Final Magnetic Moment6.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.662 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.018 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.88 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi6V3P8O29 + Mn(PO3)2 + Mn2P2O7 |
Band Gap0.366 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21 [4] |
HallP 2yb |
Point Group2 |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <1 0 1> | 119.0 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 201.7 |
GaAs (mp-2534) | <1 1 1> | <1 0 1> | 119.0 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 282.4 |
GaN (mp-804) | <1 1 1> | <0 1 0> | 324.9 |
DyScO3 (mp-31120) | <0 1 0> | <0 1 0> | 129.9 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 161.4 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 201.7 |
ZnSe (mp-1190) | <1 1 0> | <1 0 1> | 237.9 |
ZnSe (mp-1190) | <1 1 1> | <1 0 1> | 119.0 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 282.4 |
LiF (mp-1138) | <1 1 0> | <1 1 0> | 257.0 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 282.4 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 282.4 |
Te2Mo (mp-602) | <1 0 1> | <0 1 1> | 229.4 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 201.7 |
BN (mp-984) | <1 0 0> | <0 0 1> | 322.8 |
BN (mp-984) | <1 0 1> | <0 1 1> | 305.9 |
BN (mp-984) | <1 1 1> | <1 0 1> | 237.9 |
Al (mp-134) | <1 0 0> | <0 0 1> | 201.7 |
LiGaO2 (mp-5854) | <1 0 1> | <1 0 0> | 221.8 |
LiGaO2 (mp-5854) | <1 1 0> | <0 0 1> | 282.4 |
LiGaO2 (mp-5854) | <1 1 1> | <0 1 0> | 324.9 |
CdTe (mp-406) | <1 1 0> | <1 1 0> | 128.5 |
CdTe (mp-406) | <1 1 1> | <1 0 1> | 237.9 |
Fe3O4 (mp-19306) | <1 0 0> | <0 0 1> | 282.4 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 282.4 |
GdScO3 (mp-5690) | <0 1 1> | <0 0 1> | 161.4 |
Mg (mp-153) | <1 0 1> | <0 0 1> | 282.4 |
PbS (mp-21276) | <1 0 0> | <0 0 1> | 282.4 |
PbS (mp-21276) | <1 1 0> | <0 0 1> | 201.7 |
GaP (mp-2490) | <1 1 0> | <1 1 0> | 128.5 |
InP (mp-20351) | <1 0 0> | <0 0 1> | 282.4 |
InP (mp-20351) | <1 1 1> | <1 0 1> | 119.0 |
TbScO3 (mp-31119) | <0 1 1> | <0 0 1> | 161.4 |
Ni (mp-23) | <1 0 0> | <0 0 1> | 121.0 |
Ni (mp-23) | <1 1 0> | <0 0 1> | 121.0 |
LaAlO3 (mp-2920) | <1 0 0> | <1 0 0> | 221.8 |
LaAlO3 (mp-2920) | <1 0 1> | <1 0 1> | 237.9 |
LaAlO3 (mp-2920) | <1 1 0> | <1 1 0> | 128.5 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 322.8 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 282.4 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 201.7 |
CeO2 (mp-20194) | <1 1 0> | <1 1 0> | 128.5 |
GaAs (mp-2534) | <1 1 0> | <1 0 1> | 237.9 |
GaN (mp-804) | <0 0 1> | <0 1 0> | 259.9 |
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 161.4 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 201.7 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 121.0 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 282.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
V5(P3O11)2 (mp-767351) | 0.4274 | 0.023 | 3 |
Co5(P3O11)2 (mp-31617) | 0.4520 | 0.034 | 3 |
Ni5(P3O11)2 (mp-32359) | 0.3580 | 0.082 | 3 |
Mn5(P3O11)2 (mp-705036) | 0.4502 | 0.028 | 3 |
Fe5(P3O11)2 (mp-705342) | 0.4318 | 0.038 | 3 |
LiVP2O7 (mp-18911) | 0.1085 | 0.033 | 4 |
LiCrP2O7 (mp-19103) | 0.1390 | 0.000 | 4 |
LiFeP2O7 (mp-19294) | 0.1217 | 0.000 | 4 |
LiScP2O7 (mp-10517) | 0.1326 | 0.000 | 4 |
LiTiP2O7 (mp-26629) | 0.1849 | 0.055 | 4 |
Li4MnV3(P2O7)4 (mp-850462) | 0.0414 | 0.002 | 5 |
Li2MnV(P2O7)2 (mp-764893) | 0.0426 | 0.018 | 5 |
Li2MnV(P2O7)2 (mp-779885) | 0.0391 | 0.017 | 5 |
Li2MnV(P2O7)2 (mp-779842) | 0.0365 | 0.018 | 5 |
Li4MnV3(P2O7)4 (mp-780005) | 0.0357 | 0.000 | 5 |
LiMgCr3Se2(SO6)4 (mp-769552) | 0.5921 | 0.255 | 6 |
Li2MgCr3Se3(SO8)3 (mp-773983) | 0.5265 | 0.330 | 6 |
Ca2Al2FeSi4BHO16 (mp-540713) | 0.5598 | 0.002 | 7 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eVV: 3.25 eV |
PseudopotentialsVASP PAW: Li_sv Mn_pv V_pv P O |
Final Energy/Atom-7.1979 eV |
Corrected Energy-343.0974 eV
-343.0974 eV = -316.7076 eV (uncorrected energy) - 19.6641 eV (MP Anion Correction) - 6.7257 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)