Final Magnetic Moment0.999 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.221 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.132 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.89 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToNa5LiFe2P2(CO7)2 + FeCO3 + Li3PO4 |
Band Gap3.630 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPc [7] |
HallP 2yc |
Point Groupm |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
GaN (mp-804) | <1 0 0> | <1 0 0> | 68.1 |
GaN (mp-804) | <1 1 0> | <1 0 0> | 204.4 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 176.8 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 235.8 |
SiO2 (mp-6930) | <1 0 1> | <1 0 1> | 274.0 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 294.7 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 294.7 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 176.8 |
TePb (mp-19717) | <1 1 0> | <1 0 1> | 182.7 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 176.8 |
Ag (mp-124) | <1 1 0> | <1 0 1> | 274.0 |
GaSe (mp-1943) | <1 1 0> | <0 0 1> | 117.9 |
BN (mp-984) | <1 0 1> | <0 1 0> | 183.5 |
BN (mp-984) | <1 1 0> | <0 1 0> | 275.2 |
LiGaO2 (mp-5854) | <0 1 0> | <1 0 0> | 68.1 |
LiGaO2 (mp-5854) | <1 0 0> | <0 0 1> | 176.8 |
LiGaO2 (mp-5854) | <1 1 0> | <0 0 1> | 294.7 |
LiGaO2 (mp-5854) | <1 1 1> | <0 1 0> | 275.2 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 294.7 |
SiC (mp-7631) | <1 0 0> | <0 0 1> | 235.8 |
CdTe (mp-406) | <1 0 0> | <0 0 1> | 176.8 |
CdTe (mp-406) | <1 1 0> | <1 0 1> | 182.7 |
TeO2 (mp-2125) | <0 1 0> | <0 1 0> | 275.2 |
TeO2 (mp-2125) | <1 0 0> | <0 1 0> | 275.2 |
MgO (mp-1265) | <1 0 0> | <1 0 0> | 272.6 |
TiO2 (mp-2657) | <0 0 1> | <0 0 1> | 176.8 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 58.9 |
C (mp-66) | <1 0 0> | <1 0 0> | 204.4 |
C (mp-66) | <1 1 1> | <0 0 1> | 176.8 |
TiO2 (mp-2657) | <1 0 0> | <1 0 1> | 274.0 |
TiO2 (mp-2657) | <1 1 1> | <0 0 1> | 58.9 |
PbS (mp-21276) | <1 0 0> | <1 0 1> | 182.7 |
Mg (mp-153) | <0 0 1> | <0 0 1> | 294.7 |
BaTiO3 (mp-5986) | <0 0 1> | <0 0 1> | 235.8 |
Ni (mp-23) | <1 0 0> | <0 0 1> | 294.7 |
Ni (mp-23) | <1 1 0> | <1 0 1> | 274.0 |
InSb (mp-20012) | <1 0 0> | <0 0 1> | 176.8 |
InSb (mp-20012) | <1 1 0> | <1 0 1> | 182.7 |
MoSe2 (mp-1634) | <1 0 0> | <1 0 0> | 204.4 |
MoSe2 (mp-1634) | <1 0 1> | <1 0 0> | 204.4 |
BaTiO3 (mp-5986) | <1 0 0> | <0 1 1> | 218.1 |
BaTiO3 (mp-5986) | <1 1 0> | <0 1 1> | 218.1 |
SiC (mp-11714) | <1 0 1> | <0 0 1> | 235.8 |
SiC (mp-11714) | <1 1 0> | <1 0 0> | 272.6 |
Ga2O3 (mp-886) | <0 1 0> | <0 1 1> | 218.1 |
Ga2O3 (mp-886) | <1 0 0> | <0 0 1> | 294.7 |
C (mp-48) | <0 0 1> | <0 0 1> | 235.8 |
Au (mp-81) | <1 1 0> | <1 0 1> | 274.0 |
C (mp-48) | <1 0 1> | <0 1 0> | 275.2 |
ZrO2 (mp-2858) | <1 1 1> | <0 0 1> | 294.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Na3ZnPCO7 (mp-767545) | 0.2102 | 0.002 | 5 |
Na3FeAsCO7 (mp-771494) | 0.1841 | 0.000 | 5 |
Na3VSiCO7 (mp-771420) | 0.1954 | 0.000 | 5 |
Na3CoAsCO7 (mp-773177) | 0.2017 | 0.000 | 5 |
Na3FePCO7 (mp-24996) | 0.1916 | 0.132 | 5 |
Na5LiFe2P2(CO7)2 (mp-773529) | 0.1529 | 0.157 | 6 |
Na5LiFe2P2(CO7)2 (mp-773523) | 0.1460 | 0.148 | 6 |
Na5LiFe2P2(CO7)2 (mp-770144) | 0.1476 | 0.001 | 6 |
Na2LiFePCO7 (mp-773940) | 0.1522 | 0.099 | 6 |
Na5LiFe2P2(CO7)2 (mp-773446) | 0.1465 | 0.188 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesFe: 5.3 eV |
PseudopotentialsVASP PAW: Na_pv Li_sv Fe_pv P C O |
Final Energy/Atom-6.4236 eV |
Corrected Energy-364.6228 eV
-364.6228 eV = -334.0267 eV (uncorrected energy) - 19.6641 eV (MP Anion Correction) - 10.9320 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)