Final Magnetic Moment2.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.247 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.002 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.52 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToSbPO5 + CuP4O11 + Cu(PO3)2 + O2 |
Band Gap0.459 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinR3 [146] |
HallR 3 |
Point Group3 |
Crystal Systemtrigonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 320.4 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 320.4 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 192.2 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 320.4 |
BN (mp-984) | <1 1 0> | <0 0 1> | 64.1 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 64.1 |
SiO2 (mp-6930) | <1 1 0> | <1 0 0> | 189.9 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 256.3 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 192.2 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 64.1 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 256.3 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 320.4 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 192.2 |
LaF3 (mp-905) | <1 0 0> | <0 0 1> | 320.4 |
PbS (mp-21276) | <1 1 1> | <0 0 1> | 64.1 |
InP (mp-20351) | <1 0 0> | <0 0 1> | 320.4 |
InP (mp-20351) | <1 1 0> | <0 0 1> | 256.3 |
Al (mp-134) | <1 1 1> | <0 0 1> | 192.2 |
LiGaO2 (mp-5854) | <0 1 1> | <0 0 1> | 128.2 |
LiGaO2 (mp-5854) | <1 1 0> | <0 0 1> | 192.2 |
Ni (mp-23) | <1 1 1> | <0 0 1> | 64.1 |
MoSe2 (mp-1634) | <0 0 1> | <0 0 1> | 256.3 |
Ge3(BiO3)4 (mp-23560) | <1 1 1> | <0 0 1> | 192.2 |
C (mp-48) | <0 0 1> | <1 0 0> | 189.9 |
WSe2 (mp-1821) | <0 0 1> | <0 0 1> | 256.3 |
WSe2 (mp-1821) | <1 1 1> | <0 0 1> | 256.3 |
LaF3 (mp-905) | <0 0 1> | <0 0 1> | 192.2 |
PbS (mp-21276) | <1 0 0> | <0 0 1> | 320.4 |
PbS (mp-21276) | <1 1 0> | <0 0 1> | 256.3 |
InP (mp-20351) | <1 1 1> | <0 0 1> | 64.1 |
ZrO2 (mp-2858) | <0 1 1> | <0 0 1> | 192.2 |
Ni (mp-23) | <1 1 0> | <0 0 1> | 256.3 |
PbSe (mp-2201) | <1 0 0> | <0 0 1> | 192.2 |
PbSe (mp-2201) | <1 1 1> | <0 0 1> | 64.1 |
BaTiO3 (mp-5986) | <1 1 0> | <1 0 0> | 189.9 |
SiC (mp-11714) | <0 0 1> | <0 0 1> | 256.3 |
CdSe (mp-2691) | <1 0 0> | <0 0 1> | 192.2 |
CdSe (mp-2691) | <1 1 1> | <0 0 1> | 64.1 |
WSe2 (mp-1821) | <1 1 0> | <0 0 1> | 256.3 |
Ge(Bi3O5)4 (mp-23352) | <1 1 1> | <0 0 1> | 192.2 |
CaCO3 (mp-3953) | <1 0 0> | <0 0 1> | 256.3 |
YAlO3 (mp-3792) | <0 1 0> | <0 0 1> | 320.4 |
YAlO3 (mp-3792) | <1 0 0> | <0 0 1> | 320.4 |
SiC (mp-8062) | <1 0 0> | <0 0 1> | 192.2 |
SiC (mp-8062) | <1 1 0> | <0 0 1> | 320.4 |
ZnO (mp-2133) | <0 0 1> | <0 0 1> | 256.3 |
ZnO (mp-2133) | <1 0 0> | <0 0 1> | 320.4 |
GaSb (mp-1156) | <1 0 0> | <0 0 1> | 192.2 |
GaSb (mp-1156) | <1 1 1> | <0 0 1> | 64.1 |
LiAlO2 (mp-3427) | <0 0 1> | <0 0 1> | 320.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
P3(WO6)2 (mp-851036) | 0.1893 | 0.000 | 3 |
Cr2(PO4)3 (mp-540340) | 0.1750 | 0.060 | 3 |
Cr2(PO4)3 (mp-540317) | 0.1899 | 0.061 | 3 |
Cr2(PO4)3 (mp-540211) | 0.1916 | 0.061 | 3 |
V2(PO4)3 (mp-32469) | 0.1891 | 0.015 | 3 |
MnSb3(PO4)6 (mp-775465) | 0.0252 | 0.012 | 4 |
NiSb3(PO4)6 (mp-775231) | 0.0226 | 0.026 | 4 |
VSb3(PO4)6 (mp-775206) | 0.0580 | 0.013 | 4 |
CrSb3(PO4)6 (mp-775202) | 0.0324 | 0.033 | 4 |
FeSb3(PO4)6 (mp-774425) | 0.0423 | 0.000 | 4 |
Cr5O12 (mp-773920) | 0.3965 | 0.000 | 2 |
Nb2O5 (mp-776896) | 0.5773 | 0.059 | 2 |
Mo4O11 (mp-565865) | 0.7093 | 0.005 | 2 |
V5O12 (mp-778252) | 0.4200 | 0.003 | 2 |
Cr3O8 (mp-557959) | 0.7092 | 0.048 | 2 |
VCrP2(O4F)2 (mp-765139) | 0.3790 | 0.041 | 5 |
MgCr3Se2(SO6)4 (mp-769544) | 0.4637 | 0.249 | 5 |
MnVP2(O4F)2 (mp-777435) | 0.3589 | 0.003 | 5 |
MgCr3Se3(SO8)3 (mp-773999) | 0.4602 | 0.263 | 5 |
VFeP2(O4F)2 (mp-778349) | 0.3803 | 0.038 | 5 |
Zr12Si2Bi2P16PbO72 (mp-693759) | 0.6976 | 0.009 | 6 |
LiTi3MnCr(PO4)6 (mp-772224) | 0.6162 | 0.001 | 6 |
NaLiTiAl(PO4)3 (mp-776520) | 0.7005 | 0.023 | 6 |
Na2LiTi3Al(PO4)6 (mp-769074) | 0.6306 | 0.011 | 6 |
Na2LiTi3Al(PO4)6 (mp-769073) | 0.6313 | 0.014 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Cu_pv Sb P O |
Final Energy/Atom-6.6839 eV |
Corrected Energy-244.1079 eV
-244.1079 eV = -227.2530 eV (uncorrected energy) - 16.8550 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)