Final Magnetic Moment11.317 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.196 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.073 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.85 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCo3(PO4)2 + CoPO4 + CoO2 + SnP2O7 |
Band Gap0.213 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPm [6] |
HallP 2y |
Point Groupm |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 0> | <0 0 1> | 205.8 |
AlN (mp-661) | <0 0 1> | <0 1 0> | 194.9 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 235.2 |
AlN (mp-661) | <1 1 1> | <1 0 1> | 198.9 |
GaAs (mp-2534) | <1 1 0> | <0 1 1> | 284.5 |
GaN (mp-804) | <0 0 1> | <0 1 1> | 284.5 |
GaN (mp-804) | <1 0 0> | <1 1 0> | 153.3 |
GaN (mp-804) | <1 1 0> | <1 0 1> | 265.1 |
SiO2 (mp-6930) | <1 0 0> | <0 1 0> | 194.9 |
SiO2 (mp-6930) | <1 1 1> | <1 0 1> | 265.1 |
DyScO3 (mp-31120) | <1 0 0> | <0 1 1> | 284.5 |
InAs (mp-20305) | <1 0 0> | <0 1 0> | 194.9 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 264.6 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 323.3 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 1> | 284.5 |
KTaO3 (mp-3614) | <1 1 1> | <0 1 0> | 194.9 |
CdS (mp-672) | <1 0 0> | <0 1 0> | 341.1 |
CdS (mp-672) | <1 1 0> | <0 1 1> | 341.4 |
LiF (mp-1138) | <1 1 1> | <0 1 0> | 194.9 |
Te2W (mp-22693) | <0 0 1> | <0 1 0> | 341.1 |
Te2W (mp-22693) | <0 1 1> | <0 1 0> | 292.4 |
YVO4 (mp-19133) | <1 0 1> | <0 1 0> | 146.2 |
Te2Mo (mp-602) | <1 1 0> | <0 0 1> | 293.9 |
Ag (mp-124) | <1 1 1> | <1 0 0> | 59.2 |
GaSe (mp-1943) | <0 0 1> | <1 0 0> | 177.6 |
BN (mp-984) | <1 1 1> | <0 0 1> | 205.8 |
LiNbO3 (mp-3731) | <1 0 1> | <0 1 1> | 227.6 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 1 0> | 292.4 |
MoS2 (mp-1434) | <1 1 0> | <0 1 0> | 243.6 |
Al (mp-134) | <1 0 0> | <0 0 1> | 235.2 |
Al (mp-134) | <1 1 1> | <0 1 0> | 194.9 |
LiGaO2 (mp-5854) | <0 0 1> | <1 0 1> | 331.4 |
LiGaO2 (mp-5854) | <0 1 1> | <0 1 0> | 341.1 |
LiGaO2 (mp-5854) | <1 0 1> | <0 1 1> | 227.6 |
TeO2 (mp-2125) | <1 1 0> | <0 0 1> | 293.9 |
LaAlO3 (mp-2920) | <0 0 1> | <0 1 1> | 341.4 |
AlN (mp-661) | <1 0 0> | <0 1 1> | 170.7 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 205.8 |
CeO2 (mp-20194) | <1 0 0> | <0 1 0> | 243.6 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 293.9 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 323.3 |
BaF2 (mp-1029) | <1 0 0> | <0 1 0> | 194.9 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 58.8 |
GaN (mp-804) | <1 1 1> | <0 1 0> | 243.6 |
SiO2 (mp-6930) | <0 0 1> | <0 1 1> | 170.7 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 205.8 |
KCl (mp-23193) | <1 0 0> | <0 1 0> | 194.9 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 1> | 246.8 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 1> | 331.4 |
DyScO3 (mp-31120) | <1 0 1> | <1 1 0> | 230.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
FePO4 (mp-25001) | 0.1583 | 0.024 | 3 |
CoPO4 (mp-510669) | 0.2828 | 0.197 | 3 |
PWO4 (mp-25654) | 0.3280 | 0.108 | 3 |
TiPO4 (mp-25435) | 0.2497 | 0.128 | 3 |
VPO4 (mp-32453) | 0.2670 | 0.112 | 3 |
VFe(PO4)2 (mp-775394) | 0.1518 | 0.200 | 4 |
CoSb(PO4)2 (mp-775019) | 0.1917 | 0.079 | 4 |
TiCo3(PO4)4 (mp-863879) | 0.1784 | 0.068 | 4 |
CoSn(PO4)2 (mp-863848) | 0.2020 | 0.039 | 4 |
VCo3(PO4)4 (mp-761621) | 0.1912 | 0.164 | 4 |
CrO2 (mvc-11581) | 0.7241 | 0.351 | 2 |
VO2 (mp-777469) | 0.7304 | 0.038 | 2 |
Cr5O12 (mp-19575) | 0.6665 | 0.142 | 2 |
VO2 (mvc-6918) | 0.6679 | 0.095 | 2 |
MoO2 (mvc-6944) | 0.6057 | 0.387 | 2 |
MnFeCo(PO4)3 (mp-764410) | 0.2850 | 0.027 | 5 |
MnFeCo(PO4)3 (mp-764392) | 0.2783 | 0.028 | 5 |
MnFeCo(PO4)3 (mp-763496) | 0.2580 | 0.026 | 5 |
MnFeCo(PO4)3 (mp-764383) | 0.2887 | 0.038 | 5 |
MnFeCo(PO4)3 (mp-764739) | 0.2728 | 0.023 | 5 |
Li4Mn3CrCo2(PO4)6 (mp-763479) | 0.6179 | 0.080 | 6 |
LiMgCr3Se2(SO6)4 (mp-769552) | 0.5287 | 0.003 | 6 |
NaLi3Ti2Cr2(PO4)6 (mp-777190) | 0.5439 | 0.028 | 6 |
LiTi3MnCr(PO4)6 (mp-772224) | 0.5873 | 0.001 | 6 |
Li2Ti2MnCr2(PO4)6 (mp-777244) | 0.5971 | 0.015 | 6 |
Ca2Al2FeSi4BHO16 (mp-540713) | 0.7436 | 0.068 | 7 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesCo: 3.32 eV |
PseudopotentialsVASP PAW: Co Sn_d P O |
Final Energy/Atom-6.7491 eV |
Corrected Energy-178.8382 eV
-178.8382 eV = -161.9796 eV (uncorrected energy) - 11.2366 eV (MP Anion Correction) - 5.6220 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)