material

TiCrO4

ID:

mp-755596


Material Details

Final Magnetic Moment
1.999 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
FM
Formation Energy / Atom
-2.716 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.071 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
3.97 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
CrO2 + TiO2
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
I4m2 [119]
Hall
I 4 2
Point Group
42m
Crystal System
tetragonal

Electronic Structure

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
Ni (mp-23) <1 1 1> <1 0 0> 0.007 256.4
MgF2 (mp-1249) <1 0 1> <0 0 1> 0.008 210.6
DyScO3 (mp-31120) <1 1 0> <0 0 1> 0.018 126.3
GaN (mp-804) <1 0 1> <0 0 1> 0.021 210.6
PbSe (mp-2201) <1 0 0> <0 0 1> 0.027 350.9
YAlO3 (mp-3792) <1 1 0> <0 0 1> 0.031 56.1
SrTiO3 (mp-4651) <1 0 0> <1 0 1> 0.032 353.0
TbScO3 (mp-31119) <0 1 0> <0 0 1> 0.035 350.9
ZrO2 (mp-2858) <1 0 1> <1 1 1> 0.037 214.7
TbScO3 (mp-31119) <1 1 0> <0 0 1> 0.047 126.3
Ni (mp-23) <1 1 0> <1 0 1> 0.048 156.9
Au (mp-81) <1 0 0> <0 0 1> 0.060 70.2
Te2Mo (mp-602) <0 0 1> <1 0 1> 0.069 196.1
Mg (mp-153) <1 0 0> <0 0 1> 0.076 84.2
ZnO (mp-2133) <1 0 0> <1 1 0> 0.081 51.8
Fe2O3 (mp-24972) <0 0 1> <0 0 1> 0.087 252.7
GaN (mp-804) <1 1 0> <1 0 1> 0.089 117.7
CdWO4 (mp-19387) <0 1 1> <1 1 1> 0.093 161.0
LiGaO2 (mp-5854) <1 1 0> <1 0 0> 0.097 146.5
AlN (mp-661) <1 0 1> <1 0 1> 0.102 196.1
ZrO2 (mp-2858) <1 0 -1> <1 1 1> 0.103 107.3
Al (mp-134) <1 1 0> <1 1 0> 0.105 207.2
InP (mp-20351) <1 0 0> <0 0 1> 0.107 70.2
GdScO3 (mp-5690) <0 1 0> <0 0 1> 0.112 350.9
KTaO3 (mp-3614) <1 1 0> <1 1 0> 0.117 207.2
NdGaO3 (mp-3196) <1 0 0> <0 0 1> 0.118 350.9
SiO2 (mp-6930) <1 1 1> <1 0 1> 0.119 156.9
CdS (mp-672) <1 0 1> <0 0 1> 0.127 322.8
KP(HO2)2 (mp-23959) <0 0 1> <0 0 1> 0.132 224.6
BaF2 (mp-1029) <1 0 0> <0 0 1> 0.134 350.9
Ge3(BiO3)4 (mp-23560) <1 0 0> <0 0 1> 0.136 112.3
WS2 (mp-224) <1 0 0> <1 0 1> 0.137 313.8
LiAlO2 (mp-3427) <1 0 1> <1 1 1> 0.150 214.7
Ag (mp-124) <1 0 0> <0 0 1> 0.156 70.2
SiO2 (mp-6930) <1 0 1> <1 0 1> 0.157 313.8
Ni (mp-23) <1 0 0> <0 0 1> 0.162 112.3
CdWO4 (mp-19387) <0 0 1> <1 1 1> 0.168 214.7
LiNbO3 (mp-3731) <1 0 1> <1 1 0> 0.170 155.4
NdGaO3 (mp-3196) <1 1 1> <1 1 0> 0.174 207.2
BaTiO3 (mp-5986) <0 0 1> <0 0 1> 0.175 126.3
SrTiO3 (mp-4651) <1 1 0> <0 0 1> 0.181 126.3
ZrO2 (mp-2858) <0 1 1> <0 0 1> 0.190 196.5
YAlO3 (mp-3792) <0 1 0> <1 1 0> 0.202 155.4
LaF3 (mp-905) <1 1 0> <0 0 1> 0.204 280.7
YAlO3 (mp-3792) <0 0 1> <0 0 1> 0.208 28.1
Al2O3 (mp-1143) <1 0 0> <1 0 0> 0.210 256.4
CdWO4 (mp-19387) <1 1 1> <1 0 1> 0.212 156.9
SiC (mp-11714) <1 1 0> <0 0 1> 0.212 322.8
GaN (mp-804) <0 0 1> <0 0 1> 0.214 168.4
LiNbO3 (mp-3731) <1 0 0> <0 0 1> 0.216 224.6
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.

Once you have registered you can also "vote" for full calculation of this material's elastic properties.

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
TiVO4 (mp-780818) 0.1307 0.043 3
NbFeO4 (mp-774156) 0.0871 0.023 3
MnNbO4 (mp-774148) 0.1801 0.052 3
Ti15NbO32 (mp-1099073) 0.1623 0.004 3
TiMnO4 (mp-775296) 0.1550 0.053 3
LiFe5(OF2)4 (mp-782691) 0.2991 0.081 4
Ti2Mn3Cr3O16 (mp-771540) 0.5131 0.084 4
Mn3Cr3(WO8)2 (mp-778921) 0.5178 0.103 4
LiV(OF)2 (mp-764229) 0.4499 0.026 4
AlV(WO4)2 (mvc-704) 0.5095 0.014 4
ZrO2 (mp-754403) 0.2324 0.015 2
IrO2 (mp-1014261) 0.2459 0.263 2
SnO2 (mp-755071) 0.2343 0.057 2
TiO2 (mp-390) 0.1651 0.006 2
TiO2 (mp-34688) 0.2232 0.008 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Structure Optimization

Run Type
GGA+U
Energy Cutoff
520 eV
# of K-points
None
U Values
Cr: 3.7 eV
Pseudopotentials
VASP PAW: Ti_pv Cr_pv O
Final Energy/Atom
-8.1355 eV
Corrected Energy
-53.6350 eV
-53.6350 eV = -48.8128 eV (uncorrected energy) - 2.8092 eV (MP Anion Correction) - 2.0130 eV (MP Advanced Correction)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
Submitted by