Final Magnetic Moment0.068 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.676 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.102 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.30 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToNi9S8 + Ni3S4 + Li2S |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [2] |
Hall-P 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 1 0> | 219.5 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 111.9 |
AlN (mp-661) | <1 0 1> | <0 1 1> | 126.5 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 291.6 |
AlN (mp-661) | <1 1 1> | <0 1 -1> | 205.4 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 149.1 |
GaAs (mp-2534) | <1 1 1> | <1 1 0> | 272.2 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 194.4 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 111.9 |
GaN (mp-804) | <0 0 1> | <1 1 1> | 89.9 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 186.4 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 243.0 |
SiO2 (mp-6930) | <1 0 0> | <0 1 -1> | 256.7 |
SiO2 (mp-6930) | <1 1 1> | <0 1 1> | 253.0 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 111.9 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 340.2 |
DyScO3 (mp-31120) | <1 0 1> | <0 1 0> | 219.5 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 243.0 |
LaAlO3 (mp-2920) | <0 0 1> | <1 -1 0> | 314.2 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 194.4 |
InAs (mp-20305) | <1 1 1> | <0 1 -1> | 256.7 |
ZnSe (mp-1190) | <1 0 0> | <1 1 1> | 269.6 |
ZnSe (mp-1190) | <1 1 1> | <1 1 0> | 272.2 |
KTaO3 (mp-3614) | <1 0 0> | <1 -1 1> | 310.6 |
KTaO3 (mp-3614) | <1 1 1> | <0 1 -1> | 256.7 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 335.6 |
CeO2 (mp-20194) | <1 1 1> | <1 1 0> | 272.2 |
CdS (mp-672) | <1 0 0> | <1 -1 1> | 233.0 |
CdS (mp-672) | <1 1 0> | <1 1 -1> | 251.9 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 149.1 |
GaAs (mp-2534) | <1 0 0> | <1 1 1> | 269.6 |
GaAs (mp-2534) | <1 1 0> | <1 -1 0> | 314.2 |
LiF (mp-1138) | <1 1 0> | <0 1 1> | 189.7 |
LiF (mp-1138) | <1 1 1> | <0 1 -1> | 256.7 |
GaN (mp-804) | <1 0 1> | <0 1 0> | 175.6 |
GaN (mp-804) | <1 1 0> | <1 -1 1> | 310.6 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 223.7 |
YVO4 (mp-19133) | <1 1 0> | <0 0 1> | 186.4 |
SiO2 (mp-6930) | <0 0 1> | <0 1 -1> | 256.7 |
SiO2 (mp-6930) | <1 0 1> | <0 1 0> | 307.4 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 194.4 |
Te2Mo (mp-602) | <1 0 1> | <1 1 0> | 272.2 |
Te2Mo (mp-602) | <1 1 0> | <0 0 1> | 186.4 |
Te2Mo (mp-602) | <1 1 1> | <1 0 0> | 97.2 |
Ag (mp-124) | <1 0 0> | <0 1 -1> | 51.3 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 74.6 |
Ag (mp-124) | <1 1 1> | <0 1 -1> | 154.0 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 -1> | 154.0 |
DyScO3 (mp-31120) | <1 0 0> | <1 -1 0> | 314.2 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 111.9 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
LiCoS2 (mp-753946) | 0.7186 | 0.003 | 3 |
Cr10Sb3Te7 (mp-676935) | 0.5578 | 0.149 | 3 |
LiNi9S10 (mp-676685) | 0.1829 | 0.095 | 3 |
TmAgTe2 (mp-12953) | 0.6092 | 0.016 | 3 |
GdAgSe2 (mp-1097028) | 0.6729 | 0.012 | 3 |
VS (mp-849065) | 0.3147 | 0.244 | 2 |
ZrB (mp-1014246) | 0.2958 | 0.330 | 2 |
ErH (mp-1007906) | 0.2989 | 0.169 | 2 |
VTe (mp-10256) | 0.2976 | 0.150 | 2 |
CrSb (mp-1641) | 0.3004 | 0.098 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Li_sv Ni_pv S |
Final Energy/Atom-5.1085 eV |
Corrected Energy-108.8055 eV
-108.8055 eV = -102.1709 eV (uncorrected energy) - 6.6346 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)