material

TiSnO4

ID:

mp-773864

DOI:

10.17188/1302191


Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-2.751 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.066 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
4.88 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
SnO2 + TiO2
Band Gap
2.270 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
I4m2 [119]
Hall
I 4 2
Point Group
42m
Crystal System
tetragonal

Electronic Structure

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
GaP (mp-2490) <1 0 0> <0 0 1> 0.000 30.3
Mg (mp-153) <0 0 1> <0 0 1> 0.001 166.8
LiAlO2 (mp-3427) <0 0 1> <0 0 1> 0.004 136.4
GaP (mp-2490) <1 1 0> <1 1 0> 0.008 171.0
CaF2 (mp-2741) <1 0 0> <0 0 1> 0.009 30.3
MoS2 (mp-1434) <0 0 1> <0 0 1> 0.017 166.8
GdScO3 (mp-5690) <1 1 0> <0 0 1> 0.017 257.7
WS2 (mp-224) <0 0 1> <0 0 1> 0.017 166.8
GdScO3 (mp-5690) <1 1 1> <0 0 1> 0.023 288.1
LaF3 (mp-905) <1 0 1> <1 0 0> 0.024 282.1
NdGaO3 (mp-3196) <0 1 0> <1 1 0> 0.026 171.0
C (mp-48) <1 0 0> <1 0 1> 0.026 172.2
MgF2 (mp-1249) <0 0 1> <0 0 1> 0.030 197.1
CaF2 (mp-2741) <1 1 0> <1 1 0> 0.031 171.0
Al2O3 (mp-1143) <0 0 1> <0 0 1> 0.038 318.4
LiTaO3 (mp-3666) <0 0 1> <1 0 0> 0.044 282.1
LiNbO3 (mp-3731) <0 0 1> <1 0 0> 0.051 282.1
KCl (mp-23193) <1 1 0> <1 0 1> 0.051 172.2
InAs (mp-20305) <1 0 0> <0 0 1> 0.052 75.8
TiO2 (mp-2657) <1 0 0> <0 0 1> 0.053 166.8
CaCO3 (mp-3953) <1 1 0> <0 0 1> 0.059 151.6
MgF2 (mp-1249) <1 0 0> <1 0 0> 0.060 161.2
LiAlO2 (mp-3427) <1 0 1> <1 1 0> 0.062 171.0
ZnTe (mp-2176) <1 0 0> <0 0 1> 0.067 75.8
NdGaO3 (mp-3196) <1 1 0> <0 0 1> 0.068 60.6
SrTiO3 (mp-4651) <1 0 1> <1 0 1> 0.074 215.3
Si (mp-149) <1 1 0> <1 1 0> 0.084 171.0
Bi2Te3 (mp-34202) <0 0 1> <1 0 1> 0.089 86.1
CeO2 (mp-20194) <1 1 0> <1 1 0> 0.092 171.0
MgO (mp-1265) <1 1 0> <1 1 0> 0.093 228.0
ZrO2 (mp-2858) <0 0 1> <0 0 1> 0.096 136.4
GdScO3 (mp-5690) <1 0 1> <0 0 1> 0.096 227.4
Ga2O3 (mp-886) <1 0 0> <1 0 0> 0.101 201.5
CsI (mp-614603) <1 1 1> <1 0 1> 0.106 215.3
LiF (mp-1138) <1 1 0> <0 0 1> 0.108 257.7
TiO2 (mp-2657) <0 0 1> <0 0 1> 0.109 197.1
SiC (mp-8062) <1 0 0> <0 0 1> 0.114 75.8
Mg (mp-153) <1 1 1> <1 0 1> 0.115 301.4
Au (mp-81) <1 1 1> <1 0 0> 0.119 120.9
GdScO3 (mp-5690) <0 0 1> <1 0 1> 0.123 129.2
Te2W (mp-22693) <0 1 0> <1 0 0> 0.124 161.2
TeO2 (mp-2125) <1 0 1> <1 1 1> 0.141 235.9
LiGaO2 (mp-5854) <1 0 1> <1 1 0> 0.142 228.0
Ag (mp-124) <1 1 1> <1 0 0> 0.142 120.9
DyScO3 (mp-31120) <0 1 1> <1 0 1> 0.143 215.3
TbScO3 (mp-31119) <0 1 1> <1 0 1> 0.145 215.3
Si (mp-149) <1 0 0> <0 0 1> 0.145 30.3
AlN (mp-661) <1 0 0> <1 1 0> 0.150 171.0
ZrO2 (mp-2858) <0 1 1> <0 0 1> 0.152 318.4
AlN (mp-661) <1 0 1> <1 0 1> 0.153 215.3
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
282 99 130 0 0 0
99 282 130 0 0 0
130 130 208 0 0 0
0 0 0 34 0 0
0 0 0 0 34 0
0 0 0 0 0 43
Compliance Tensor Sij (10-12Pa-1)
5 -0.4 -2.9 0 0 0
-0.4 5 -2.9 0 0 0
-2.9 -2.9 8.4 0 0 0
0 0 0 29.2 0 0
0 0 0 0 29.2 0
0 0 0 0 0 23.4
Shear Modulus GV
50 GPa
Bulk Modulus KV
166 GPa
Shear Modulus GR
44 GPa
Bulk Modulus KR
164 GPa
Shear Modulus GVRH
47 GPa
Bulk Modulus KVRH
165 GPa
Elastic Anisotropy
0.72
Poisson's Ratio
0.37

Piezoelectricity

Reference for tensor and properties: Methodology
Piezoelectric Tensor eij (C/m2)
0.00000 0.00000 0.00000 0.00000 2.37538 0.00000
0.00000 0.00000 0.00000 -2.37538 0.00000 0.00000
-0.18779 0.18779 0.00000 0.00000 0.00000 0.00000
Piezoelectric Modulus ‖eijmax
2.37538 C/m2
Crystallographic Direction vmax
0.00000
1.00000
0.00000

Dielectric Properties

Reference for tensor and properties: Methodology
Dielectric Tensor εij (electronic contribution)
5.55 0.00 0.00
0.00 5.55 0.00
0.00 0.00 5.18
Dielectric Tensor εij (total)
206.31 0.00 0.00
0.00 206.31 0.00
0.00 0.00 14.22
Polycrystalline dielectric constant εpoly
(electronic contribution)
5.43
Polycrystalline dielectric constant εpoly
(total)
142.28
Refractive Index n
2.33
Potentially ferroelectric?
Unknown

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
TiVO4 (mp-780818) 0.2851 0.043 3
TiCrO4 (mp-773450) 0.2090 0.071 3
SnBiO4 (mp-754839) 0.0949 0.089 3
NbFeO4 (mp-774156) 0.2021 0.023 3
TiMnO4 (mp-775296) 0.2630 0.053 3
LiFe5(OF2)4 (mp-782691) 0.3730 0.081 4
AlMo(WO4)2 (mvc-685) 0.5030 0.075 4
AlV(WO4)2 (mvc-704) 0.4833 0.014 4
AlFe(WO4)2 (mvc-836) 0.4910 0.266 4
MnAl(WO4)2 (mvc-648) 0.5003 0.062 4
K2O (mp-684904) 0.2687 0.040 2
ZrO2 (mp-754403) 0.2088 0.015 2
FeO2 (mp-25517) 0.2904 0.477 2
EuN2 (mp-1072167) 0.2753 1.388 2
SnO2 (mp-755071) 0.2808 0.057 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Ti_pv Sn_d O
Final Energy/Atom
-7.5631 eV
Corrected Energy
-48.1879 eV
-48.1879 eV = -45.3787 eV (uncorrected energy) - 2.8092 eV (MP Anion Correction)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
Submitted by

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)