Final Magnetic Moment0.073 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-1.731 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.784 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.39 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCr2P2O7 + Cr2O3 |
Band Gap0.060 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPnma [62] |
Hall-P 2ac 2n |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <0 0 1> | 64.0 |
AlN (mp-661) | <1 0 1> | <0 1 0> | 281.5 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 192.0 |
BaF2 (mp-1029) | <1 1 0> | <0 1 1> | 113.6 |
GaN (mp-804) | <1 0 0> | <1 0 1> | 168.2 |
SiO2 (mp-6930) | <1 0 0> | <1 0 1> | 168.2 |
KCl (mp-23193) | <1 0 0> | <0 1 0> | 281.5 |
KCl (mp-23193) | <1 1 0> | <0 1 1> | 113.6 |
CdS (mp-672) | <0 0 1> | <0 1 1> | 227.1 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 256.0 |
InAs (mp-20305) | <1 0 0> | <0 1 1> | 113.6 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 320.0 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 256.0 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 320.0 |
Te2W (mp-22693) | <1 0 0> | <0 1 0> | 93.8 |
Te2W (mp-22693) | <1 0 1> | <0 0 1> | 192.0 |
Te2Mo (mp-602) | <1 1 0> | <0 1 0> | 93.8 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 320.0 |
YVO4 (mp-19133) | <1 0 0> | <0 1 1> | 227.1 |
YVO4 (mp-19133) | <1 1 0> | <0 0 1> | 64.0 |
YVO4 (mp-19133) | <1 1 1> | <1 0 1> | 168.2 |
BN (mp-984) | <1 0 0> | <1 0 0> | 155.6 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 192.0 |
Te2Mo (mp-602) | <1 1 1> | <0 0 1> | 192.0 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 256.0 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 1 1> | 227.1 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 320.0 |
SiC (mp-7631) | <1 0 0> | <0 1 0> | 93.8 |
SiC (mp-7631) | <1 0 1> | <0 0 1> | 192.0 |
MoS2 (mp-1434) | <0 0 1> | <0 1 0> | 281.5 |
LiGaO2 (mp-5854) | <0 0 1> | <1 0 1> | 168.2 |
Fe3O4 (mp-19306) | <1 0 0> | <0 1 1> | 227.1 |
MgO (mp-1265) | <1 1 0> | <1 0 0> | 155.6 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 320.0 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 256.0 |
Mg (mp-153) | <0 0 1> | <0 1 0> | 281.5 |
C (mp-66) | <1 1 0> | <0 0 1> | 320.0 |
Mg (mp-153) | <1 0 0> | <1 0 1> | 168.2 |
Mg (mp-153) | <1 1 0> | <0 0 1> | 320.0 |
PbS (mp-21276) | <1 1 0> | <1 0 0> | 155.6 |
LaF3 (mp-905) | <0 0 1> | <0 1 1> | 227.1 |
Ni (mp-23) | <1 0 0> | <0 0 1> | 256.0 |
PbSe (mp-2201) | <1 0 0> | <0 1 1> | 113.6 |
PbSe (mp-2201) | <1 1 0> | <0 1 0> | 281.5 |
Ni (mp-23) | <1 1 0> | <1 0 0> | 155.6 |
BaTiO3 (mp-5986) | <1 0 0> | <0 0 1> | 256.0 |
BaTiO3 (mp-5986) | <1 0 1> | <0 0 1> | 256.0 |
SiC (mp-11714) | <0 0 1> | <0 0 1> | 320.0 |
SiC (mp-11714) | <1 0 0> | <0 0 1> | 64.0 |
Au (mp-81) | <1 0 0> | <0 0 1> | 256.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Cu4(PO4)3 (mp-26742) | 0.5193 | 0.028 | 3 |
Cr4(PO4)3 (mp-705240) | 0.0220 | 0.784 | 3 |
Cr3(PO4)2 (mp-579247) | 0.5782 | 0.089 | 3 |
Na2Si3O7 (mp-556198) | 0.5929 | 0.016 | 3 |
Cr4(PO4)3 (mp-773959) | 0.0290 | 0.784 | 3 |
MgCuP2O7 (mvc-5496) | 0.5144 | 0.030 | 4 |
LiCrPO4 (mp-761385) | 0.5163 | 0.093 | 4 |
Li3Sb5(PO4)6 (mp-26281) | 0.5102 | 0.019 | 4 |
ZnCr2(PO4)2 (mvc-10010) | 0.5098 | 0.149 | 4 |
ZnCu2(PO4)2 (mvc-9496) | 0.4161 | 0.053 | 4 |
Na3LiMg4(Si2O5)6 (mp-695366) | 0.7098 | 0.710 | 5 |
NaCaGaSi2O7 (mp-698690) | 0.6700 | 0.666 | 5 |
Na6Al4Fe(Si4O13)2 (mp-42298) | 0.6955 | 0.000 | 5 |
LiCu2P3(HO5)2 (mp-849424) | 0.7208 | 0.071 | 5 |
Na6Al4Fe(Si4O13)2 (mp-705484) | 0.6647 | 0.033 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesCr: 3.7 eV |
PseudopotentialsVASP PAW: Cr_pv P O |
Final Energy/Atom-6.8761 eV |
Corrected Energy-588.5038 eV
-588.5038 eV = -522.5859 eV (uncorrected energy) - 33.7099 eV (MP Anion Correction) - 32.2080 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)