Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.485 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.065 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.64 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToNbPO5 + Cu(PO3)2 + Cu |
Band Gap0.304 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/m [11] |
Hall-P 2yb |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 0> | <0 0 1> | 222.5 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 127.2 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 31.8 |
AlN (mp-661) | <1 0 1> | <1 0 1> | 70.1 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 190.7 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 190.7 |
CeO2 (mp-20194) | <1 1 0> | <0 1 0> | 254.8 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 317.9 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 158.9 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 222.5 |
GaN (mp-804) | <0 0 1> | <0 1 0> | 254.8 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 222.5 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 222.5 |
GaN (mp-804) | <1 1 1> | <0 1 0> | 254.8 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 222.5 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 222.5 |
SiO2 (mp-6930) | <1 0 1> | <0 1 1> | 240.3 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 185.3 |
SiO2 (mp-6930) | <1 1 0> | <0 1 1> | 240.3 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 286.1 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 0> | 254.8 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 286.1 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 317.9 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 247.1 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 222.5 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 317.9 |
DyScO3 (mp-31120) | <0 1 1> | <1 1 0> | 160.2 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 317.9 |
DyScO3 (mp-31120) | <1 1 0> | <0 1 0> | 254.8 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 190.7 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 158.9 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 222.5 |
CdS (mp-672) | <1 0 1> | <0 1 1> | 300.3 |
LiF (mp-1138) | <1 1 1> | <0 1 0> | 203.8 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 63.6 |
Te2W (mp-22693) | <1 0 0> | <0 0 1> | 95.4 |
Te2W (mp-22693) | <1 0 1> | <0 0 1> | 95.4 |
YVO4 (mp-19133) | <1 1 1> | <0 0 1> | 254.3 |
CdS (mp-672) | <1 1 1> | <0 1 1> | 300.3 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 247.1 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 349.7 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 254.3 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 222.5 |
YVO4 (mp-19133) | <1 1 0> | <1 0 0> | 61.8 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 222.5 |
Ag (mp-124) | <1 0 0> | <1 1 0> | 240.2 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 349.7 |
Ag (mp-124) | <1 1 1> | <1 1 0> | 240.2 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 286.1 |
Te2Mo (mp-602) | <1 1 0> | <0 0 1> | 95.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
V2P3O10 (mp-540351) | 0.4993 | 0.116 | 3 |
MnPO4 (mp-771363) | 0.5235 | 0.025 | 3 |
Co2P3O10 (mp-25658) | 0.4774 | 0.123 | 3 |
Fe2P3O10 (mp-540498) | 0.4926 | 0.277 | 3 |
Ni2P3O10 (mp-25610) | 0.5011 | 0.052 | 3 |
TiMn(PO4)2 (mp-775663) | 0.2725 | 0.030 | 4 |
TiMn3(PO4)4 (mp-772362) | 0.2306 | 0.022 | 4 |
V3Cu(PO4)4 (mp-775334) | 0.2386 | 0.062 | 4 |
TiCu(PO4)2 (mp-755864) | 0.2356 | 0.037 | 4 |
NbCu3(PO4)4 (mp-772046) | 0.2525 | 0.066 | 4 |
MnFeCo(PO4)3 (mp-764392) | 0.3439 | 0.028 | 5 |
MnFeCo(PO4)3 (mp-764415) | 0.3543 | 0.035 | 5 |
MnFeCo(PO4)3 (mp-764383) | 0.3452 | 0.038 | 5 |
MnFeCo(PO4)3 (mp-763446) | 0.3355 | 0.033 | 5 |
MnFeCo(PO4)3 (mp-764739) | 0.3493 | 0.023 | 5 |
LiMgCr3Se2(SO6)4 (mp-769552) | 0.6935 | 0.003 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Nb_pv Cu_pv P O |
Final Energy/Atom-7.4008 eV |
Corrected Energy-188.8570 eV
-188.8570 eV = -177.6204 eV (uncorrected energy) - 11.2366 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)