Final Magnetic Moment10.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.115 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.100 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.85 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi24Mn11CrO36 + LiMnCrO4 + MnCr2O4 + Mn3O4 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCmce [64] |
Hall-C 2bc 2 |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
CeO2 (mp-20194) | <1 1 1> | <0 1 1> | 211.1 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 137.8 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 275.5 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 137.8 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 321.4 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 321.4 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 321.4 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 137.8 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 229.6 |
InAs (mp-20305) | <1 1 1> | <1 0 0> | 269.2 |
KTaO3 (mp-3614) | <1 0 0> | <1 1 0> | 208.8 |
LiF (mp-1138) | <1 0 0> | <0 1 1> | 281.5 |
LiF (mp-1138) | <1 1 0> | <0 1 0> | 213.3 |
Te2W (mp-22693) | <0 0 1> | <0 1 0> | 266.7 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 275.5 |
YVO4 (mp-19133) | <0 0 1> | <1 1 0> | 104.4 |
YVO4 (mp-19133) | <1 1 0> | <0 1 0> | 266.7 |
TePb (mp-19717) | <1 0 0> | <1 1 0> | 208.8 |
AlN (mp-661) | <1 0 0> | <0 1 0> | 160.0 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 269.2 |
AlN (mp-661) | <1 1 1> | <0 1 1> | 140.8 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 229.6 |
BaF2 (mp-1029) | <1 1 0> | <1 0 0> | 269.2 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 229.6 |
SiO2 (mp-6930) | <0 0 1> | <0 1 0> | 266.7 |
KCl (mp-23193) | <1 0 0> | <1 1 0> | 208.8 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 229.6 |
InAs (mp-20305) | <1 1 0> | <1 0 0> | 269.2 |
CdS (mp-672) | <0 0 1> | <0 1 0> | 266.7 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 275.5 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 275.5 |
Ag (mp-124) | <1 1 1> | <0 1 0> | 213.3 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 137.8 |
GaSe (mp-1943) | <1 0 0> | <1 0 1> | 201.6 |
GaSe (mp-1943) | <1 0 1> | <0 1 0> | 213.3 |
BN (mp-984) | <0 0 1> | <0 0 1> | 229.6 |
BN (mp-984) | <1 0 0> | <0 1 0> | 160.0 |
BN (mp-984) | <1 0 1> | <0 1 0> | 160.0 |
BN (mp-984) | <1 1 0> | <0 0 1> | 137.8 |
BN (mp-984) | <1 1 1> | <0 0 1> | 137.8 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 45.9 |
LiGaO2 (mp-5854) | <0 0 1> | <0 1 1> | 140.8 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 275.5 |
SiC (mp-7631) | <1 1 0> | <0 1 0> | 160.0 |
Al (mp-134) | <1 0 0> | <0 1 1> | 281.5 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 137.8 |
LiGaO2 (mp-5854) | <0 1 1> | <0 1 0> | 266.7 |
LiGaO2 (mp-5854) | <1 1 1> | <1 0 0> | 269.2 |
LiTaO3 (mp-3666) | <0 0 1> | <0 0 1> | 45.9 |
MgO (mp-1265) | <1 1 1> | <0 1 0> | 213.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li2Cr3O6 (mp-771534) | 0.1439 | 0.114 | 3 |
Li5Fe5O12 (mp-771687) | 0.2677 | 0.091 | 3 |
Li2Mn3O6 (mp-773276) | 0.2604 | 0.098 | 3 |
Li2(NiO2)3 (mp-773252) | 0.2577 | 0.241 | 3 |
TlIn5S7 (mp-562480) | 0.5345 | 0.000 | 3 |
Li4TiCr5O12 (mp-771562) | 0.1163 | 0.105 | 4 |
Li2TiCr2O6 (mp-767334) | 0.1111 | 0.082 | 4 |
Li2Co2SnO6 (mp-768010) | 0.1313 | 0.101 | 4 |
Li2Mn2FeO6 (mp-774086) | 0.0696 | 0.107 | 4 |
Li4MnCr5O12 (mp-771221) | 0.1281 | 0.096 | 4 |
In6Se7 (mp-567596) | 0.6204 | 0.042 | 2 |
In6S7 (mp-555853) | 0.5444 | 0.008 | 2 |
Li4Ti4MnCr4O18 (mp-769442) | 0.6238 | 0.092 | 5 |
Li4Ti4V4CoO18 (mp-769478) | 0.6616 | 0.092 | 5 |
Li4Ti4Mn(Fe2O9)2 (mp-769443) | 0.6639 | 0.087 | 5 |
Li4Ti4VCr4O18 (mp-775391) | 0.6548 | 0.085 | 5 |
Li4Ti2Fe4(CoO6)3 (mp-776197) | 0.6450 | 0.217 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eVCr: 3.7 eV |
PseudopotentialsVASP PAW: Li_sv Mn_pv Cr_pv O |
Final Energy/Atom-6.8326 eV |
Corrected Energy-169.4932 eV
-169.4932 eV = -150.3163 eV (uncorrected energy) - 10.7494 eV (MP Advanced Correction) - 8.4275 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)