Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingAFM |
Formation Energy / Atom-2.517 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.055 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.28 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiNbO3 + FeO |
Band Gap0.788 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinImma [74] |
Hall-I 2b 2 |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <0 1 0> | 276.0 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 348.6 |
LaAlO3 (mp-2920) | <0 0 1> | <0 1 1> | 202.3 |
AlN (mp-661) | <0 0 1> | <0 1 1> | 67.4 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 154.9 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 309.8 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 38.7 |
BaF2 (mp-1029) | <1 1 0> | <0 1 0> | 55.2 |
CeO2 (mp-20194) | <1 1 0> | <0 1 0> | 165.6 |
BaF2 (mp-1029) | <1 1 1> | <0 1 0> | 276.0 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 309.8 |
GaN (mp-804) | <1 0 1> | <0 1 1> | 134.9 |
SiO2 (mp-6930) | <1 1 1> | <1 1 1> | 261.8 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 38.7 |
GaN (mp-804) | <1 1 0> | <0 1 0> | 331.3 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 154.9 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 193.6 |
KCl (mp-23193) | <1 1 0> | <0 1 0> | 55.2 |
KCl (mp-23193) | <1 1 1> | <0 1 0> | 276.0 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 0> | 331.3 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 348.6 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 309.8 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 38.7 |
InAs (mp-20305) | <1 1 0> | <0 1 0> | 55.2 |
InAs (mp-20305) | <1 1 1> | <0 1 0> | 276.0 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 309.8 |
CdS (mp-672) | <0 0 1> | <1 0 1> | 135.2 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 154.9 |
Te2W (mp-22693) | <0 0 1> | <0 1 0> | 110.4 |
Te2W (mp-22693) | <1 0 0> | <0 0 1> | 193.6 |
Te2W (mp-22693) | <1 0 1> | <0 0 1> | 193.6 |
YVO4 (mp-19133) | <1 0 0> | <0 1 1> | 134.9 |
YVO4 (mp-19133) | <1 1 0> | <0 0 1> | 193.6 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 348.6 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 193.6 |
Te2Mo (mp-602) | <1 1 0> | <0 0 1> | 193.6 |
Te2Mo (mp-602) | <1 1 1> | <0 0 1> | 193.6 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 154.9 |
Ag (mp-124) | <1 1 0> | <0 1 0> | 220.8 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 271.1 |
BN (mp-984) | <0 0 1> | <1 1 1> | 87.3 |
BN (mp-984) | <1 0 1> | <0 0 1> | 309.8 |
BN (mp-984) | <1 1 0> | <0 0 1> | 271.1 |
BN (mp-984) | <1 1 1> | <0 0 1> | 271.1 |
LiNbO3 (mp-3731) | <0 0 1> | <1 1 0> | 234.6 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 1 1> | 134.9 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 309.8 |
MoS2 (mp-1434) | <1 0 0> | <0 0 1> | 271.1 |
MoS2 (mp-1434) | <1 0 1> | <0 0 1> | 271.1 |
LiGaO2 (mp-5854) | <1 0 0> | <0 0 1> | 309.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ti(FeO2)2 (mp-690090) | 0.1152 | 0.020 | 3 |
Mn2ZnO4 (mvc-6911) | 0.0892 | 0.103 | 3 |
MgMn2O4 (mvc-6916) | 0.1057 | 0.047 | 3 |
Ti(FeO2)2 (mp-33684) | 0.0857 | 0.020 | 3 |
Mn2NiO4 (mp-690523) | 0.1114 | 0.012 | 3 |
LiMnNbO4 (mp-769557) | 0.1266 | 0.080 | 4 |
LiNbCoO4 (mp-775532) | 0.1004 | 0.062 | 4 |
LiCoSbO4 (mp-773544) | 0.1159 | 0.000 | 4 |
LiFeSbO4 (mp-776869) | 0.1329 | 0.000 | 4 |
LiFeCoO4 (mp-761710) | 0.1340 | 0.014 | 4 |
Hf3N4 (mp-755988) | 0.2927 | 0.016 | 2 |
Zr3N4 (mp-754381) | 0.2939 | 0.035 | 2 |
In3S4 (mp-556597) | 0.2820 | 0.042 | 2 |
Sn3N4 (mp-16031) | 0.2837 | 0.000 | 2 |
Ge3N4 (mp-476) | 0.2898 | 0.109 | 2 |
Li14Mn22Cr3Cu3O56 (mp-735790) | 0.2900 | 0.014 | 5 |
Li4Mn3Cr3(CuO8)2 (mp-765456) | 0.2940 | 0.069 | 5 |
Li4Fe3Co3(TeO8)2 (mp-849468) | 0.3027 | 0.067 | 5 |
TaTi9Al3Zn23O48 (mp-686614) | 0.3033 | 0.055 | 5 |
TaTi9Al3Zn23O48 (mp-695545) | 0.2795 | 0.054 | 5 |
Li3MnFeCo(PO4)3 (mp-764809) | 0.6943 | 0.014 | 6 |
Li3MnFeCo(PO4)3 (mp-764869) | 0.6987 | 0.032 | 6 |
Li3MnFeCo(PO4)3 (mp-764707) | 0.7038 | 0.035 | 6 |
Li3MnFeCo(PO4)3 (mp-764969) | 0.6977 | 0.057 | 6 |
Li3MnFeCo(PO4)3 (mp-764870) | 0.7021 | 0.466 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesFe: 5.3 eV |
PseudopotentialsVASP PAW: Li_sv Nb_pv Fe_pv O |
Final Energy/Atom-7.4780 eV |
Corrected Energy-115.7764 eV
-115.7764 eV = -104.6921 eV (uncorrected energy) - 5.6183 eV (MP Anion Correction) - 5.4660 eV (MP Advanced Correction)
|