Final Magnetic Moment2.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.624 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.051 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.54 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToVP2O7 + Li6V3P8O29 + LiPO3 + VPO5 |
Band Gap0.748 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [1] |
HallP 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 1 0> | <1 1 1> | 161.4 |
GaAs (mp-2534) | <1 1 0> | <0 1 0> | 137.9 |
SiO2 (mp-6930) | <1 0 1> | <0 1 0> | 137.9 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 0> | 137.9 |
Al (mp-134) | <1 1 0> | <0 1 0> | 137.9 |
Al (mp-134) | <1 1 1> | <0 0 1> | 83.6 |
C (mp-66) | <1 1 0> | <0 0 1> | 250.7 |
GdScO3 (mp-5690) | <0 1 1> | <0 0 1> | 167.1 |
GdScO3 (mp-5690) | <1 0 0> | <0 1 0> | 137.9 |
GdScO3 (mp-5690) | <1 0 1> | <0 0 1> | 167.1 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 250.7 |
PbS (mp-21276) | <1 1 1> | <0 0 1> | 250.7 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 250.7 |
DyScO3 (mp-31120) | <1 0 0> | <0 1 0> | 137.9 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 167.1 |
InP (mp-20351) | <1 1 1> | <0 0 1> | 250.7 |
ZnSe (mp-1190) | <1 1 0> | <0 1 0> | 137.9 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 83.6 |
TbScO3 (mp-31119) | <1 0 0> | <0 1 0> | 137.9 |
TbScO3 (mp-31119) | <1 0 1> | <0 0 1> | 167.1 |
Ni (mp-23) | <1 1 0> | <0 1 0> | 137.9 |
Ni (mp-23) | <1 1 1> | <0 0 1> | 83.6 |
YVO4 (mp-19133) | <1 0 1> | <0 1 0> | 137.9 |
NdGaO3 (mp-3196) | <1 0 1> | <0 0 1> | 167.1 |
WS2 (mp-224) | <1 0 0> | <0 1 0> | 137.9 |
NaCl (mp-22862) | <1 1 0> | <0 1 0> | 137.9 |
C (mp-48) | <1 0 1> | <1 0 1> | 161.2 |
ZnO (mp-2133) | <0 0 1> | <0 0 1> | 83.6 |
Al2O3 (mp-1143) | <0 0 1> | <0 1 1> | 161.1 |
SrTiO3 (mp-4651) | <1 0 1> | <0 0 1> | 167.1 |
Ge (mp-32) | <1 1 0> | <0 1 0> | 137.9 |
Al2O3 (mp-1143) | <1 0 0> | <0 0 1> | 250.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Mn7Cr12O48 (mp-774029) | 0.6138 | 0.078 | 3 |
Ti7Cr12O48 (mp-853216) | 0.4949 | 0.084 | 3 |
Fe2(WO4)3 (mvc-8014) | 0.5423 | 0.124 | 3 |
Fe2(MoO4)3 (mvc-8023) | 0.5377 | 0.047 | 3 |
Cr3(FeO6)2 (mvc-7922) | 0.6066 | 0.031 | 3 |
Li9V6(P8O29)2 (mp-850768) | 0.2576 | 0.052 | 4 |
Li4V3P8O29 (mp-851247) | 0.2178 | 0.051 | 4 |
Li9V6(P8O29)2 (mp-851212) | 0.2163 | 0.051 | 4 |
Li5V3P8O29 (mp-762979) | 0.2528 | 0.047 | 4 |
Li5V3P8O29 (mp-762968) | 0.1763 | 0.046 | 4 |
Cr19O48 (mp-850874) | 0.5025 | 0.097 | 2 |
Cr19O48 (mp-780521) | 0.5689 | 0.085 | 2 |
Cr8O21 (mp-565489) | 0.7216 | 0.032 | 2 |
FeP3H5NO10 (mp-743646) | 0.6406 | 0.000 | 5 |
LiSn2P4H3O16 (mp-759095) | 0.6085 | 0.041 | 5 |
LiSn2P4H3O16 (mp-754500) | 0.5704 | 0.059 | 5 |
SnP4H8N2O13 (mp-603633) | 0.6256 | 0.010 | 5 |
Li2Mn2P4H6O17 (mp-780897) | 0.6303 | 0.026 | 5 |
Ti2P4H9C2NO16 (mp-709069) | 0.5652 | 0.039 | 6 |
FeBP2H5NO9 (mp-766957) | 0.7390 | 0.005 | 6 |
VBP2H5NO9 (mp-25798) | 0.6936 | 0.000 | 6 |
Al3P3H9C3NO14 (mp-699455) | 0.6913 | 0.065 | 6 |
AlBP2H5NO9 (mp-24757) | 0.7371 | 0.000 | 6 |
Al2P2H8C2NO8F (mp-708964) | 0.7470 | 0.050 | 7 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesV: 3.25 eV |
PseudopotentialsVASP PAW: Li_sv V_pv P O |
Final Energy/Atom-7.0282 eV |
Corrected Energy-683.3647 eV
-683.3647 eV = -632.5399 eV (uncorrected energy) - 40.7328 eV (MP Anion Correction) - 10.0920 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)