Final Magnetic Moment2.500 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-2.399 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.045 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.80 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToNa3MnPCO7 + MnCO3 + Li3PO4 |
Band Gap3.557 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [1] |
HallP 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 1 0> | <0 0 1> | 291.0 |
GaN (mp-804) | <1 0 0> | <1 1 0> | 221.8 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 174.6 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 232.8 |
SiO2 (mp-6930) | <1 1 1> | <1 0 1> | 105.1 |
DyScO3 (mp-31120) | <0 1 1> | <0 1 0> | 269.8 |
DyScO3 (mp-31120) | <1 1 1> | <1 1 0> | 221.8 |
InAs (mp-20305) | <1 1 0> | <1 0 1> | 105.1 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 1> | 210.3 |
CdS (mp-672) | <1 0 0> | <0 1 0> | 202.4 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 291.0 |
LiF (mp-1138) | <1 1 0> | <1 0 1> | 210.3 |
YVO4 (mp-19133) | <0 0 1> | <0 1 0> | 202.4 |
TePb (mp-19717) | <1 0 0> | <0 1 0> | 134.9 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 232.8 |
Te2Mo (mp-602) | <1 1 1> | <0 0 1> | 291.0 |
Ag (mp-124) | <1 1 0> | <0 1 1> | 270.4 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 174.6 |
GaSe (mp-1943) | <1 1 0> | <0 0 1> | 116.4 |
BN (mp-984) | <0 0 1> | <0 0 1> | 174.6 |
BN (mp-984) | <1 1 0> | <1 0 0> | 262.2 |
Al (mp-134) | <1 1 0> | <1 0 1> | 210.3 |
TeO2 (mp-2125) | <1 0 1> | <0 0 1> | 232.8 |
SiC (mp-7631) | <1 0 0> | <0 0 1> | 291.0 |
LiGaO2 (mp-5854) | <0 1 1> | <0 0 1> | 174.6 |
CdTe (mp-406) | <1 0 0> | <0 1 1> | 90.1 |
TeO2 (mp-2125) | <1 0 0> | <1 0 1> | 210.3 |
MgO (mp-1265) | <1 0 0> | <0 1 0> | 269.8 |
Fe3O4 (mp-19306) | <1 0 0> | <0 0 1> | 291.0 |
Fe3O4 (mp-19306) | <1 1 0> | <1 0 1> | 105.1 |
TiO2 (mp-2657) | <0 0 1> | <0 0 1> | 174.6 |
TiO2 (mp-2657) | <1 0 0> | <1 0 0> | 262.2 |
TiO2 (mp-2657) | <1 1 1> | <0 0 1> | 58.2 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 58.2 |
C (mp-66) | <1 0 0> | <0 1 0> | 202.4 |
C (mp-66) | <1 1 0> | <0 0 1> | 291.0 |
GdScO3 (mp-5690) | <0 1 1> | <0 1 0> | 269.8 |
GdScO3 (mp-5690) | <1 1 1> | <1 1 0> | 221.8 |
C (mp-66) | <1 1 1> | <0 0 1> | 174.6 |
TbScO3 (mp-31119) | <1 1 1> | <1 1 0> | 221.8 |
Ni (mp-23) | <1 1 1> | <0 0 1> | 174.6 |
InSb (mp-20012) | <1 0 0> | <0 1 1> | 90.1 |
PbS (mp-21276) | <1 0 0> | <0 1 1> | 180.3 |
PbS (mp-21276) | <1 1 0> | <1 0 1> | 105.1 |
InP (mp-20351) | <1 0 0> | <0 1 1> | 180.3 |
BaTiO3 (mp-5986) | <1 0 1> | <1 0 1> | 210.3 |
BaTiO3 (mp-5986) | <1 1 0> | <0 0 1> | 291.0 |
NdGaO3 (mp-3196) | <0 1 1> | <0 1 1> | 270.4 |
SiC (mp-11714) | <1 0 1> | <0 0 1> | 232.8 |
SiC (mp-11714) | <1 1 0> | <0 1 0> | 269.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Na3Ca(BO2)5 (mp-542719) | 0.6966 | 0.000 | 4 |
Na3MnAsCO7 (mp-771476) | 0.3388 | 0.000 | 5 |
Na5Mn2P2(CO7)2 (mp-769529) | 0.3704 | 0.003 | 5 |
Na5Mn2P2(CO7)2 (mp-769465) | 0.3516 | 0.004 | 5 |
Na5Mn2P2(CO7)2 (mp-769461) | 0.3495 | 0.009 | 5 |
Na3CuSiCO7 (mp-771162) | 0.3752 | 0.057 | 5 |
Na3Li3Fe2P2(CO7)2 (mp-770914) | 0.1679 | 0.026 | 6 |
NaLi2MnPCO7 (mp-773802) | 0.1570 | 0.047 | 6 |
Na3Li3Mn2P2(CO7)2 (mp-773755) | 0.1518 | 0.035 | 6 |
Na3Li3Mn2P2(CO7)2 (mp-773688) | 0.1639 | 0.036 | 6 |
Na3Li3Mn2P2(CO7)2 (mp-773403) | 0.1470 | 0.035 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eV |
PseudopotentialsVASP PAW: Na_pv Li_sv Mn_pv P C O |
Final Energy/Atom-6.7819 eV |
Corrected Energy-379.0457 eV
-379.0457 eV = -352.6582 eV (uncorrected energy) - 19.6641 eV (MP Anion Correction) - 6.7234 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)