Final Magnetic Moment15.002 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.512 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.100 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.36 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToFe2O3 + Li3FeF6 + FeF3 |
Band Gap2.333 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [1] |
HallP 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 0> | <0 0 1> | 138.3 |
LaAlO3 (mp-2920) | <0 0 1> | <1 0 0> | 122.7 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 221.3 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 193.6 |
AlN (mp-661) | <1 0 0> | <1 0 -1> | 81.1 |
AlN (mp-661) | <1 0 1> | <1 1 0> | 145.6 |
AlN (mp-661) | <1 1 0> | <1 -1 1> | 212.9 |
AlN (mp-661) | <1 1 1> | <1 1 0> | 145.6 |
CeO2 (mp-20194) | <1 0 0> | <1 -1 1> | 212.9 |
CeO2 (mp-20194) | <1 1 0> | <0 1 -1> | 208.8 |
CeO2 (mp-20194) | <1 1 1> | <1 1 1> | 306.3 |
GaAs (mp-2534) | <1 0 0> | <1 -1 -1> | 266.1 |
GaAs (mp-2534) | <1 1 0> | <1 -1 0> | 276.3 |
GaAs (mp-2534) | <1 1 1> | <0 1 0> | 223.2 |
BaF2 (mp-1029) | <1 1 0> | <1 -1 1> | 170.3 |
BaF2 (mp-1029) | <1 1 1> | <1 0 1> | 210.1 |
GaN (mp-804) | <0 0 1> | <1 -1 1> | 212.9 |
GaN (mp-804) | <1 0 1> | <1 0 1> | 168.1 |
GaN (mp-804) | <1 1 0> | <0 1 -1> | 208.8 |
GaN (mp-804) | <1 1 1> | <1 -1 0> | 276.3 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 83.0 |
SiO2 (mp-6930) | <1 0 0> | <1 -1 1> | 212.9 |
SiO2 (mp-6930) | <0 0 1> | <1 1 1> | 245.0 |
SiO2 (mp-6930) | <1 0 1> | <1 0 0> | 276.0 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 138.3 |
KCl (mp-23193) | <1 0 0> | <1 -1 -1> | 212.9 |
KCl (mp-23193) | <1 1 0> | <1 -1 1> | 170.3 |
KCl (mp-23193) | <1 1 1> | <1 0 1> | 210.1 |
ZnSe (mp-1190) | <1 1 0> | <0 1 0> | 223.2 |
ZnSe (mp-1190) | <1 1 1> | <0 1 0> | 223.2 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 193.6 |
DyScO3 (mp-31120) | <0 1 0> | <0 1 0> | 223.2 |
DyScO3 (mp-31120) | <0 1 1> | <1 -1 1> | 212.9 |
DyScO3 (mp-31120) | <1 0 0> | <0 1 0> | 223.2 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 0> | 276.0 |
DyScO3 (mp-31120) | <1 1 0> | <1 1 0> | 194.2 |
DyScO3 (mp-31120) | <1 1 1> | <1 1 -1> | 149.7 |
KTaO3 (mp-3614) | <1 0 0> | <1 -1 1> | 127.7 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 -1> | 283.9 |
InAs (mp-20305) | <1 0 0> | <1 1 0> | 145.6 |
InAs (mp-20305) | <1 1 0> | <1 -1 0> | 157.9 |
CdS (mp-672) | <0 0 1> | <1 1 -1> | 249.5 |
CdS (mp-672) | <1 0 0> | <1 -1 0> | 197.3 |
CdS (mp-672) | <1 1 1> | <1 -1 0> | 157.9 |
ZnSe (mp-1190) | <1 0 0> | <1 -1 -1> | 266.1 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 138.3 |
Te2W (mp-22693) | <0 0 1> | <0 1 -1> | 174.0 |
Te2W (mp-22693) | <0 1 0> | <1 0 1> | 168.1 |
Te2W (mp-22693) | <0 1 1> | <0 1 0> | 287.0 |
CdS (mp-672) | <1 0 1> | <1 -1 1> | 127.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Piezoelectric Tensor eij (C/m2) |
|||||
---|---|---|---|---|---|
0.12668 | 0.02193 | -0.00596 | 0.15166 | -0.09216 | -0.00475 |
-0.10563 | -0.03655 | -0.03989 | -0.02421 | 0.01499 | 0.00747 |
0.13420 | 0.08531 | 0.11573 | 0.05700 | -0.04778 | 0.03001 |
Piezoelectric Modulus ‖eij‖max0.29985 C/m2 |
Crystallographic Direction vmax |
---|
-1.00000 |
-1.00000 |
0.00000 |
Dielectric Tensor εij∞ (electronic contribution) |
||
---|---|---|
3.33 | 0.02 | 0.02 |
0.02 | 2.27 | 0.00 |
0.02 | 0.00 | 3.06 |
Dielectric Tensor εij (total) |
||
---|---|---|
11.73 | -1.23 | 0.54 |
-1.23 | 5.52 | -0.05 |
0.54 | -0.05 | 8.90 |
Polycrystalline dielectric constant
εpoly∞
2.89
|
Polycrystalline dielectric constant
εpoly
8.72
|
Refractive Index n1.70 |
Potentially ferroelectric?Unknown |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesFe: 5.3 eV |
PseudopotentialsVASP PAW: Li_sv Fe_pv O F |
Final Energy/Atom-5.5233 eV |
Corrected Energy-75.8827 eV
-75.8827 eV = -66.2791 eV (uncorrected energy) - 8.1990 eV (MP Advanced Correction) - 1.4046 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)