Final Magnetic Moment17.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.077 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.069 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.20 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiFeO2 + LiMnO2 |
Band Gap0.145 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinR3m [166] |
Hall-R 3 2" |
Point Group3m |
Crystal Systemtrigonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 0 1> | 213.2 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 121.8 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 274.1 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 213.2 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 213.2 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 274.1 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 335.0 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 173.7 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 335.0 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 91.4 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 335.0 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 213.2 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 274.1 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 243.7 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 365.5 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 152.3 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 121.8 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 30.5 |
YVO4 (mp-19133) | <0 0 1> | <1 1 1> | 153.5 |
TePb (mp-19717) | <1 1 1> | <0 0 1> | 213.2 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 213.2 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 274.1 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 335.0 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 121.8 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 30.5 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 121.8 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 91.4 |
BN (mp-984) | <0 0 1> | <0 0 1> | 213.2 |
BN (mp-984) | <1 0 1> | <0 0 1> | 213.2 |
BN (mp-984) | <1 1 0> | <0 0 1> | 274.1 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 91.4 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 365.5 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 274.1 |
Al (mp-134) | <1 0 0> | <0 0 1> | 243.7 |
Al (mp-134) | <1 1 1> | <0 0 1> | 365.5 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 274.1 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 335.0 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 365.5 |
LiTaO3 (mp-3666) | <0 0 1> | <0 0 1> | 91.4 |
Fe3O4 (mp-19306) | <1 1 1> | <0 0 1> | 121.8 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 91.4 |
MgO (mp-1265) | <1 1 1> | <0 0 1> | 30.5 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 274.1 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 152.3 |
C (mp-66) | <1 0 0> | <0 0 1> | 152.3 |
C (mp-66) | <1 1 0> | <0 0 1> | 335.0 |
C (mp-66) | <1 1 1> | <0 0 1> | 91.4 |
GdScO3 (mp-5690) | <0 0 1> | <1 0 0> | 260.6 |
GdScO3 (mp-5690) | <1 0 0> | <0 0 1> | 243.7 |
GdScO3 (mp-5690) | <1 0 1> | <1 0 0> | 173.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
EuYO2 (mp-769167) | 0.2537 | 0.099 | 3 |
NaInO2 (mp-5175) | 0.2550 | 0.000 | 3 |
Sr2HN (mp-690794) | 0.2537 | 0.000 | 3 |
Li2PtO3 (mp-531826) | 0.2493 | 0.000 | 3 |
CaZrN2 (mp-1029267) | 0.2503 | 0.000 | 3 |
Li3Fe4CuO8 (mp-770911) | 0.2051 | 0.084 | 4 |
Li2CuNiO4 (mp-771847) | 0.2152 | 0.054 | 4 |
Li2MnFeO4 (mp-770627) | 0.2067 | 0.031 | 4 |
Li3Fe4SnO8 (mp-769833) | 0.2152 | 0.034 | 4 |
Li4Mn3CuO8 (mp-773427) | 0.2152 | 0.088 | 4 |
LiTe3 (mp-27466) | 0.3307 | 0.009 | 2 |
Bi2Te3 (mp-568390) | 0.2841 | 0.248 | 2 |
In2Se3 (mp-1068548) | 0.2966 | 0.530 | 2 |
In2Se3 (mp-20830) | 0.3088 | 0.530 | 2 |
Sb2Te3 (mp-1080789) | 0.2715 | 0.129 | 2 |
Na6MnNi3(SbO6)2 (mp-1094109) | 0.5016 | 0.139 | 5 |
Hg (mp-982872) | 0.4753 | 0.020 | 1 |
Sb (mp-632286) | 0.4498 | 0.059 | 1 |
Te (mp-570459) | 0.4460 | 0.044 | 1 |
Te (mp-10654) | 0.5330 | 0.047 | 1 |
Te (mp-105) | 0.4132 | 0.047 | 1 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eVFe: 5.3 eV |
PseudopotentialsVASP PAW: Li_sv Mn_pv Fe_pv O |
Final Energy/Atom-6.4385 eV |
Corrected Energy-115.7716 eV
Uncorrected energy = -103.0156 eV
Composition-based energy adjustment (-0.687 eV/atom x 8.0 atoms) = -5.4960 eV
Composition-based energy adjustment (-1.668 eV/atom x 3.0 atoms) = -5.0040 eV
Composition-based energy adjustment (-2.256 eV/atom x 1.0 atoms) = -2.2560 eV
Corrected energy = -115.7716 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)