Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingAFM |
Formation Energy / Atom-2.541 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.084 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.90 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi2Si2O5 + Fe2O3 |
Band Gap1.311 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinImma [74] |
Hall-I 2b 2 |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 0 0> | 282.2 |
AlN (mp-661) | <0 0 1> | <0 1 1> | 111.2 |
AlN (mp-661) | <1 0 0> | <1 0 1> | 230.3 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 232.3 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 329.3 |
AlN (mp-661) | <1 1 1> | <1 1 1> | 145.7 |
GaAs (mp-2534) | <1 1 1> | <0 1 0> | 223.1 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 232.3 |
GaN (mp-804) | <1 0 0> | <0 1 0> | 312.4 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 94.1 |
GaN (mp-804) | <1 1 0> | <0 1 0> | 89.2 |
CeO2 (mp-20194) | <1 0 0> | <0 1 1> | 278.0 |
CeO2 (mp-20194) | <1 1 0> | <0 1 0> | 44.6 |
CeO2 (mp-20194) | <1 1 1> | <0 1 0> | 312.4 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 33.2 |
GaAs (mp-2534) | <1 1 0> | <0 1 0> | 44.6 |
SiO2 (mp-6930) | <1 0 0> | <0 1 1> | 55.6 |
SiO2 (mp-6930) | <1 0 1> | <0 1 1> | 278.0 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 99.5 |
KCl (mp-23193) | <1 1 0> | <0 1 0> | 178.5 |
GaN (mp-804) | <1 1 1> | <0 1 1> | 222.4 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 33.2 |
DyScO3 (mp-31120) | <0 1 0> | <0 1 0> | 44.6 |
DyScO3 (mp-31120) | <0 1 1> | <0 1 1> | 55.6 |
DyScO3 (mp-31120) | <1 0 0> | <0 1 0> | 44.6 |
DyScO3 (mp-31120) | <1 1 0> | <1 1 0> | 64.8 |
DyScO3 (mp-31120) | <1 1 1> | <1 1 1> | 72.8 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 33.2 |
ZnSe (mp-1190) | <1 1 0> | <0 1 0> | 44.6 |
ZnSe (mp-1190) | <1 1 1> | <0 1 0> | 223.1 |
DyScO3 (mp-31120) | <1 0 1> | <0 1 1> | 55.6 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 0> | 44.6 |
CdS (mp-672) | <0 0 1> | <1 1 0> | 259.3 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 298.6 |
KTaO3 (mp-3614) | <1 0 0> | <1 1 0> | 64.8 |
KTaO3 (mp-3614) | <1 1 1> | <0 1 1> | 55.6 |
CdS (mp-672) | <1 0 1> | <0 1 0> | 223.1 |
CdS (mp-672) | <1 1 1> | <1 1 0> | 259.3 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 33.2 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 47.0 |
Te2W (mp-22693) | <0 1 0> | <1 0 0> | 282.2 |
Te2W (mp-22693) | <0 1 1> | <0 0 1> | 298.6 |
LiF (mp-1138) | <1 1 1> | <0 1 1> | 55.6 |
TePb (mp-19717) | <1 1 0> | <0 1 0> | 178.5 |
YVO4 (mp-19133) | <0 0 1> | <1 1 0> | 259.3 |
YVO4 (mp-19133) | <1 0 1> | <1 0 1> | 287.8 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 298.6 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 141.1 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 265.5 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 99.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Yb2FeS4 (mp-5643) | 0.2351 | 0.377 | 3 |
Mg2SiO4 (mp-5639) | 0.2283 | 0.072 | 3 |
Y(NiO2)2 (mvc-16809) | 0.1984 | 0.234 | 3 |
Y(FeO2)2 (mvc-16797) | 0.2263 | 0.106 | 3 |
Yb2MnSe4 (mp-19719) | 0.2279 | 0.242 | 3 |
LiTiSiO4 (mp-753305) | 0.1399 | 0.076 | 4 |
LiVSiO4 (mp-767033) | 0.1054 | 0.044 | 4 |
LiCrSiO4 (mp-763701) | 0.0637 | 0.059 | 4 |
LiVFeO4 (mp-773535) | 0.1266 | 0.016 | 4 |
LiCoSiO4 (mp-762883) | 0.1011 | 0.142 | 4 |
Fe3O4 (mp-715491) | 0.3464 | 0.015 | 2 |
Cr3N4 (mp-1014358) | 0.3483 | 0.227 | 2 |
Fe3O4 (mp-650112) | 0.3490 | 0.057 | 2 |
Fe3O4 (mp-31770) | 0.3618 | 0.015 | 2 |
Fe3O4 (mp-716052) | 0.3708 | 0.073 | 2 |
Li2CoNi(PO4)2 (mp-761996) | 0.3760 | 0.016 | 5 |
Li4Mn3Ni3(TeO8)2 (mp-770951) | 0.3863 | 0.001 | 5 |
Li4CoNi3(PO4)4 (mp-853138) | 0.3837 | 0.013 | 5 |
Li4Fe3Ni3(TeO8)2 (mp-773382) | 0.3738 | 0.009 | 5 |
Li2FeNi(PO4)2 (mp-769706) | 0.3841 | 0.002 | 5 |
Li3MnFeCo(PO4)3 (mp-764931) | 0.4671 | 0.015 | 6 |
Li3MnFeCo(PO4)3 (mp-764809) | 0.4547 | 0.015 | 6 |
Li3MnFeCo(PO4)3 (mp-764869) | 0.4659 | 0.032 | 6 |
Li3MnFeCo(PO4)3 (mp-764969) | 0.4642 | 0.032 | 6 |
Li3MnFeCo(PO4)3 (mp-764870) | 0.4673 | 0.661 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesFe: 5.3 eV |
PseudopotentialsVASP PAW: Li_sv Fe_pv Si O |
Final Energy/Atom-6.8349 eV |
Corrected Energy-213.5460 eV
-213.5460 eV = -191.3774 eV (uncorrected energy) - 11.2366 eV (MP Anion Correction) - 10.9320 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)