Final Magnetic Moment6.961 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.248 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.108 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.07 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToV3O5 + Li3VO4 + V2O3 + Ni |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/m [12] |
Hall-C 2y |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 1> | <0 0 1> | 122.7 |
AlN (mp-661) | <1 1 1> | <1 0 -1> | 200.8 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 141.7 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 318.8 |
SiO2 (mp-6930) | <0 0 1> | <1 1 -1> | 213.5 |
SiO2 (mp-6930) | <1 1 0> | <1 1 -1> | 142.3 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 318.8 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 0> | 283.4 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 318.8 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 283.4 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 -1> | 200.8 |
CdS (mp-672) | <0 0 1> | <1 0 0> | 248.0 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 177.1 |
LiF (mp-1138) | <1 1 1> | <1 0 0> | 177.1 |
Te2W (mp-22693) | <0 1 0> | <0 1 1> | 158.9 |
Te2W (mp-22693) | <0 1 1> | <1 0 -1> | 301.2 |
Ag (mp-124) | <1 1 0> | <1 0 -1> | 50.2 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 122.7 |
LiNbO3 (mp-3731) | <1 0 1> | <0 0 1> | 306.9 |
Bi2Se3 (mp-541837) | <1 0 0> | <1 0 0> | 248.0 |
Al (mp-134) | <1 0 0> | <1 0 0> | 141.7 |
Al (mp-134) | <1 1 0> | <1 0 -1> | 200.8 |
LiGaO2 (mp-5854) | <1 0 0> | <0 1 1> | 317.7 |
TeO2 (mp-2125) | <0 0 1> | <1 0 0> | 283.4 |
TeO2 (mp-2125) | <1 0 0> | <0 1 0> | 201.7 |
SiC (mp-7631) | <1 0 1> | <0 1 1> | 238.3 |
LiTaO3 (mp-3666) | <0 0 1> | <0 0 1> | 184.1 |
LiTaO3 (mp-3666) | <1 0 1> | <0 0 1> | 306.9 |
Fe3O4 (mp-19306) | <1 0 0> | <1 0 0> | 70.8 |
MgO (mp-1265) | <1 0 0> | <1 0 0> | 35.4 |
MgO (mp-1265) | <1 1 1> | <0 0 1> | 61.4 |
C (mp-66) | <1 0 0> | <0 0 1> | 306.9 |
C (mp-66) | <1 1 0> | <0 0 1> | 184.1 |
GdScO3 (mp-5690) | <1 0 0> | <1 0 0> | 141.7 |
GdScO3 (mp-5690) | <1 1 0> | <1 0 0> | 318.8 |
Mg (mp-153) | <1 0 0> | <1 0 0> | 177.1 |
Mg (mp-153) | <1 0 1> | <1 0 0> | 212.5 |
PbS (mp-21276) | <1 1 0> | <1 0 -1> | 50.2 |
PbS (mp-21276) | <1 1 1> | <1 0 -1> | 251.0 |
AlN (mp-661) | <0 0 1> | <1 0 0> | 177.1 |
AlN (mp-661) | <1 1 0> | <1 0 -1> | 301.2 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 283.4 |
GaN (mp-804) | <0 0 1> | <1 0 -1> | 251.0 |
GaN (mp-804) | <1 0 0> | <0 1 1> | 238.3 |
GaN (mp-804) | <1 0 1> | <1 0 1> | 173.5 |
GaN (mp-804) | <1 1 0> | <1 0 0> | 318.8 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 283.4 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 318.8 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 141.7 |
LiF (mp-1138) | <1 0 0> | <1 1 1> | 100.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li3Co11O14 (mp-761816) | 0.1505 | 0.271 | 3 |
LiCoO2 (mp-853240) | 0.1514 | 0.075 | 3 |
Li5V7O12 (mp-764746) | 0.1584 | 0.369 | 3 |
Li5Fe11O16 (mp-762692) | 0.1308 | 0.043 | 3 |
LiCoO2 (mp-1097885) | 0.1154 | 0.103 | 3 |
Li4V3CoO8 (mp-771711) | 0.0757 | 0.115 | 4 |
Li2TiVO4 (mp-763993) | 0.0873 | 0.029 | 4 |
Li4TiV3O8 (mp-764005) | 0.1168 | 0.021 | 4 |
Li5Fe5(SbO6)2 (mp-771103) | 0.1198 | 0.055 | 4 |
Li5FeOF5 (mp-777907) | 0.1196 | 0.098 | 4 |
LiTe3 (mp-27466) | 0.2423 | 0.009 | 2 |
Bi2Te3 (mp-568390) | 0.2897 | 0.248 | 2 |
In2Se3 (mp-1068548) | 0.3072 | 0.530 | 2 |
In2Se3 (mp-20830) | 0.2873 | 0.530 | 2 |
Sb2Te3 (mp-1080789) | 0.2788 | 0.129 | 2 |
Na6MnNi3(SbO6)2 (mp-1094109) | 0.5302 | 0.139 | 5 |
Hg (mp-982872) | 0.4508 | 0.020 | 1 |
Sb (mp-632286) | 0.4031 | 0.059 | 1 |
Te (mp-570459) | 0.4549 | 0.044 | 1 |
Te (mp-10654) | 0.4818 | 0.047 | 1 |
Te (mp-105) | 0.3792 | 0.047 | 1 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesV: 3.25 eVNi: 6.2 eV |
PseudopotentialsVASP PAW: Li_sv V_pv Ni_pv O |
Final Energy/Atom-6.4619 eV |
Corrected Energy-116.5267 eV
Uncorrected energy = -103.3897 eV
Composition-based energy adjustment (-0.687 eV/atom x 8.0 atoms) = -5.4960 eV
Composition-based energy adjustment (-1.700 eV/atom x 3.0 atoms) = -5.1000 eV
Composition-based energy adjustment (-2.541 eV/atom x 1.0 atoms) = -2.5410 eV
Corrected energy = -116.5267 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)