Final Magnetic Moment29.728 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-1.953 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.811 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.24 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiCoO2 + Li10Co4O9 + LiCrO2 + Li4CrFe3O8 + CoO |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCm [8] |
HallC 2y |
Point Groupm |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <1 1 0> | 234.5 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 123.2 |
GaN (mp-804) | <1 0 0> | <0 1 0> | 101.5 |
GaN (mp-804) | <1 0 1> | <1 0 1> | 170.4 |
GaN (mp-804) | <1 1 0> | <1 1 1> | 265.1 |
SiO2 (mp-6930) | <0 0 1> | <1 0 0> | 176.0 |
SiO2 (mp-6930) | <1 1 1> | <1 1 1> | 265.1 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 246.4 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 0> | 203.1 |
CdS (mp-672) | <1 0 1> | <1 0 0> | 293.4 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 246.4 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 308.0 |
YVO4 (mp-19133) | <1 1 0> | <0 1 0> | 203.1 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 176.0 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 123.2 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 61.6 |
GaSe (mp-1943) | <0 0 1> | <1 0 0> | 176.0 |
BN (mp-984) | <0 0 1> | <1 0 0> | 176.0 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 184.8 |
LiNbO3 (mp-3731) | <1 0 1> | <0 0 1> | 308.0 |
LiNbO3 (mp-3731) | <1 1 0> | <1 0 1> | 255.6 |
Al (mp-134) | <1 0 0> | <0 0 1> | 246.4 |
LiGaO2 (mp-5854) | <0 1 0> | <1 0 0> | 234.7 |
SiC (mp-7631) | <1 0 0> | <1 1 0> | 234.5 |
SiC (mp-7631) | <1 0 1> | <0 1 1> | 237.5 |
LiTaO3 (mp-3666) | <0 0 1> | <0 0 1> | 184.8 |
LiTaO3 (mp-3666) | <1 0 1> | <0 0 1> | 308.0 |
LiTaO3 (mp-3666) | <1 1 0> | <1 0 1> | 255.6 |
Fe3O4 (mp-19306) | <1 1 1> | <0 0 1> | 123.2 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 184.8 |
MgO (mp-1265) | <1 1 0> | <1 0 0> | 176.0 |
MgO (mp-1265) | <1 1 1> | <0 0 1> | 61.6 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 308.0 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 308.0 |
C (mp-66) | <1 0 0> | <0 1 0> | 101.5 |
C (mp-66) | <1 1 0> | <1 0 0> | 176.0 |
C (mp-66) | <1 1 1> | <1 0 0> | 176.0 |
GdScO3 (mp-5690) | <1 0 1> | <1 1 0> | 117.3 |
Mg (mp-153) | <1 0 0> | <0 1 0> | 101.5 |
Mg (mp-153) | <1 0 1> | <1 0 1> | 170.4 |
Mg (mp-153) | <1 1 0> | <1 1 1> | 265.1 |
PbS (mp-21276) | <1 0 0> | <1 0 0> | 176.0 |
PbS (mp-21276) | <1 1 0> | <0 0 1> | 246.4 |
InP (mp-20351) | <1 0 0> | <1 0 0> | 176.0 |
InP (mp-20351) | <1 1 0> | <0 0 1> | 246.4 |
Ni (mp-23) | <1 0 0> | <1 0 0> | 293.4 |
Ni (mp-23) | <1 1 0> | <1 0 0> | 176.0 |
BaTiO3 (mp-5986) | <0 0 1> | <1 0 0> | 234.7 |
BaTiO3 (mp-5986) | <1 0 0> | <1 0 0> | 293.4 |
BaTiO3 (mp-5986) | <1 0 1> | <1 0 0> | 117.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li5(NiO2)4 (mp-780518) | 0.3436 | 0.327 | 3 |
Li5(FeO2)4 (mp-780312) | 0.1447 | 0.259 | 3 |
Li12Cr5O16 (mp-764428) | 0.6304 | 0.177 | 3 |
Li5(CoO2)4 (mp-780140) | 0.2528 | 0.251 | 3 |
Li5Cr4O8 (mp-850237) | 0.2746 | 0.101 | 3 |
Li10Mn3V5O16 (mp-764265) | 0.1897 | 0.587 | 4 |
Li10V3Cr5O16 (mp-764096) | 0.1611 | 0.100 | 4 |
Li10Fe5Co3O16 (mp-763869) | 0.1393 | 0.090 | 4 |
Li5V3CrO8 (mp-764013) | 0.1651 | 0.481 | 4 |
Li5FeNi3O8 (mp-765057) | 0.1898 | 0.269 | 4 |
Ti3N4 (mp-1080192) | 0.7224 | 0.101 | 2 |
Li10Mn2Fe3Ni3O16 (mp-764933) | 0.1608 | 0.079 | 5 |
Li10Fe2Co3Ni3O16 (mp-780632) | 0.1812 | 0.142 | 5 |
Li10Fe3Co2Ni3O16 (mp-779868) | 0.1511 | 0.302 | 5 |
Li10Cr3Co2Ni3O16 (mp-778771) | 0.1468 | 0.263 | 5 |
Li10Cr3Fe3(NiO8)2 (mp-775215) | 0.1650 | 0.890 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesCr: 3.7 eVFe: 5.3 eV Co: 3.32 eV |
PseudopotentialsVASP PAW: Li_sv Cr_pv Fe_pv Co O |
Final Energy/Atom-5.9294 eV |
Corrected Energy-230.6845 eV
-230.6845 eV = -201.6009 eV (uncorrected energy) - 17.8470 eV (MP Advanced Correction) - 11.2366 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)