Final Magnetic Moment7.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.503 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.141 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.37 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCr2O3 + Al2O3 + Cr |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinFd3m [227] |
HallF 4d 2 3 1d |
Point Groupm3m |
Crystal Systemcubic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
GaN (mp-804) | <1 0 1> | <1 0 0> | 211.7 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 282.3 |
CeO2 (mp-20194) | <1 0 0> | <1 1 0> | 299.4 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 0> | 282.3 |
KTaO3 (mp-3614) | <1 0 0> | <1 1 1> | 244.5 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 70.6 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 282.3 |
Ag (mp-124) | <1 1 0> | <1 1 0> | 99.8 |
Ag (mp-124) | <1 1 1> | <1 1 1> | 122.2 |
LiNbO3 (mp-3731) | <1 0 0> | <1 1 0> | 299.4 |
Al (mp-134) | <1 0 0> | <1 1 1> | 244.5 |
LiGaO2 (mp-5854) | <0 1 1> | <1 0 0> | 211.7 |
LiGaO2 (mp-5854) | <1 0 1> | <1 0 0> | 141.1 |
TeO2 (mp-2125) | <0 0 1> | <1 0 0> | 282.3 |
Fe3O4 (mp-19306) | <1 1 0> | <1 1 0> | 99.8 |
Fe3O4 (mp-19306) | <1 0 0> | <1 0 0> | 70.6 |
Fe3O4 (mp-19306) | <1 1 1> | <1 1 1> | 122.2 |
C (mp-66) | <1 1 0> | <1 1 0> | 199.6 |
Mg (mp-153) | <1 0 1> | <1 0 0> | 211.7 |
TiO2 (mp-2657) | <0 0 1> | <1 0 0> | 282.3 |
Mg (mp-153) | <1 0 0> | <1 0 0> | 282.3 |
Mg (mp-153) | <1 1 1> | <1 0 0> | 282.3 |
PbS (mp-21276) | <1 0 0> | <1 0 0> | 70.6 |
PbS (mp-21276) | <1 1 0> | <1 1 0> | 99.8 |
GaP (mp-2490) | <1 0 0> | <1 0 0> | 282.3 |
InP (mp-20351) | <1 0 0> | <1 0 0> | 70.6 |
InP (mp-20351) | <1 1 0> | <1 1 0> | 99.8 |
TbScO3 (mp-31119) | <0 0 1> | <1 0 0> | 282.3 |
Ni (mp-23) | <1 1 0> | <1 1 0> | 299.4 |
BaTiO3 (mp-5986) | <1 0 0> | <1 1 0> | 99.8 |
Ni (mp-23) | <1 1 1> | <1 0 0> | 211.7 |
NdGaO3 (mp-3196) | <0 0 1> | <1 0 0> | 282.3 |
Au (mp-81) | <1 1 0> | <1 1 0> | 99.8 |
Au (mp-81) | <1 1 1> | <1 1 1> | 122.2 |
Ga2O3 (mp-886) | <1 1 0> | <1 1 0> | 299.4 |
Si (mp-149) | <1 0 0> | <1 1 0> | 299.4 |
Au (mp-81) | <1 0 0> | <1 0 0> | 70.6 |
C (mp-48) | <0 0 1> | <1 0 0> | 211.7 |
C (mp-48) | <1 0 0> | <1 0 0> | 211.7 |
NaCl (mp-22862) | <1 0 0> | <1 0 0> | 282.3 |
ZrO2 (mp-2858) | <0 0 1> | <1 0 0> | 141.1 |
ZrO2 (mp-2858) | <1 1 0> | <1 0 0> | 282.3 |
SiC (mp-8062) | <1 1 0> | <1 1 0> | 299.4 |
YAlO3 (mp-3792) | <1 1 0> | <1 0 0> | 282.3 |
CdWO4 (mp-19387) | <0 0 1> | <1 1 0> | 299.4 |
MgF2 (mp-1249) | <0 0 1> | <1 0 0> | 282.3 |
ZnO (mp-2133) | <0 0 1> | <1 1 1> | 122.2 |
MgAl2O4 (mp-3536) | <1 0 0> | <1 0 0> | 70.6 |
MgAl2O4 (mp-3536) | <1 1 0> | <1 1 0> | 99.8 |
SrTiO3 (mp-4651) | <0 0 1> | <1 0 0> | 282.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
V(FeO2)2 (mp-690463) | 0.1596 | 0.216 | 3 |
Co2GeO4 (mp-561853) | 0.1407 | 0.173 | 3 |
Zn(NiO2)2 (mvc-6924) | 0.1316 | 0.137 | 3 |
MgTi2O4 (mvc-6475) | 0.1570 | 0.095 | 3 |
Al(FeO2)2 (mvc-10947) | 0.1582 | 0.539 | 3 |
LiMnNbO4 (mp-861574) | 0.2250 | 0.017 | 4 |
LiVNiO4 (mp-771631) | 0.1822 | 0.001 | 4 |
LiNbCoO4 (mp-772384) | 0.1977 | 0.143 | 4 |
LiNbFeO4 (mp-772339) | 0.2248 | 0.005 | 4 |
LiVCoO4 (mp-768046) | 0.2264 | 0.000 | 4 |
Fe3O4 (mp-715490) | 0.1720 | 0.000 | 2 |
Fe3O4 (mp-542433) | 0.2042 | 0.075 | 2 |
Fe3O4 (mp-567124) | 0.2061 | 0.017 | 2 |
Fe3O4 (mp-31770) | 0.2099 | 0.017 | 2 |
Fe3O4 (mp-715558) | 0.2095 | 0.785 | 2 |
Li2Cr2FeSbO8 (mp-861530) | 0.3688 | 4.856 | 5 |
Li4Mn3Fe3(SbO8)2 (mp-775013) | 0.3669 | 6.473 | 5 |
Li4Cr3Fe3(TeO8)2 (mp-773518) | 0.3593 | 0.054 | 5 |
Li4Fe3Ni3(TeO8)2 (mp-773382) | 0.3569 | 0.197 | 5 |
Li4Cr3Fe3(SbO8)2 (mp-771925) | 0.3513 | 6.495 | 5 |
Li3MnFeCo(PO4)3 (mp-764931) | 0.6695 | 0.017 | 6 |
Li3MnFeCo(PO4)3 (mp-764809) | 0.6587 | 0.014 | 6 |
Li3MnFeCo(PO4)3 (mp-764869) | 0.6659 | 0.032 | 6 |
Li3MnFeCo(PO4)3 (mp-764969) | 0.6641 | 0.057 | 6 |
Li3MnFeCo(PO4)3 (mp-764870) | 0.6692 | 0.466 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesCr: 3.7 eV |
PseudopotentialsVASP PAW: Al Cr_pv O |
Final Energy/Atom-7.6473 eV |
Corrected Energy-120.5548 eV
Uncorrected energy = -107.0628 eV
Composition-based energy adjustment (-0.687 eV/atom x 8.0 atoms) = -5.4960 eV
Composition-based energy adjustment (-1.999 eV/atom x 4.0 atoms) = -7.9960 eV
Corrected energy = -120.5548 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)