Final Magnetic Moment10.002 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.391 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.035 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.82 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToNa3MnPCO7 + MnCO3 + Li3PO4 |
Band Gap3.578 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [1] |
HallP 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
TeO2 (mp-2125) | <1 0 0> | <1 0 1> | 213.3 |
TeO2 (mp-2125) | <1 0 1> | <0 0 1> | 236.9 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 296.1 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 236.9 |
Fe3O4 (mp-19306) | <1 0 0> | <0 0 1> | 296.1 |
Fe3O4 (mp-19306) | <1 1 0> | <1 0 1> | 106.7 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 296.1 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 177.7 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 296.1 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 236.9 |
SiO2 (mp-6930) | <1 1 1> | <1 0 1> | 106.7 |
MgO (mp-1265) | <1 0 0> | <0 1 0> | 274.6 |
TiO2 (mp-2657) | <0 0 1> | <0 0 1> | 177.7 |
TiO2 (mp-2657) | <1 0 0> | <1 0 0> | 266.0 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 59.2 |
TiO2 (mp-2657) | <1 1 1> | <0 0 1> | 59.2 |
C (mp-66) | <1 0 0> | <0 1 0> | 205.9 |
C (mp-66) | <1 1 0> | <0 0 1> | 296.1 |
DyScO3 (mp-31120) | <0 1 1> | <0 1 0> | 274.6 |
InAs (mp-20305) | <1 1 0> | <1 0 1> | 106.7 |
C (mp-66) | <1 1 1> | <0 0 1> | 177.7 |
GdScO3 (mp-5690) | <0 1 1> | <0 1 0> | 274.6 |
GdScO3 (mp-5690) | <1 1 1> | <1 1 0> | 224.7 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 296.1 |
Mg (mp-153) | <1 0 0> | <0 0 1> | 296.1 |
LiF (mp-1138) | <1 1 0> | <1 0 1> | 213.3 |
YVO4 (mp-19133) | <0 0 1> | <0 1 0> | 205.9 |
PbS (mp-21276) | <1 0 0> | <0 1 1> | 183.1 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 296.1 |
Te2Mo (mp-602) | <1 1 1> | <0 0 1> | 296.1 |
InP (mp-20351) | <1 0 0> | <0 1 1> | 183.1 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 1 1> | 255.4 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 177.7 |
GaSe (mp-1943) | <1 1 0> | <0 0 1> | 118.4 |
BN (mp-984) | <1 0 1> | <1 0 0> | 266.0 |
TbScO3 (mp-31119) | <0 1 1> | <0 1 0> | 274.6 |
TbScO3 (mp-31119) | <1 1 1> | <1 1 0> | 224.7 |
Ni (mp-23) | <1 1 1> | <0 0 1> | 296.1 |
InSb (mp-20012) | <1 0 0> | <0 1 1> | 91.6 |
BN (mp-984) | <1 1 0> | <1 0 0> | 266.0 |
PbSe (mp-2201) | <1 1 0> | <1 0 1> | 106.7 |
BaTiO3 (mp-5986) | <0 0 1> | <0 0 1> | 236.9 |
BaTiO3 (mp-5986) | <1 0 1> | <1 0 1> | 213.3 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 296.1 |
SiC (mp-11714) | <0 0 1> | <0 0 1> | 296.1 |
SiC (mp-11714) | <1 0 0> | <0 1 0> | 274.6 |
SiC (mp-11714) | <1 1 0> | <0 1 0> | 274.6 |
CdTe (mp-406) | <1 0 0> | <0 1 1> | 91.6 |
MoSe2 (mp-1634) | <0 0 1> | <0 0 1> | 296.1 |
MoSe2 (mp-1634) | <1 0 0> | <0 1 0> | 205.9 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Na3Ca(BO2)5 (mp-542719) | 0.7402 | 0.000 | 4 |
Na3FeAsCO7 (mp-771494) | 0.3416 | 0.000 | 5 |
Na3MnAsCO7 (mp-771476) | 0.3018 | 0.000 | 5 |
Na3CrAsCO7 (mp-771454) | 0.3079 | 0.038 | 5 |
Na3CuAsCO7 (mp-772153) | 0.3263 | 0.010 | 5 |
Na3CuSiCO7 (mp-771162) | 0.3387 | 0.057 | 5 |
Na2LiMnPCO7 (mp-770672) | 0.1524 | 0.019 | 6 |
Na2LiMnPCO7 (mp-773726) | 0.1247 | 0.025 | 6 |
NaLi2MnPCO7 (mp-773404) | 0.1518 | 0.045 | 6 |
Na3Li3Mn2P2(CO7)2 (mp-773403) | 0.0782 | 0.035 | 6 |
Na2LiMnPCO7 (mp-774267) | 0.1344 | 0.025 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eV |
PseudopotentialsVASP PAW: Na_pv Li_sv Mn_pv P C O |
Final Energy/Atom-6.7515 eV |
Corrected Energy-377.4648 eV
-377.4648 eV = -351.0772 eV (uncorrected energy) - 19.6641 eV (MP Anion Correction) - 6.7234 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)