Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingAFM |
Formation Energy / Atom-3.058 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.01 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap2.661 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinFd3m [227] |
HallF 4d 2 3 1d |
Point Groupm3m |
Crystal Systemcubic |
Topological ClassificationSM*
|
SubclassificationESFD†
|
Crossing TypePoint
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 97.6 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 207.0 |
CdS (mp-672) | <1 0 0> | <1 1 0> | 292.7 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 276.0 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 69.0 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 276.0 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 276.0 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 1 1> | 119.5 |
KTaO3 (mp-3614) | <1 0 0> | <1 1 0> | 97.6 |
Al (mp-134) | <1 0 0> | <1 0 0> | 276.0 |
LiGaO2 (mp-5854) | <0 1 1> | <1 0 0> | 207.0 |
CdTe (mp-406) | <1 1 0> | <1 1 0> | 195.1 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 69.0 |
Ag (mp-124) | <1 1 0> | <1 1 0> | 97.6 |
Ag (mp-124) | <1 1 1> | <1 1 1> | 119.5 |
LiNbO3 (mp-3731) | <1 0 0> | <1 1 0> | 292.7 |
Fe3O4 (mp-19306) | <1 0 0> | <1 0 0> | 69.0 |
TiO2 (mp-2657) | <0 0 1> | <1 0 0> | 276.0 |
LiGaO2 (mp-5854) | <1 0 1> | <1 0 0> | 138.0 |
TeO2 (mp-2125) | <1 0 0> | <1 1 0> | 292.7 |
C (mp-66) | <1 1 0> | <1 1 0> | 292.7 |
PbS (mp-21276) | <1 0 0> | <1 0 0> | 69.0 |
Fe3O4 (mp-19306) | <1 1 0> | <1 1 0> | 97.6 |
Fe3O4 (mp-19306) | <1 1 1> | <1 1 1> | 119.5 |
Mg (mp-153) | <1 0 1> | <1 0 0> | 207.0 |
Mg (mp-153) | <1 1 1> | <1 0 0> | 276.0 |
InP (mp-20351) | <1 0 0> | <1 0 0> | 69.0 |
Ni (mp-23) | <1 1 0> | <1 1 0> | 292.7 |
InSb (mp-20012) | <1 1 0> | <1 1 0> | 195.1 |
BaTiO3 (mp-5986) | <0 0 1> | <1 1 1> | 239.0 |
NdGaO3 (mp-3196) | <0 0 1> | <1 0 0> | 276.0 |
PbS (mp-21276) | <1 1 0> | <1 1 0> | 97.6 |
GaP (mp-2490) | <1 0 0> | <1 0 0> | 276.0 |
Ga2O3 (mp-886) | <1 0 0> | <1 1 0> | 292.7 |
Ga2O3 (mp-886) | <1 1 0> | <1 1 0> | 292.7 |
Au (mp-81) | <1 0 0> | <1 0 0> | 69.0 |
Au (mp-81) | <1 1 1> | <1 1 1> | 119.5 |
InP (mp-20351) | <1 1 0> | <1 1 0> | 97.6 |
ZrO2 (mp-2858) | <1 1 0> | <1 0 0> | 276.0 |
YAlO3 (mp-3792) | <1 1 0> | <1 0 0> | 276.0 |
Ga2O3 (mp-886) | <0 1 0> | <1 1 0> | 292.7 |
Si (mp-149) | <1 0 0> | <1 0 0> | 276.0 |
Au (mp-81) | <1 1 0> | <1 1 0> | 97.6 |
SiC (mp-8062) | <1 1 0> | <1 1 0> | 292.7 |
ZrO2 (mp-2858) | <0 0 1> | <1 0 0> | 138.0 |
MgAl2O4 (mp-3536) | <1 0 0> | <1 0 0> | 69.0 |
MgAl2O4 (mp-3536) | <1 1 0> | <1 1 0> | 97.6 |
MgAl2O4 (mp-3536) | <1 1 1> | <1 1 1> | 119.5 |
Cu (mp-30) | <1 1 0> | <1 1 0> | 292.7 |
ZnO (mp-2133) | <1 1 1> | <1 0 0> | 276.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Dielectric Tensor εij∞ (electronic contribution) |
||
---|---|---|
3.48 | 0.00 | 0.00 |
0.00 | 3.48 | 0.00 |
0.00 | 0.00 | 3.48 |
Dielectric Tensor εij (total) |
||
---|---|---|
9.49 | 0.00 | 0.00 |
0.00 | 9.49 | 0.00 |
0.00 | 0.00 | 9.49 |
Polycrystalline dielectric constant
εpoly∞
3.48
|
Polycrystalline dielectric constant
εpoly
9.49
|
Refractive Index n1.87 |
Potentially ferroelectric?Unknown |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Cr2HgSe4 (mp-5602) | 0.0026 | 0.000 | 3 |
V2CdO4 (mp-18847) | 0.0337 | 0.000 | 3 |
Cd(FeO2)2 (mp-24940) | 0.0444 | 0.000 | 3 |
Cr2HgS4 (mp-15973) | 0.0268 | 0.000 | 3 |
Cr2CdS4 (mp-4338) | 0.0340 | 0.000 | 3 |
Li2CoNi3O8 (mp-761777) | 0.2260 | 0.016 | 4 |
LiCrNiO4 (mp-770245) | 0.2282 | 0.103 | 4 |
LiCoNiO4 (mp-776511) | 0.1897 | 0.000 | 4 |
Li2Co3NiO8 (mp-761738) | 0.1854 | 0.226 | 4 |
Li2MnFe3O8 (mp-775094) | 0.1928 | 0.095 | 4 |
Co3O4 (mp-559191) | 0.1938 | 0.010 | 2 |
In3S4 (mp-556597) | 0.3561 | 0.042 | 2 |
Co3O4 (mp-18748) | 0.1862 | 0.010 | 2 |
Ni3S4 (mp-1050) | 0.3961 | 0.000 | 2 |
Sn3N4 (mp-16031) | 0.3748 | 0.000 | 2 |
Li4Cr2Fe3Co3O16 (mp-775698) | 0.5295 | 0.894 | 5 |
Li4Mn2Fe3Co3O16 (mp-761441) | 0.5285 | 0.079 | 5 |
Li14Mn22Cr3Cu3O56 (mp-735790) | 0.5144 | 0.019 | 5 |
Li4Mn3Cr3(CuO8)2 (mp-765456) | 0.5157 | 0.080 | 5 |
Li4Cr3Cu3(SbO8)2 (mp-783908) | 0.5334 | 0.040 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eV |
PseudopotentialsVASP PAW: Mn_pv Al O |
Final Energy/Atom-7.6233 eV |
Corrected Energy-115.7065 eV
-115.7065 eV = -106.7265 eV (uncorrected energy) - 5.6183 eV (MP Anion Correction) - 3.3617 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)