Final Magnetic Moment0.044 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-1.812 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.724 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.24 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiMnNbO4 + Li3NbO4 + LiNbO3 + Mn3O4 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [1] |
HallP 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 98.6 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 230.1 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 230.1 |
AlN (mp-661) | <1 0 0> | <1 -1 0> | 61.7 |
AlN (mp-661) | <1 0 1> | <1 0 1> | 69.8 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 295.8 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 230.1 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 164.4 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 230.1 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 197.2 |
BaF2 (mp-1029) | <1 1 0> | <0 1 1> | 278.6 |
GaN (mp-804) | <1 0 0> | <0 1 0> | 183.5 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 131.5 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 230.1 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 295.8 |
SiO2 (mp-6930) | <1 1 1> | <1 -1 1> | 209.4 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 295.8 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 1> | 278.6 |
DyScO3 (mp-31120) | <0 1 1> | <1 1 0> | 105.9 |
DyScO3 (mp-31120) | <1 1 1> | <1 1 0> | 211.7 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 263.0 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 263.0 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 230.1 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 0> | 244.6 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 245.4 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 295.8 |
CdS (mp-672) | <1 0 0> | <0 1 1> | 209.0 |
CdS (mp-672) | <1 0 1> | <0 1 0> | 305.8 |
LiF (mp-1138) | <1 0 0> | <0 1 0> | 244.6 |
LiF (mp-1138) | <1 1 0> | <1 1 0> | 211.7 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 164.4 |
MgO (mp-1265) | <1 1 0> | <0 0 1> | 131.5 |
MgO (mp-1265) | <1 1 1> | <0 0 1> | 32.9 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 65.7 |
Te2W (mp-22693) | <1 0 0> | <1 0 1> | 279.0 |
TiO2 (mp-2657) | <1 0 0> | <0 1 0> | 305.8 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 361.6 |
TiO2 (mp-2657) | <1 1 1> | <0 0 1> | 263.0 |
YVO4 (mp-19133) | <0 0 1> | <0 1 0> | 305.8 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 131.5 |
YVO4 (mp-19133) | <1 1 0> | <1 -1 0> | 61.7 |
C (mp-66) | <1 0 0> | <0 0 1> | 263.0 |
C (mp-66) | <1 1 0> | <0 1 0> | 183.5 |
C (mp-66) | <1 1 1> | <0 0 1> | 295.8 |
TePb (mp-19717) | <1 1 1> | <0 0 1> | 230.1 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 32.9 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 164.4 |
Te2Mo (mp-602) | <1 1 0> | <0 1 0> | 183.5 |
Te2Mo (mp-602) | <1 1 1> | <0 0 1> | 98.6 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 263.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Fe2CuO4 (mp-705659) | 0.3093 | 0.589 | 3 |
Mg(MoO2)2 (mvc-6124) | 0.3249 | 0.200 | 3 |
Mg(SnO2)2 (mvc-9524) | 0.3221 | 0.284 | 3 |
Ca(WO2)2 (mvc-10243) | 0.2992 | 0.458 | 3 |
Ca(WO2)2 (mvc-10486) | 0.2775 | 0.499 | 3 |
Li4Co3Sb5O16 (mp-770677) | 0.1494 | 0.057 | 4 |
Li4Mn5Sb3O16 (mp-769848) | 0.1473 | 0.112 | 4 |
Li4Mn5V3O16 (mp-773194) | 0.1942 | 0.230 | 4 |
Li4Fe3Sb5O16 (mp-769870) | 0.1760 | 0.046 | 4 |
Li4Ni3Sb5O16 (mp-774248) | 0.1865 | 0.081 | 4 |
Si3N4 (mp-641539) | 0.5466 | 0.288 | 2 |
Ge3N4 (mp-641541) | 0.4941 | 0.208 | 2 |
Fe3O4 (mp-650112) | 0.5419 | 0.060 | 2 |
Fe3O4 (mp-716052) | 0.5635 | 0.781 | 2 |
Fe3O4 (mp-715811) | 0.5643 | 0.037 | 2 |
Li4Mn3Cu2Sb3O16 (mp-775072) | 0.1822 | 0.242 | 5 |
Li4Nb3Fe3(NiO8)2 (mp-775068) | 0.2007 | 0.118 | 5 |
Li4V3Fe2Sb3O16 (mp-853181) | 0.1948 | 0.341 | 5 |
Li4Co3Cu2Sb3O16 (mp-763275) | 0.1379 | 0.147 | 5 |
Li4Ti3Mn3(CuO8)2 (mp-781494) | 0.1674 | 0.083 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eV |
PseudopotentialsVASP PAW: Li_sv Mn_pv Nb_pv O |
Final Energy/Atom-6.9291 eV |
Corrected Energy-213.6552 eV
-213.6552 eV = -194.0143 eV (uncorrected energy) - 11.2366 eV (MP Anion Correction) - 8.4043 eV (MP Advanced Correction)
|