Final Magnetic Moment1.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.918 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.00 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinR3 [146] |
HallR 3 |
Point Group3 |
Crystal Systemtrigonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 201.1 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 201.1 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 67.0 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 67.0 |
SiO2 (mp-6930) | <1 1 0> | <1 0 0> | 195.5 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 201.1 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 67.0 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 268.1 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 67.0 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 201.1 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 201.1 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 201.1 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 268.1 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 268.1 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 268.1 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 268.1 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 201.1 |
BN (mp-984) | <0 0 1> | <0 0 1> | 201.1 |
BN (mp-984) | <1 1 0> | <0 0 1> | 67.0 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 201.1 |
Al (mp-134) | <1 1 1> | <0 0 1> | 201.1 |
LiGaO2 (mp-5854) | <1 1 0> | <0 0 1> | 201.1 |
TiO2 (mp-2657) | <1 1 1> | <0 0 1> | 201.1 |
Ge3(BiO3)4 (mp-23560) | <1 1 1> | <0 0 1> | 201.1 |
C (mp-66) | <1 1 0> | <0 0 1> | 268.1 |
C (mp-66) | <1 1 1> | <0 0 1> | 67.0 |
GaP (mp-2490) | <1 1 1> | <0 0 1> | 201.1 |
PbSe (mp-2201) | <1 1 1> | <0 0 1> | 67.0 |
MoSe2 (mp-1634) | <1 1 0> | <0 0 1> | 268.1 |
Si (mp-149) | <1 1 1> | <0 0 1> | 201.1 |
CdSe (mp-2691) | <1 1 0> | <0 0 1> | 268.1 |
CdSe (mp-2691) | <1 1 1> | <0 0 1> | 67.0 |
C (mp-48) | <0 0 1> | <1 0 0> | 195.5 |
WSe2 (mp-1821) | <0 0 1> | <0 0 1> | 67.0 |
WSe2 (mp-1821) | <1 1 0> | <0 0 1> | 268.1 |
CaCO3 (mp-3953) | <0 0 1> | <0 0 1> | 67.0 |
CaCO3 (mp-3953) | <1 0 0> | <0 0 1> | 268.1 |
CdWO4 (mp-19387) | <0 0 1> | <0 0 1> | 268.1 |
Cu (mp-30) | <1 1 1> | <0 0 1> | 67.0 |
CaF2 (mp-2741) | <1 1 1> | <0 0 1> | 201.1 |
Fe2O3 (mp-24972) | <0 0 1> | <0 0 1> | 67.0 |
PbSe (mp-2201) | <1 1 0> | <0 0 1> | 268.1 |
MoSe2 (mp-1634) | <0 0 1> | <0 0 1> | 67.0 |
Ga2O3 (mp-886) | <1 0 0> | <0 0 1> | 268.1 |
Au (mp-81) | <1 1 1> | <0 0 1> | 268.1 |
WSe2 (mp-1821) | <1 1 1> | <0 0 1> | 268.1 |
ZrO2 (mp-2858) | <0 1 1> | <0 0 1> | 201.1 |
GaSb (mp-1156) | <1 1 0> | <0 0 1> | 268.1 |
GaSb (mp-1156) | <1 1 1> | <0 0 1> | 67.0 |
ZnTe (mp-2176) | <1 1 0> | <0 0 1> | 268.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Fe2(PO4)3 (mp-540329) | 0.0977 | 0.265 | 3 |
Nb2(PO4)3 (mp-540332) | 0.1005 | 0.005 | 3 |
Ti2(PO4)3 (mp-774537) | 0.1259 | 0.013 | 3 |
Nb2(PO4)3 (mp-17242) | 0.1047 | 0.000 | 3 |
V2(PO4)3 (mp-540480) | 0.1350 | 0.027 | 3 |
Nb3Fe(PO4)6 (mp-861583) | 0.0611 | 0.000 | 4 |
TiP6(WO8)3 (mp-772373) | 0.0630 | 0.027 | 4 |
Nb3Cr(PO4)6 (mp-774426) | 0.0686 | 0.000 | 4 |
Nb3V(PO4)6 (mp-853177) | 0.0568 | 0.000 | 4 |
VP6(WO8)3 (mp-765732) | 0.0713 | 0.009 | 4 |
Cr5O12 (mp-773920) | 0.3459 | 0.000 | 2 |
Mo4O11 (mp-622101) | 0.6599 | 0.018 | 2 |
Nb2O5 (mp-776896) | 0.6543 | 0.059 | 2 |
Mo4O11 (mp-565865) | 0.6810 | 0.026 | 2 |
V5O12 (mp-778252) | 0.4231 | 0.024 | 2 |
VCrP2(O4F)2 (mp-765139) | 0.4661 | 0.041 | 5 |
CaTi2Fe2(PO4)6 (mvc-11942) | 0.4962 | 0.210 | 5 |
LiTi3V(PO4)6 (mp-761331) | 0.5138 | 0.015 | 5 |
MnVP2(O4F)2 (mp-777435) | 0.4919 | 0.002 | 5 |
VFeP2(O4F)2 (mp-778349) | 0.4718 | 0.038 | 5 |
Zr12Si2Bi2P16PbO72 (mp-693759) | 0.7163 | 0.009 | 6 |
LiTi3MnCr(PO4)6 (mp-772224) | 0.6172 | 0.001 | 6 |
NaLiTiAl(PO4)3 (mp-776520) | 0.7414 | 0.023 | 6 |
Na2LiTi3Al(PO4)6 (mp-769074) | 0.6685 | 0.011 | 6 |
Na2LiTi3Al(PO4)6 (mp-769073) | 0.6696 | 0.014 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ti_pv Nb_pv P O |
Final Energy/Atom-7.9934 eV |
Corrected Energy-288.6316 eV
-288.6316 eV = -271.7767 eV (uncorrected energy) - 16.8550 eV (MP Anion Correction)
|