Final Magnetic Moment19.003 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.218 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.119 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.45 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToFe2NiO4 + LiNbO3 + Li3NbO4 + NiO |
Band Gap0.511 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCm [8] |
HallC 2y |
Point Groupm |
Crystal Systemmonoclinic |
sign indicates spin ↑ ↓
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 0 1> | 322.4 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 239.7 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 193.5 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 257.9 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 257.9 |
InAs (mp-20305) | <1 1 0> | <1 0 1> | 264.9 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 322.4 |
BaF2 (mp-1029) | <1 1 0> | <1 0 1> | 264.9 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 239.7 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 0> | 207.4 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 322.4 |
GaN (mp-804) | <0 0 1> | <0 1 0> | 207.4 |
GaN (mp-804) | <1 0 1> | <1 0 1> | 264.9 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 322.4 |
DyScO3 (mp-31120) | <1 1 1> | <0 1 0> | 207.4 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 193.5 |
YVO4 (mp-19133) | <1 0 1> | <0 1 0> | 207.4 |
Te2Mo (mp-602) | <0 0 1> | <1 0 1> | 88.3 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 322.4 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 322.4 |
Te2Mo (mp-602) | <1 1 1> | <0 0 1> | 193.5 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 257.9 |
CdS (mp-672) | <1 1 0> | <1 0 0> | 299.6 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 193.5 |
LiNbO3 (mp-3731) | <1 1 0> | <1 0 1> | 264.9 |
BN (mp-984) | <1 1 1> | <1 0 0> | 299.6 |
Al (mp-134) | <1 1 0> | <0 1 0> | 207.4 |
LiNbO3 (mp-3731) | <1 0 1> | <0 0 1> | 322.4 |
MoS2 (mp-1434) | <1 0 0> | <0 1 0> | 207.4 |
Al (mp-134) | <1 0 0> | <1 0 0> | 239.7 |
SiC (mp-7631) | <0 0 1> | <1 0 1> | 264.9 |
LiTaO3 (mp-3666) | <0 0 1> | <0 0 1> | 193.5 |
LiGaO2 (mp-5854) | <0 1 0> | <1 0 0> | 239.7 |
LiGaO2 (mp-5854) | <1 1 1> | <0 0 1> | 322.4 |
MgO (mp-1265) | <1 0 0> | <1 0 0> | 179.8 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 193.5 |
SiC (mp-7631) | <1 0 1> | <0 0 1> | 193.5 |
Fe3O4 (mp-19306) | <1 1 1> | <0 0 1> | 129.0 |
MgO (mp-1265) | <1 1 0> | <0 0 1> | 129.0 |
MgO (mp-1265) | <1 1 1> | <0 0 1> | 64.5 |
TiO2 (mp-2657) | <1 1 1> | <0 0 1> | 257.9 |
Mg (mp-153) | <1 0 0> | <1 0 0> | 179.8 |
C (mp-66) | <1 1 0> | <1 0 0> | 299.6 |
GdScO3 (mp-5690) | <1 1 1> | <0 1 0> | 207.4 |
LaF3 (mp-905) | <0 0 1> | <0 0 1> | 129.0 |
PbS (mp-21276) | <1 1 0> | <0 0 1> | 257.9 |
InP (mp-20351) | <1 0 0> | <1 0 1> | 176.6 |
InP (mp-20351) | <1 1 0> | <0 0 1> | 257.9 |
LaF3 (mp-905) | <1 0 0> | <0 0 1> | 322.4 |
PbS (mp-21276) | <1 0 0> | <1 0 0> | 179.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Fe2CuO4 (mp-705659) | 0.2788 | 0.074 | 3 |
Mg(SnO2)2 (mvc-9524) | 0.2878 | 0.270 | 3 |
Zn(SnO2)2 (mvc-9533) | 0.2981 | 0.245 | 3 |
Ca(WO2)2 (mvc-10243) | 0.2851 | 0.333 | 3 |
Ca(WO2)2 (mvc-10486) | 0.2342 | 0.389 | 3 |
Li4Mn5Nb3O16 (mp-773388) | 0.2007 | 0.082 | 4 |
Li6Cr3Sb3O16 (mp-773191) | 0.2354 | 0.080 | 4 |
Li4Mn5Sb3O16 (mp-769848) | 0.1612 | 0.036 | 4 |
Li4Mn5V3O16 (mp-773194) | 0.2148 | 0.068 | 4 |
Li4Co5Sb3O16 (mp-771118) | 0.1878 | 0.076 | 4 |
Si3N4 (mp-641539) | 0.4733 | 0.287 | 2 |
Ge3N4 (mp-641541) | 0.4351 | 0.207 | 2 |
Fe3O4 (mp-542433) | 0.4845 | 0.034 | 2 |
Fe3O4 (mp-650112) | 0.4726 | 0.041 | 2 |
Fe3O4 (mp-715811) | 0.4857 | 0.018 | 2 |
Li4Cr3Co2Sb3O16 (mp-764773) | 0.1249 | 0.068 | 5 |
Li4Nb3V3(NiO8)2 (mp-771722) | 0.1317 | 0.152 | 5 |
Li4V3Co2Sb3O16 (mp-770636) | 0.1268 | 0.055 | 5 |
Li4Cr3Fe2Sb3O16 (mp-773763) | 0.1016 | 0.143 | 5 |
Li4V3Fe2Sb3O16 (mp-853181) | 0.0861 | 0.041 | 5 |
Li3MnFeCo(PO4)3 (mp-764809) | 0.7467 | 0.030 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesFe: 5.3 eVNi: 6.2 eV |
PseudopotentialsVASP PAW: Li_sv Nb_pv Fe_pv Ni_pv O |
Final Energy/Atom-6.8739 eV |
Corrected Energy-216.2325 eV
-216.2325 eV = -192.4689 eV (uncorrected energy) - 12.5270 eV (MP Advanced Correction) - 11.2366 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)