Final Magnetic Moment3.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.956 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.058 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.89 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi2Ti3CoO8 |
Band Gap1.005 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinR3m [166] |
Hall-R 3 2" |
Point Group3m |
Crystal Systemtrigonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 0 1> | 215.6 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 123.2 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 277.1 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 215.6 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 215.6 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 170.8 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 338.7 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 215.6 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 246.3 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 154.0 |
Te2Mo (mp-602) | <1 0 1> | <1 0 1> | 272.3 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 154.0 |
BN (mp-984) | <0 0 1> | <0 0 1> | 215.6 |
BN (mp-984) | <1 1 0> | <1 0 1> | 272.3 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 92.4 |
LiNbO3 (mp-3731) | <1 1 0> | <1 0 0> | 256.1 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 277.1 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 215.6 |
LiTaO3 (mp-3666) | <0 0 1> | <0 0 1> | 92.4 |
LiTaO3 (mp-3666) | <1 0 0> | <1 1 0> | 147.9 |
LiTaO3 (mp-3666) | <1 1 0> | <1 0 0> | 256.1 |
Fe3O4 (mp-19306) | <1 1 1> | <0 0 1> | 123.2 |
MgO (mp-1265) | <1 0 0> | <1 0 1> | 90.8 |
MgO (mp-1265) | <1 1 0> | <1 0 1> | 181.5 |
MgO (mp-1265) | <1 1 1> | <0 0 1> | 30.8 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 215.6 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 154.0 |
TiO2 (mp-2657) | <1 1 1> | <0 0 1> | 338.7 |
C (mp-66) | <1 0 0> | <0 0 1> | 154.0 |
C (mp-66) | <1 1 0> | <0 0 1> | 215.6 |
C (mp-66) | <1 1 1> | <0 0 1> | 92.4 |
GdScO3 (mp-5690) | <0 0 1> | <1 0 0> | 256.1 |
GdScO3 (mp-5690) | <1 0 0> | <0 0 1> | 246.3 |
GdScO3 (mp-5690) | <1 0 1> | <1 0 0> | 170.8 |
Mg (mp-153) | <0 0 1> | <0 0 1> | 215.6 |
Mg (mp-153) | <1 0 0> | <1 0 1> | 181.5 |
Mg (mp-153) | <1 0 1> | <1 0 0> | 170.8 |
Mg (mp-153) | <1 1 0> | <0 0 1> | 277.1 |
PbS (mp-21276) | <1 0 0> | <1 0 1> | 181.5 |
PbS (mp-21276) | <1 1 0> | <0 0 1> | 246.3 |
GaP (mp-2490) | <1 1 1> | <0 0 1> | 215.6 |
InP (mp-20351) | <1 0 0> | <1 0 1> | 181.5 |
InP (mp-20351) | <1 1 0> | <1 1 0> | 147.9 |
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 215.6 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 215.6 |
Ni (mp-23) | <1 0 0> | <1 1 0> | 147.9 |
Ni (mp-23) | <1 1 1> | <0 0 1> | 277.1 |
InSb (mp-20012) | <1 1 1> | <0 0 1> | 215.6 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 277.1 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 338.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Y(FeO2)2 (mvc-11640) | 0.1041 | 0.567 | 3 |
CaGd2O4 (mp-752679) | 0.1146 | 0.056 | 3 |
Cr2NiO4 (mp-566016) | 0.1071 | 0.008 | 3 |
CaTb2O4 (mp-755044) | 0.1147 | 0.048 | 3 |
YTi2O4 (mvc-13097) | 0.1024 | 0.248 | 3 |
Li2Mn3FeO8 (mp-773283) | 0.0747 | 0.025 | 4 |
Li2TiCo3O8 (mp-775109) | 0.0706 | 0.206 | 4 |
Li2V3FeO8 (mp-773440) | 0.0588 | 0.065 | 4 |
Li2Ti3FeO8 (mp-775530) | 0.0310 | 0.072 | 4 |
Li2Mn3VO8 (mp-772730) | 0.0731 | 0.072 | 4 |
Co3O4 (mp-559191) | 0.1874 | 0.046 | 2 |
In3S4 (mp-556597) | 0.1621 | 0.042 | 2 |
Co3O4 (mp-18748) | 0.1475 | 0.046 | 2 |
Sn3N4 (mp-16031) | 0.1783 | 0.000 | 2 |
Ge3N4 (mp-476) | 0.2069 | 0.109 | 2 |
Li4Cr2Fe3Co3O16 (mp-775698) | 0.3532 | 0.897 | 5 |
Li4Mn2Fe3Co3O16 (mp-761441) | 0.3601 | 0.078 | 5 |
Li14Mn22Cr3Cu3O56 (mp-735790) | 0.3293 | 0.014 | 5 |
Li4Mn3Cr3(CuO8)2 (mp-765456) | 0.3288 | 0.069 | 5 |
Li4Cr3Cu3(SbO8)2 (mp-783908) | 0.3614 | 0.035 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesCo: 3.32 eV |
PseudopotentialsVASP PAW: Li_sv Ti_pv Co O |
Final Energy/Atom-7.7208 eV |
Corrected Energy-115.5841 eV
-115.5841 eV = -108.0918 eV (uncorrected energy) - 5.6183 eV (MP Anion Correction) - 1.8740 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)