Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-2.383 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.027 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.82 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToNa3MnPCO7 + MnCO3 + Li3PO4 |
Band Gap3.370 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPc [7] |
HallP 2yc |
Point Groupm |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 1 0> | <0 0 1> | 241.2 |
BaF2 (mp-1029) | <1 1 0> | <0 1 1> | 109.3 |
BaF2 (mp-1029) | <1 1 1> | <0 1 0> | 273.6 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 301.5 |
GaN (mp-804) | <1 1 0> | <1 1 0> | 114.7 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 241.2 |
SiO2 (mp-6930) | <1 0 1> | <1 0 1> | 277.6 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 241.2 |
SiO2 (mp-6930) | <1 1 1> | <0 1 1> | 109.3 |
KCl (mp-23193) | <1 1 1> | <0 1 0> | 273.6 |
InAs (mp-20305) | <1 0 0> | <1 0 1> | 185.1 |
InAs (mp-20305) | <1 1 0> | <0 1 1> | 109.3 |
InAs (mp-20305) | <1 1 1> | <0 1 0> | 273.6 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 241.2 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 1> | 277.6 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 139.3 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 241.2 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 209.0 |
Ag (mp-124) | <1 1 0> | <0 1 1> | 218.7 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 1 1> | 259.8 |
GaSe (mp-1943) | <0 0 1> | <1 0 1> | 277.6 |
GaSe (mp-1943) | <1 1 0> | <0 0 1> | 120.6 |
BN (mp-984) | <0 0 1> | <0 1 1> | 109.3 |
BN (mp-984) | <1 1 0> | <0 1 0> | 273.6 |
BN (mp-984) | <1 1 1> | <0 1 0> | 273.6 |
Al (mp-134) | <1 0 0> | <0 0 1> | 241.2 |
Al (mp-134) | <1 1 1> | <1 0 1> | 277.6 |
LiGaO2 (mp-5854) | <0 0 1> | <0 1 0> | 273.6 |
TeO2 (mp-2125) | <0 1 0> | <0 1 0> | 273.6 |
TeO2 (mp-2125) | <1 0 0> | <0 1 1> | 218.7 |
LiTaO3 (mp-3666) | <1 0 0> | <1 0 1> | 277.6 |
LiTaO3 (mp-3666) | <1 1 0> | <0 0 1> | 120.6 |
C (mp-66) | <1 1 1> | <0 0 1> | 180.9 |
Mg (mp-153) | <1 1 0> | <1 1 0> | 114.7 |
InSb (mp-20012) | <1 0 0> | <0 0 1> | 180.9 |
PbSe (mp-2201) | <1 1 1> | <0 1 0> | 273.6 |
BaTiO3 (mp-5986) | <0 0 1> | <0 0 1> | 241.2 |
BaTiO3 (mp-5986) | <1 0 0> | <0 0 1> | 301.5 |
MoSe2 (mp-1634) | <1 0 1> | <1 0 0> | 209.0 |
Ga2O3 (mp-886) | <1 0 -1> | <1 0 1> | 185.1 |
LiGaO2 (mp-5854) | <1 1 1> | <0 1 0> | 273.6 |
CdTe (mp-406) | <1 0 0> | <0 0 1> | 180.9 |
TeO2 (mp-2125) | <1 0 1> | <0 0 1> | 241.2 |
MgO (mp-1265) | <1 1 0> | <1 1 0> | 229.5 |
C (mp-66) | <1 1 0> | <0 1 1> | 109.3 |
LaF3 (mp-905) | <1 0 1> | <0 1 0> | 273.6 |
PbS (mp-21276) | <1 0 0> | <1 0 1> | 185.1 |
Ni (mp-23) | <1 0 0> | <1 1 1> | 259.8 |
Ni (mp-23) | <1 1 0> | <1 0 1> | 277.6 |
PbSe (mp-2201) | <1 1 0> | <0 1 1> | 109.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Na3Ca(BO2)5 (mp-542719) | 0.7335 | 0.000 | 4 |
Na3ZnPCO7 (mp-767545) | 0.2566 | 0.002 | 5 |
Na3CuCSO7 (mp-772726) | 0.2583 | 0.090 | 5 |
Na3MnAsCO7 (mp-771476) | 0.2552 | 0.000 | 5 |
Na3CuSiCO7 (mp-771162) | 0.2697 | 0.057 | 5 |
Na3MnPCO7 (mp-19261) | 0.2770 | 0.000 | 5 |
Na2LiMnPCO7 (mp-770672) | 0.0870 | 0.019 | 6 |
Na2LiMnPCO7 (mp-773686) | 0.1612 | 0.323 | 6 |
Na2LiMnPCO7 (mp-773681) | 0.1622 | 0.159 | 6 |
Na3Li3Mn2P2(CO7)2 (mp-773403) | 0.1658 | 0.212 | 6 |
Na2LiMnPCO7 (mp-774267) | 0.1543 | 0.152 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eV |
PseudopotentialsVASP PAW: Na_pv Li_sv Mn_pv P C O |
Final Energy/Atom-6.7200 eV |
Corrected Energy-375.8263 eV
-375.8263 eV = -349.4388 eV (uncorrected energy) - 19.6641 eV (MP Anion Correction) - 6.7234 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)