Final Magnetic Moment9.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.439 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.069 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.12 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiMnBO3 + Mn2BO4 + Mn3O4 + Li3B7O12 |
Band Gap0.565 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPc [7] |
HallP 2yc |
Point Groupm |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
GaN (mp-804) | <0 0 1> | <0 1 1> | 292.8 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 240.8 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 144.5 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 289.0 |
SiO2 (mp-6930) | <1 0 0> | <0 1 1> | 219.6 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 337.1 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 240.8 |
KCl (mp-23193) | <1 1 0> | <1 0 0> | 281.3 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 144.5 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 240.8 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 337.1 |
DyScO3 (mp-31120) | <1 0 0> | <0 1 0> | 275.6 |
DyScO3 (mp-31120) | <1 1 1> | <0 1 0> | 275.6 |
ZnSe (mp-1190) | <1 1 0> | <0 1 0> | 275.6 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 0> | 275.6 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 289.0 |
LiF (mp-1138) | <1 0 0> | <1 1 0> | 217.5 |
LiF (mp-1138) | <1 1 0> | <0 1 0> | 275.6 |
YVO4 (mp-19133) | <1 0 0> | <0 1 0> | 275.6 |
TePb (mp-19717) | <1 0 0> | <1 1 0> | 217.5 |
TePb (mp-19717) | <1 1 0> | <0 0 1> | 240.8 |
TePb (mp-19717) | <1 1 1> | <0 0 1> | 144.5 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 289.0 |
Ag (mp-124) | <1 0 0> | <0 1 0> | 275.6 |
BN (mp-984) | <0 0 1> | <0 1 0> | 330.8 |
BN (mp-984) | <1 0 0> | <0 1 1> | 292.8 |
BN (mp-984) | <1 1 0> | <0 1 0> | 165.4 |
BN (mp-984) | <1 1 1> | <1 1 1> | 240.5 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 48.2 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 289.0 |
MoS2 (mp-1434) | <0 0 1> | <0 1 1> | 292.8 |
LaAlO3 (mp-2920) | <0 0 1> | <0 1 0> | 330.8 |
LaAlO3 (mp-2920) | <1 0 0> | <0 0 1> | 144.5 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 337.1 |
AlN (mp-661) | <1 0 0> | <0 1 1> | 219.6 |
Al (mp-134) | <1 1 0> | <0 1 0> | 275.6 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 192.7 |
LiGaO2 (mp-5854) | <1 0 0> | <0 0 1> | 240.8 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 192.7 |
AlN (mp-661) | <1 1 1> | <1 0 0> | 281.3 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 144.5 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 240.8 |
GaAs (mp-2534) | <1 1 0> | <0 1 0> | 275.6 |
LiGaO2 (mp-5854) | <1 1 0> | <0 1 0> | 330.8 |
LiGaO2 (mp-5854) | <1 1 1> | <1 0 0> | 281.3 |
CdTe (mp-406) | <1 0 0> | <1 1 0> | 217.5 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 240.8 |
BaF2 (mp-1029) | <1 1 0> | <1 0 0> | 281.3 |
BaF2 (mp-1029) | <1 1 1> | <1 0 0> | 281.3 |
TeO2 (mp-2125) | <0 1 0> | <0 1 0> | 275.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li3BO3 (mp-27275) | 0.7006 | 0.000 | 3 |
Li6B4O9 (mp-768875) | 0.6209 | 0.063 | 3 |
Na3CoO3 (mp-777919) | 0.6539 | 0.018 | 3 |
Li6B4O9 (mp-1020024) | 0.5988 | 0.000 | 3 |
LiMn2(BO3)2 (mp-779335) | 0.2978 | 0.077 | 4 |
Li5Mn8(BO3)8 (mp-778679) | 0.2497 | 0.055 | 4 |
LiMn2(BO3)2 (mp-849990) | 0.3134 | 0.073 | 4 |
LiMn2(BO3)2 (mp-781074) | 0.2827 | 0.074 | 4 |
LiMn2(BO3)2 (mp-778551) | 0.2809 | 0.071 | 4 |
Li4Mn2Fe(BO3)4 (mp-767650) | 0.3633 | 0.067 | 5 |
Li3Mn2Fe(BO3)4 (mp-767643) | 0.5101 | 0.070 | 5 |
Li8MnFe7(BO3)8 (mp-850743) | 0.6565 | 0.017 | 5 |
Li4MnFe2(BO3)4 (mp-767642) | 0.4333 | 0.055 | 5 |
Li8Mn3Fe5(BO3)8 (mp-778883) | 0.6417 | 0.015 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eV |
PseudopotentialsVASP PAW: Li_sv Mn_pv B O |
Final Energy/Atom-7.5031 eV |
Corrected Energy-360.4364 eV
-360.4364 eV = -330.1346 eV (uncorrected energy) - 16.8550 eV (MP Anion Correction) - 13.4468 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)