Final Magnetic Moment8.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-1.891 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.890 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.18 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToNiO + Li2O + Li4CrFe3O8 + LiCrO2 |
Band Gap1.633 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCm [8] |
HallC 2y |
Point Groupm |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <1 0 0> | 234.7 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 123.6 |
GaN (mp-804) | <1 0 0> | <0 1 0> | 102.0 |
GaN (mp-804) | <1 1 0> | <1 1 1> | 266.0 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 0> | 203.9 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 309.1 |
YVO4 (mp-19133) | <1 1 0> | <0 1 0> | 203.9 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 176.1 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 123.6 |
BN (mp-984) | <0 0 1> | <1 0 0> | 176.1 |
LiNbO3 (mp-3731) | <1 0 1> | <0 0 1> | 309.1 |
LiNbO3 (mp-3731) | <1 1 0> | <1 0 1> | 256.3 |
GaN (mp-804) | <1 0 1> | <1 0 1> | 170.9 |
SiO2 (mp-6930) | <0 0 1> | <1 0 0> | 176.1 |
Al (mp-134) | <1 0 0> | <0 0 1> | 247.2 |
Al (mp-134) | <1 1 0> | <0 1 0> | 203.9 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 247.2 |
CdS (mp-672) | <1 0 1> | <1 0 0> | 293.4 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 247.2 |
LiTaO3 (mp-3666) | <0 0 1> | <0 0 1> | 185.4 |
LiTaO3 (mp-3666) | <1 1 0> | <1 0 1> | 256.3 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 61.8 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 185.4 |
MgO (mp-1265) | <1 1 0> | <0 0 1> | 123.6 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 309.1 |
GaSe (mp-1943) | <0 0 1> | <1 0 0> | 176.1 |
C (mp-66) | <1 1 0> | <1 0 0> | 176.1 |
C (mp-66) | <1 1 1> | <1 0 0> | 176.1 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 185.4 |
MoS2 (mp-1434) | <1 0 0> | <0 1 0> | 203.9 |
Mg (mp-153) | <1 0 1> | <1 0 1> | 170.9 |
LiGaO2 (mp-5854) | <0 1 0> | <1 0 0> | 234.7 |
SiC (mp-7631) | <1 0 0> | <1 0 0> | 234.7 |
SiC (mp-7631) | <1 0 1> | <0 1 1> | 238.5 |
LiTaO3 (mp-3666) | <1 0 1> | <0 0 1> | 309.1 |
Fe3O4 (mp-19306) | <1 1 1> | <0 0 1> | 123.6 |
MgO (mp-1265) | <1 1 1> | <0 0 1> | 61.8 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 309.1 |
BaTiO3 (mp-5986) | <1 0 0> | <0 0 1> | 247.2 |
C (mp-66) | <1 0 0> | <0 1 0> | 102.0 |
MoSe2 (mp-1634) | <0 0 1> | <0 0 1> | 123.6 |
Mg (mp-153) | <1 0 0> | <0 0 1> | 247.2 |
PbS (mp-21276) | <1 0 0> | <1 0 0> | 176.1 |
PbS (mp-21276) | <1 1 0> | <0 0 1> | 247.2 |
InP (mp-20351) | <1 0 0> | <1 0 0> | 176.1 |
InP (mp-20351) | <1 1 0> | <0 0 1> | 247.2 |
Ni (mp-23) | <1 0 0> | <1 0 0> | 293.4 |
Ni (mp-23) | <1 1 0> | <1 0 0> | 176.1 |
BaTiO3 (mp-5986) | <0 0 1> | <1 0 0> | 234.7 |
BaTiO3 (mp-5986) | <1 0 1> | <1 0 0> | 117.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li5(NiO2)4 (mp-780518) | 0.3996 | 0.327 | 3 |
Li5(FeO2)4 (mp-780312) | 0.1783 | 0.259 | 3 |
Li12Cr5O16 (mp-764428) | 0.6107 | 0.177 | 3 |
Li5(CoO2)4 (mp-780140) | 0.2349 | 0.251 | 3 |
Li5Cr4O8 (mp-850237) | 0.2989 | 0.101 | 3 |
Li5Cr3NiO8 (mp-764311) | 0.1195 | 0.279 | 4 |
Li10Fe5Co3O16 (mp-763869) | 0.1875 | 0.090 | 4 |
Li10V5Cr3O16 (mp-764037) | 0.1060 | 0.081 | 4 |
Li5VCr3O8 (mp-765717) | 0.1979 | 0.084 | 4 |
Li5MnCr3O8 (mp-765322) | 0.1705 | 0.063 | 4 |
Ti3N4 (mp-1080192) | 0.7064 | 0.101 | 2 |
Li10Cr3Co2Ni3O16 (mp-778771) | 0.2185 | 0.263 | 5 |
Li10Mn3Cr3(CoO8)2 (mp-780494) | 0.2203 | 0.074 | 5 |
Li10Cr2Fe3Co3O16 (mp-774310) | 0.1650 | 0.811 | 5 |
Li10Mn2V3Cr3O16 (mp-765364) | 0.1886 | 0.058 | 5 |
Li10Fe3Co3(NiO8)2 (mp-774318) | 0.1720 | 0.134 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesCr: 3.7 eVFe: 5.3 eV Ni: 6.2 eV |
PseudopotentialsVASP PAW: Li_sv Cr_pv Fe_pv Ni_pv O |
Final Energy/Atom-5.8439 eV |
Corrected Energy-228.4968 eV
-228.4968 eV = -198.6941 eV (uncorrected energy) - 18.5660 eV (MP Advanced Correction) - 11.2366 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)