Final Magnetic Moment52.993 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.044 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom< 0.001 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.10 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiMn2O4 + Li2Mn3NiO8 |
Band Gap0.677 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinR32 [155] |
HallR 3 2" |
Point Group32 |
Crystal Systemtrigonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 243.8 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 121.9 |
Al (mp-134) | <1 0 0> | <0 0 1> | 243.8 |
Fe3O4 (mp-19306) | <1 1 1> | <0 0 1> | 121.9 |
Au (mp-81) | <1 1 1> | <0 0 1> | 121.9 |
ZnO (mp-2133) | <0 0 1> | <0 0 1> | 121.9 |
MgAl2O4 (mp-3536) | <1 1 1> | <0 0 1> | 121.9 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li11Mn13O32 (mp-698600) | 0.1569 | 0.004 | 3 |
Li4Mn5O12 (mp-691115) | 0.1659 | 0.000 | 3 |
Li7Mn8O20 (mp-769440) | 0.1531 | 0.020 | 3 |
Mn5(FeO3)4 (mp-763271) | 0.1737 | 0.072 | 3 |
LiMn2O4 (mp-1097867) | 0.1720 | 0.000 | 3 |
Li9Mn12Cu3O32 (mp-769514) | 0.1577 | 0.019 | 4 |
Li9Mn12Ni3O32 (mp-769460) | 0.0999 | 0.000 | 4 |
Li2Ti3FeO8 (mp-775306) | 0.1644 | 0.005 | 4 |
Li2Mn3CuO8 (mp-774001) | 0.1646 | 0.008 | 4 |
Li2Mn3CuO8 (mp-775165) | 0.1627 | 0.030 | 4 |
Co3O4 (mp-559191) | 0.3607 | 0.010 | 2 |
In3S4 (mp-556597) | 0.3532 | 0.042 | 2 |
Co3O4 (mp-18748) | 0.3592 | 0.010 | 2 |
Ni3S4 (mp-1050) | 0.3580 | 0.000 | 2 |
Sn3N4 (mp-16031) | 0.3590 | 0.000 | 2 |
Li14Mn22Cr3Cu3O56 (mp-735790) | 0.2734 | 0.019 | 5 |
Li4Ti3Mn3(NiO8)2 (mp-770507) | 0.2925 | 0.061 | 5 |
Li4Mn3Cr3(CuO8)2 (mp-765456) | 0.2888 | 0.080 | 5 |
TaTi9Al3Zn23O48 (mp-686614) | 0.2812 | 0.054 | 5 |
TaTi9Al3Zn23O48 (mp-695545) | 0.2499 | 0.053 | 5 |
Li3MnFeCo(PO4)3 (mp-764809) | 0.7460 | 0.015 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eVNi: 6.2 eV |
PseudopotentialsVASP PAW: Li_sv Mn_pv Ni_pv O |
Final Energy/Atom-6.8114 eV |
Corrected Energy-431.2859 eV
-431.2859 eV = -381.4359 eV (uncorrected energy) - 27.3768 eV (MP Advanced Correction) - 22.4733 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)