PseudopotentialsVASP PAW: Li_sv Cr_pv Fe_pv O |
Final Energy/Atom-6.4372 eV |
Corrected Energy-180.6124 eV
-180.6124 eV = -154.4939 eV (uncorrected energy) - 17.6910 eV (MP Advanced Correction) - 8.4275 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)