Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-2.406 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.010 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.53 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi2V3SbO8 |
Band Gap1.568 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP63mc [186] |
HallP 6c 2c |
Point Group6mm |
Crystal Systemhexagonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 218.5 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 218.5 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 235.2 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 124.8 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 218.5 |
GaAs (mp-2534) | <1 1 0> | <1 0 1> | 332.9 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 218.5 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 280.9 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 218.5 |
GaN (mp-804) | <1 0 0> | <1 1 0> | 101.9 |
GaN (mp-804) | <1 0 1> | <1 0 1> | 133.2 |
GaN (mp-804) | <1 1 0> | <1 0 1> | 266.3 |
GaN (mp-804) | <1 1 1> | <1 0 1> | 332.9 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 218.5 |
Al (mp-134) | <1 0 0> | <0 0 1> | 249.7 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 280.9 |
SiO2 (mp-6930) | <1 0 0> | <1 0 1> | 332.9 |
SiO2 (mp-6930) | <1 1 1> | <1 0 1> | 266.3 |
LiGaO2 (mp-5854) | <0 1 0> | <1 0 0> | 235.2 |
LiGaO2 (mp-5854) | <0 1 1> | <0 0 1> | 343.3 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 218.5 |
SiC (mp-7631) | <1 0 0> | <1 0 0> | 235.2 |
MgO (mp-1265) | <1 0 0> | <1 0 0> | 176.4 |
MgO (mp-1265) | <1 1 0> | <0 0 1> | 124.8 |
MgO (mp-1265) | <1 1 1> | <0 0 1> | 31.2 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 187.3 |
InAs (mp-20305) | <1 1 0> | <1 0 1> | 266.3 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 280.9 |
ZnSe (mp-1190) | <1 1 0> | <1 0 1> | 332.9 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 218.5 |
TiO2 (mp-2657) | <1 1 1> | <0 0 1> | 343.3 |
C (mp-66) | <1 0 0> | <0 0 1> | 156.1 |
C (mp-66) | <1 1 1> | <0 0 1> | 93.6 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 0> | 203.7 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 280.9 |
CdS (mp-672) | <1 0 0> | <1 0 1> | 199.7 |
CdS (mp-672) | <1 0 1> | <1 0 0> | 294.0 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 249.7 |
LiF (mp-1138) | <1 1 0> | <1 0 1> | 332.9 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 156.1 |
YVO4 (mp-19133) | <1 1 0> | <1 1 0> | 203.7 |
PbS (mp-21276) | <1 0 0> | <1 0 0> | 176.4 |
PbS (mp-21276) | <1 1 0> | <0 0 1> | 249.7 |
GaP (mp-2490) | <1 1 1> | <0 0 1> | 218.5 |
TePb (mp-19717) | <1 1 1> | <0 0 1> | 218.5 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 280.9 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 280.9 |
Te2Mo (mp-602) | <1 1 1> | <0 0 1> | 93.6 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 156.1 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 124.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li(FeO2)2 (mp-771571) | 0.2130 | 0.665 | 3 |
LiCr2O4 (mp-771523) | 0.2253 | 0.088 | 3 |
Co7(SbO6)2 (mp-705595) | 0.2211 | 0.000 | 3 |
LiTi2O4 (mp-776170) | 0.1341 | 0.042 | 3 |
Co2SnO4 (mp-706412) | 0.2225 | 0.053 | 3 |
Li2Cr3WO8 (mp-775271) | 0.1108 | 0.056 | 4 |
Li2V3WO8 (mp-775204) | 0.0889 | 0.064 | 4 |
Li2NbV3O8 (mp-777682) | 0.1157 | 0.000 | 4 |
Li2Cr3SbO8 (mp-772283) | 0.0866 | 0.003 | 4 |
Li2Fe3SbO8 (mp-772280) | 0.0724 | 0.000 | 4 |
Fe3O4 (mp-715491) | 0.2795 | 0.017 | 2 |
Fe3O4 (mp-542433) | 0.2797 | 0.075 | 2 |
Cr3N4 (mp-1014358) | 0.2527 | 0.226 | 2 |
Fe3O4 (mp-650112) | 0.2762 | 0.060 | 2 |
Fe3O4 (mp-715558) | 0.2966 | 0.785 | 2 |
Li4V3Cr3(SbO8)2 (mp-777249) | 0.1012 | 0.037 | 5 |
Li2Cr2FeSbO8 (mp-861530) | 0.0947 | 4.856 | 5 |
Li4Fe3Co3(SbO8)2 (mp-762171) | 0.1339 | 6.482 | 5 |
Li4V3Cr3(WO8)2 (mp-772356) | 0.1168 | 0.006 | 5 |
Li4Cr3Fe3(SbO8)2 (mp-771925) | 0.0852 | 6.495 | 5 |
Li3MnFeCo(PO4)3 (mp-764931) | 0.6632 | 0.017 | 6 |
Li3MnFeCo(PO4)3 (mp-764809) | 0.6537 | 0.014 | 6 |
Li3MnFeCo(PO4)3 (mp-764869) | 0.6586 | 0.032 | 6 |
Li3MnFeCo(PO4)3 (mp-764969) | 0.6587 | 0.057 | 6 |
Li3MnFeCo(PO4)3 (mp-764870) | 0.6614 | 0.466 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesV: 3.25 eV |
PseudopotentialsVASP PAW: Li_sv V_pv Sb O |
Final Energy/Atom-6.9852 eV |
Corrected Energy-216.9130 eV
-216.9130 eV = -195.5844 eV (uncorrected energy) - 11.2366 eV (MP Anion Correction) - 10.0920 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)