Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.191 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.213 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.86 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToSbPO4 + SbPO5 + Mn2P2O7 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPm [6] |
HallP 2y |
Point Groupm |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 1 1> | 306.5 |
AlN (mp-661) | <0 0 1> | <0 1 1> | 306.5 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 167.2 |
AlN (mp-661) | <1 0 1> | <1 0 1> | 232.1 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 133.8 |
CeO2 (mp-20194) | <1 1 1> | <1 0 1> | 154.8 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 167.2 |
GaN (mp-804) | <1 0 0> | <0 1 1> | 306.5 |
GaN (mp-804) | <1 0 1> | <0 1 1> | 306.5 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 301.0 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 301.0 |
SiO2 (mp-6930) | <0 0 1> | <1 0 1> | 154.8 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 133.8 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 0> | 256.8 |
DyScO3 (mp-31120) | <0 1 0> | <0 1 1> | 306.5 |
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 267.6 |
DyScO3 (mp-31120) | <1 1 0> | <0 1 0> | 256.8 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 0> | 256.8 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 1> | 232.1 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 200.7 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 167.2 |
CdS (mp-672) | <1 0 1> | <1 1 0> | 258.1 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 100.3 |
Te2W (mp-22693) | <0 0 1> | <0 1 0> | 256.8 |
Te2W (mp-22693) | <0 1 1> | <1 1 0> | 172.1 |
Te2W (mp-22693) | <1 0 0> | <0 1 1> | 306.5 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 267.6 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 200.7 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 0 1> | 154.8 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 100.3 |
GaSe (mp-1943) | <1 1 0> | <1 0 1> | 232.1 |
GaSe (mp-1943) | <1 1 1> | <1 0 1> | 232.1 |
BN (mp-984) | <0 0 1> | <0 1 0> | 256.8 |
BN (mp-984) | <1 1 0> | <0 1 1> | 306.5 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 167.2 |
Al (mp-134) | <1 0 0> | <0 1 0> | 256.8 |
Al (mp-134) | <1 1 0> | <1 0 1> | 232.1 |
Al (mp-134) | <1 1 1> | <0 0 1> | 200.7 |
LiGaO2 (mp-5854) | <0 1 1> | <1 1 0> | 86.0 |
LiGaO2 (mp-5854) | <1 1 0> | <0 0 1> | 334.5 |
LiGaO2 (mp-5854) | <1 1 1> | <1 1 1> | 278.6 |
CdTe (mp-406) | <1 1 0> | <1 0 1> | 309.5 |
SiC (mp-7631) | <0 0 1> | <0 1 0> | 205.5 |
MgO (mp-1265) | <1 0 0> | <1 1 0> | 258.1 |
MgO (mp-1265) | <1 1 0> | <1 1 0> | 258.1 |
TiO2 (mp-2657) | <0 0 1> | <0 0 1> | 301.0 |
TiO2 (mp-2657) | <1 1 1> | <1 0 1> | 232.1 |
GdScO3 (mp-5690) | <1 1 0> | <0 1 0> | 256.8 |
Mg (mp-153) | <1 1 0> | <0 0 1> | 301.0 |
Mg (mp-153) | <1 1 1> | <0 0 1> | 301.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
MnCrO4 (mp-780641) | 0.4757 | 0.104 | 3 |
Fe3(P2O7)2 (mvc-12221) | 0.4837 | 0.327 | 3 |
Mn3(P2O7)2 (mp-694554) | 0.4733 | 0.162 | 3 |
Fe3(P2O7)2 (mp-540486) | 0.4817 | 0.327 | 3 |
Ni2P3O10 (mp-25610) | 0.4793 | 0.052 | 3 |
CuSb(PO4)2 (mp-755148) | 0.3300 | 0.074 | 4 |
Mn3Sn(PO4)4 (mp-775053) | 0.3376 | 0.019 | 4 |
MnNb(PO4)2 (mp-775045) | 0.3164 | 0.093 | 4 |
NiTe(PO4)2 (mp-778639) | 0.2463 | 0.048 | 4 |
MnSn3(PO4)4 (mp-771800) | 0.3039 | 0.070 | 4 |
MnFeCo(PO4)3 (mp-764410) | 0.3838 | 0.028 | 5 |
MnFeCo(PO4)3 (mp-764392) | 0.4061 | 0.029 | 5 |
MnFeCo(PO4)3 (mp-763496) | 0.4035 | 0.028 | 5 |
MnFeCo(PO4)3 (mp-764415) | 0.3902 | 0.300 | 5 |
MnFeCo(PO4)3 (mp-763446) | 0.4177 | 0.333 | 5 |
InBP2H5NO9 (mp-752709) | 0.6809 | 0.000 | 6 |
LiMgCr3Se2(SO6)4 (mp-769552) | 0.6983 | 0.257 | 6 |
K3Na3TeP6(HO4)6 (mp-720804) | 0.7045 | 0.030 | 6 |
Na3CaSc3Zn(SiO3)8 (mp-720987) | 0.7104 | 0.230 | 6 |
NaLiMn2Fe4(PO4)6 (mp-777193) | 0.6830 | 0.018 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eV |
PseudopotentialsVASP PAW: Mn_pv Sb P O |
Final Energy/Atom-6.7513 eV |
Corrected Energy-174.9495 eV
-174.9495 eV = -162.0320 eV (uncorrected energy) - 11.2366 eV (MP Anion Correction) - 1.6809 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)