material

LiCuS

ID:

mp-774712

DOI:

10.17188/1302644


Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
Non-magnetic
Formation Energy / Atom
-0.911 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.049 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
3.82 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
LiCuS
Band Gap
0.851 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P63/mmc [194]
Hall
-P 6c 2c
Point Group
6/mmm
Crystal System
hexagonal
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
Si (mp-149) <1 1 1> <0 0 1> 0.008 52.0
TiO2 (mp-390) <1 0 0> <1 0 1> 0.008 147.8
NaCl (mp-22862) <1 1 1> <0 0 1> 0.008 169.0
SiC (mp-7631) <1 0 0> <1 0 1> 0.009 236.5
Cu (mp-30) <1 1 1> <0 0 1> 0.010 91.0
CeO2 (mp-20194) <1 1 1> <0 0 1> 0.010 52.0
CdWO4 (mp-19387) <0 1 1> <0 0 1> 0.010 325.0
GaN (mp-804) <0 0 1> <0 0 1> 0.011 117.0
InP (mp-20351) <1 1 1> <0 0 1> 0.012 247.0
Fe2O3 (mp-24972) <0 0 1> <0 0 1> 0.013 91.0
BaTiO3 (mp-5986) <1 1 0> <0 0 1> 0.016 143.0
TiO2 (mp-390) <1 1 1> <0 0 1> 0.019 273.0
C (mp-66) <1 1 0> <1 1 1> 0.019 143.4
SrTiO3 (mp-4651) <1 0 1> <0 0 1> 0.020 325.0
SiC (mp-7631) <1 0 1> <1 0 1> 0.020 236.5
YAlO3 (mp-3792) <1 0 1> <1 0 0> 0.020 345.2
Au (mp-81) <1 1 1> <0 0 1> 0.023 91.0
LiF (mp-1138) <1 0 0> <1 0 1> 0.023 266.1
CdWO4 (mp-19387) <0 0 1> <1 0 0> 0.024 212.4
ZrO2 (mp-2858) <1 0 0> <1 1 0> 0.024 229.9
CeO2 (mp-20194) <1 0 0> <0 0 1> 0.024 208.0
Ag (mp-124) <1 1 0> <0 0 1> 0.027 195.0
CdWO4 (mp-19387) <1 0 1> <0 0 1> 0.027 312.0
KP(HO2)2 (mp-23959) <1 0 0> <1 1 0> 0.027 229.9
Si (mp-149) <1 0 0> <0 0 1> 0.028 208.0
Fe2O3 (mp-24972) <1 0 0> <1 0 0> 0.029 212.4
BaTiO3 (mp-5986) <1 0 0> <1 0 0> 0.030 239.0
MgF2 (mp-1249) <1 1 1> <0 0 1> 0.032 91.0
Ge (mp-32) <1 0 0> <1 0 1> 0.034 266.1
C (mp-48) <1 1 0> <1 0 1> 0.037 236.5
SrTiO3 (mp-4651) <1 1 1> <0 0 1> 0.037 208.0
AlN (mp-661) <1 1 1> <1 1 0> 0.041 229.9
C (mp-66) <1 0 0> <1 0 0> 0.042 265.5
BN (mp-984) <1 1 1> <0 0 1> 0.042 169.0
WSe2 (mp-1821) <1 0 0> <0 0 1> 0.042 299.0
YAlO3 (mp-3792) <1 1 1> <0 0 1> 0.044 312.0
TiO2 (mp-2657) <0 0 1> <0 0 1> 0.051 65.0
AlN (mp-661) <1 0 0> <1 0 1> 0.052 236.5
TiO2 (mp-2657) <1 0 0> <1 1 0> 0.053 138.0
TeO2 (mp-2125) <0 1 0> <0 0 1> 0.054 208.0
SiC (mp-11714) <0 0 1> <0 0 1> 0.054 156.0
GaP (mp-2490) <1 1 1> <0 0 1> 0.056 52.0
GaAs (mp-2534) <1 0 0> <1 0 1> 0.056 266.1
SiO2 (mp-6930) <1 0 1> <1 1 0> 0.059 321.9
TePb (mp-19717) <1 0 0> <0 0 1> 0.059 130.0
SiC (mp-7631) <0 0 1> <0 0 1> 0.060 156.0
CsI (mp-614603) <1 1 0> <0 0 1> 0.063 260.0
Bi2Te3 (mp-34202) <0 0 1> <0 0 1> 0.065 52.0
PbS (mp-21276) <1 1 1> <0 0 1> 0.067 247.0
SrTiO3 (mp-4651) <1 1 0> <0 0 1> 0.070 312.0
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
132 110 19 0 0 0
110 132 19 0 0 0
19 19 46 0 0 0
0 0 0 9 0 0
0 0 0 0 9 0
-0 -0 0 0 0 11
Compliance Tensor Sij (10-12Pa-1)
25.2 -20.8 -1.8 0 0 0
-20.8 25.2 -1.8 0 0 0
-1.8 -1.8 23.2 0 0 0
0 0 0 112.6 0 0
0 0 0 0 112.6 0
0 0 0 0 0 92.1
Shear Modulus GV
17 GPa
Bulk Modulus KV
67 GPa
Shear Modulus GR
11 GPa
Bulk Modulus KR
40 GPa
Shear Modulus GVRH
14 GPa
Bulk Modulus KVRH
54 GPa
Elastic Anisotropy
3.08
Poisson's Ratio
0.38

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
102
U Values
--
Pseudopotentials
VASP PAW: Li_sv Cu_pv S
Final Energy/Atom
-4.0683 eV
Corrected Energy
-25.7366 eV
-25.7366 eV = -24.4097 eV (uncorrected energy) - 1.3269 eV (MP Anion Correction)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
User remarks:
  • supplementary compounds from MIT matgen database

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)