material

FeHO2

ID:

mp-774147

DOI:

10.17188/1302386


Material Details

Final Magnetic Moment
5.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
FM
Formation Energy / Atom
-1.628 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.072 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
3.79 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Fe2O3 + H2O
Band Gap
2.119 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P3m1 [156]
Hall
P 3 2"
Point Group
3m
Crystal System
trigonal

Band Structure

Density of States
Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

sign indicates spin ↑ ↓

  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
Mg (mp-153) <1 0 1> <1 0 0> -0.105 131.5
C (mp-66) <1 0 0> <1 0 0> -0.057 102.3
GaSe (mp-1943) <1 0 1> <1 0 0> -0.041 277.7
BN (mp-984) <1 1 0> <1 0 0> -0.014 233.9
C (mp-48) <1 0 1> <1 0 0> -0.013 160.8
MoSe2 (mp-1634) <1 1 1> <1 1 1> -0.005 266.1
C (mp-48) <1 1 0> <1 0 0> -0.004 233.9
GaAs (mp-2534) <1 1 1> <0 0 1> 0.000 57.3
Bi2Se3 (mp-541837) <0 0 1> <0 0 1> 0.000 106.4
BaTiO3 (mp-5986) <0 0 1> <1 0 0> 0.000 175.4
Si (mp-149) <1 1 1> <0 0 1> 0.000 155.5
CeO2 (mp-20194) <1 1 1> <0 0 1> 0.001 155.5
BaF2 (mp-1029) <1 1 1> <0 0 1> 0.002 204.7
SiO2 (mp-6930) <1 0 1> <1 0 0> 0.003 248.5
Ga2O3 (mp-886) <1 1 0> <1 1 1> 0.003 292.7
Te2Mo (mp-602) <1 0 0> <0 0 1> 0.004 163.7
WS2 (mp-224) <1 0 0> <1 1 0> 0.004 227.8
ZnSe (mp-1190) <1 1 1> <0 0 1> 0.005 57.3
Ge (mp-32) <1 1 1> <0 0 1> 0.006 57.3
C (mp-66) <1 1 1> <0 0 1> 0.007 155.5
CdWO4 (mp-19387) <0 0 1> <1 0 1> 0.007 184.3
MoS2 (mp-1434) <1 0 0> <1 1 0> 0.008 202.5
Ga2O3 (mp-886) <1 0 -1> <0 0 1> 0.010 114.6
Te2W (mp-22693) <1 0 0> <1 0 0> 0.010 292.3
Te2Mo (mp-602) <0 0 1> <0 0 1> 0.010 32.7
CaCO3 (mp-3953) <0 0 1> <0 0 1> 0.011 155.5
ZrO2 (mp-2858) <1 1 1> <0 0 1> 0.012 204.7
CsI (mp-614603) <1 1 1> <0 0 1> 0.012 106.4
CdS (mp-672) <1 0 1> <1 0 0> 0.013 131.5
YVO4 (mp-19133) <1 0 0> <1 1 0> 0.014 227.8
WS2 (mp-224) <0 0 1> <0 0 1> 0.015 106.4
MoS2 (mp-1434) <0 0 1> <0 0 1> 0.015 106.4
InSb (mp-20012) <1 1 0> <1 0 1> 0.015 251.3
ZrO2 (mp-2858) <1 1 -1> <1 0 0> 0.017 277.7
CdTe (mp-406) <1 1 0> <1 0 1> 0.020 251.3
BN (mp-984) <1 0 0> <0 0 1> 0.022 155.5
BaTiO3 (mp-5986) <1 0 1> <0 0 1> 0.022 163.7
NdGaO3 (mp-3196) <1 1 1> <1 1 0> 0.024 202.5
Ga2O3 (mp-886) <1 0 0> <1 0 0> 0.025 73.1
Bi2Te3 (mp-34202) <0 0 1> <0 0 1> 0.028 155.5
TePb (mp-19717) <1 0 0> <1 0 1> 0.028 217.8
CdS (mp-672) <0 0 1> <0 0 1> 0.028 106.4
TeO2 (mp-2125) <1 1 0> <1 0 0> 0.028 292.3
CeO2 (mp-20194) <1 1 0> <1 0 1> 0.029 83.8
WS2 (mp-224) <1 0 1> <1 0 0> 0.030 277.7
ZnO (mp-2133) <1 0 0> <1 1 1> 0.031 53.2
Si (mp-149) <1 1 0> <1 0 1> 0.031 83.8
CdWO4 (mp-19387) <0 1 1> <1 0 0> 0.034 160.8
MoS2 (mp-1434) <1 1 1> <1 1 1> 0.035 239.5
Al2O3 (mp-1143) <1 0 1> <1 0 0> 0.038 131.5
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
225 68 6 7 0 0
68 225 6 -7 0 0
6 6 56 0 0 0
7 -7 0 -16 0 0
0 0 0 0 -16 7
0 0 0 0 7 79
Compliance Tensor Sij (10-12Pa-1)
4.8 -1.4 -0.3 2.6 0 0
-1.4 4.8 -0.3 -2.6 0 0
-0.3 -0.3 18 0 0 0
2.6 -2.6 0 -58.5 0 0
0 0 0 0 -58.5 5.2
0 0 0 0 5.2 12.3
Shear Modulus GV
38 GPa
Bulk Modulus KV
74 GPa
Shear Modulus GR
-77 GPa
Bulk Modulus KR
43 GPa
Shear Modulus GVRH
-20 GPa
Bulk Modulus KVRH
58 GPa
Elastic Anisotropy
-6.72
Poisson's Ratio
0.69

Piezoelectricity

Reference for tensor and properties: Methodology
Piezoelectric Tensor eij (C/m2)
0.00000 0.00000 0.00000 0.00000 0.74154 0.14997
0.14997 -0.14997 0.00000 0.74154 0.00000 0.00000
0.50364 0.50364 0.92595 0.00000 0.00000 0.00000
Piezoelectric Modulus ‖eijmax
0.92595 C/m2
Crystallographic Direction vmax
0.00000
0.00000
1.00000

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA+U
Energy Cutoff
520 eV
# of K-points
196
U Values
Fe: 5.3 eV
Pseudopotentials
VASP PAW: Fe_pv H O
Final Energy/Atom
-5.9863 eV
Corrected Energy
-28.0826 eV
-28.0826 eV = -23.9450 eV (uncorrected energy) - 2.7330 eV (MP Advanced Correction) - 1.4046 eV (MP Anion Correction)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
User remarks:
  • supplementary compounds from MIT matgen database

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)