Final Magnetic Moment49.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-1.901 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.104 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.73 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToFeO + Mg(FeO2)2 + LiFeO2 + Fe2O3 |
Band Gap1.369 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinR3m [160] |
HallR 3 2" |
Point Group3m |
Crystal Systemtrigonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 216.5 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 247.4 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 278.3 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 247.4 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 247.4 |
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 216.5 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 216.5 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 216.5 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 123.7 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 216.5 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 216.5 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 278.3 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 185.6 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 340.2 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 216.5 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 278.3 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 216.5 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 154.6 |
TePb (mp-19717) | <1 1 1> | <0 0 1> | 216.5 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 278.3 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 278.3 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 154.6 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 123.7 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 30.9 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 123.7 |
BN (mp-984) | <0 0 1> | <0 0 1> | 216.5 |
BN (mp-984) | <1 0 0> | <0 0 1> | 340.2 |
BN (mp-984) | <1 0 1> | <0 0 1> | 216.5 |
BN (mp-984) | <1 1 0> | <0 0 1> | 278.3 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 92.8 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 278.3 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 216.5 |
Al (mp-134) | <1 0 0> | <0 0 1> | 247.4 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 278.3 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 340.2 |
LiGaO2 (mp-5854) | <0 1 1> | <0 0 1> | 340.2 |
CdTe (mp-406) | <1 1 1> | <0 0 1> | 216.5 |
LiTaO3 (mp-3666) | <0 0 1> | <0 0 1> | 92.8 |
Fe3O4 (mp-19306) | <1 1 1> | <0 0 1> | 123.7 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 92.8 |
MgO (mp-1265) | <1 1 0> | <0 0 1> | 123.7 |
MgO (mp-1265) | <1 1 1> | <0 0 1> | 30.9 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 216.5 |
Ni (mp-23) | <1 0 0> | <0 0 1> | 278.3 |
Ni (mp-23) | <1 1 1> | <0 0 1> | 278.3 |
InSb (mp-20012) | <1 1 1> | <0 0 1> | 216.5 |
PbSe (mp-2201) | <1 1 1> | <0 0 1> | 278.3 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 154.6 |
TiO2 (mp-2657) | <1 1 1> | <0 0 1> | 340.2 |
C (mp-66) | <1 0 0> | <0 0 1> | 154.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Zn(FeO2)2 (mvc-12178) | 0.1148 | 0.044 | 3 |
ZnCr2O4 (mvc-10098) | 0.1152 | 0.102 | 3 |
Zn(FeO2)2 (mp-34425) | 0.1140 | 0.044 | 3 |
V2ZnO4 (mvc-9963) | 0.1115 | 0.000 | 3 |
V2ZnO4 (mvc-10130) | 0.1067 | 0.028 | 3 |
LiZn2Fe9O16 (mp-773576) | 0.1464 | 0.077 | 4 |
Li3Co3OF7 (mp-765761) | 0.1520 | 0.042 | 4 |
Li2V3CoO8 (mp-774950) | 0.1533 | 0.145 | 4 |
Li3MgV8O16 (mp-771733) | 0.1435 | 0.023 | 4 |
Li3Zn(Fe5O8)4 (mp-771780) | 0.1533 | 0.067 | 4 |
Fe3O4 (mp-542433) | 0.2193 | 0.072 | 2 |
Fe3O4 (mp-650112) | 0.2149 | 0.057 | 2 |
Fe3O4 (mp-31770) | 0.2313 | 0.015 | 2 |
Fe3O4 (mp-715558) | 0.2362 | 0.076 | 2 |
Fe3O4 (mp-716052) | 0.2326 | 0.073 | 2 |
Li4Ti3Cr3(SnO8)2 (mp-776780) | 0.1933 | 0.029 | 5 |
Li14Mn22Cr3Cu3O56 (mp-735790) | 0.1568 | 0.019 | 5 |
Li4Cr3Co3(SbO8)2 (mp-762055) | 0.2092 | 0.029 | 5 |
Li4Ti3Cr3(WO8)2 (mp-773537) | 0.1887 | 0.043 | 5 |
Li4Cr3Fe3(TeO8)2 (mp-773518) | 0.1921 | 0.868 | 5 |
Li3MnFeCo(PO4)3 (mp-764809) | 0.7243 | 0.015 | 6 |
Li3MnFeCo(PO4)3 (mp-764869) | 0.7293 | 0.032 | 6 |
Li3MnFeCo(PO4)3 (mp-764707) | 0.7360 | 0.035 | 6 |
Li3MnFeCo(PO4)3 (mp-764969) | 0.7287 | 0.032 | 6 |
Li3MnFeCo(PO4)3 (mp-764870) | 0.7349 | 0.661 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesFe: 5.3 eV |
PseudopotentialsVASP PAW: Li_sv Mg_pv Fe_pv O |
Final Energy/Atom-6.5011 eV |
Corrected Energy-220.5964 eV
-220.5964 eV = -182.0297 eV (uncorrected energy) - 27.3300 eV (MP Advanced Correction) - 11.2366 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)