Final Magnetic Moment9.975 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.303 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.056 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.39 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiCrO2 + CrWO4 |
Band Gap2.184 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP63mc [186] |
HallP 6c 2c |
Point Group6mm |
Crystal Systemhexagonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 92.4 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 277.1 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 277.1 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 215.6 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 246.3 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 1> | 326.0 |
CdS (mp-672) | <0 0 1> | <1 0 1> | 326.0 |
CdS (mp-672) | <1 0 0> | <1 0 1> | 195.6 |
CdS (mp-672) | <1 0 1> | <1 0 0> | 287.3 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 246.3 |
LiF (mp-1138) | <1 1 0> | <1 0 1> | 326.0 |
Te2W (mp-22693) | <0 0 1> | <1 1 0> | 199.1 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 154.0 |
YVO4 (mp-19133) | <1 1 0> | <1 1 0> | 199.1 |
TePb (mp-19717) | <1 1 1> | <0 0 1> | 215.6 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 277.1 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 277.1 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 154.0 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 123.2 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 30.8 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 123.2 |
GaSe (mp-1943) | <1 0 1> | <1 1 1> | 208.4 |
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 215.6 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 215.6 |
BN (mp-984) | <0 0 1> | <0 0 1> | 215.6 |
BN (mp-984) | <1 0 0> | <0 0 1> | 338.7 |
BN (mp-984) | <1 0 1> | <0 0 1> | 215.6 |
BN (mp-984) | <1 1 0> | <0 0 1> | 277.1 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 215.6 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 229.9 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 123.2 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 277.1 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 215.6 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 92.4 |
LiNbO3 (mp-3731) | <1 0 0> | <1 1 0> | 298.6 |
LiNbO3 (mp-3731) | <1 0 1> | <1 1 0> | 298.6 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 277.1 |
GaAs (mp-2534) | <1 1 0> | <1 0 1> | 326.0 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 215.6 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 215.6 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 277.1 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 338.7 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 246.3 |
GaN (mp-804) | <1 1 0> | <1 0 1> | 260.8 |
SiO2 (mp-6930) | <1 1 1> | <1 0 1> | 260.8 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 215.6 |
Al (mp-134) | <1 0 0> | <0 0 1> | 246.3 |
Al (mp-134) | <1 1 0> | <1 0 1> | 326.0 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 1> | 326.0 |
ZnSe (mp-1190) | <1 1 0> | <1 0 1> | 326.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li(CoO2)2 (mp-771481) | 0.2143 | 0.136 | 3 |
Li(FeO2)2 (mp-771571) | 0.1776 | 0.665 | 3 |
LiCr2O4 (mp-771523) | 0.1819 | 0.088 | 3 |
LiTi2O4 (mp-776170) | 0.1328 | 0.042 | 3 |
Li3FeO3 (mp-770886) | 0.2139 | 0.361 | 3 |
Li2NbCr3O8 (mp-762276) | 0.1058 | 0.000 | 4 |
Li2V3WO8 (mp-775204) | 0.0856 | 0.064 | 4 |
Li2NbV3O8 (mp-777682) | 0.1046 | 0.000 | 4 |
Li2Cr3SbO8 (mp-772283) | 0.0735 | 0.003 | 4 |
Li2V3SbO8 (mp-774145) | 0.1108 | 0.010 | 4 |
Fe3O4 (mp-715491) | 0.3260 | 0.017 | 2 |
Fe3O4 (mp-542433) | 0.3352 | 0.075 | 2 |
Mn3N4 (mp-1080204) | 0.3325 | 0.172 | 2 |
Cr3N4 (mp-1014358) | 0.2742 | 0.226 | 2 |
Fe3O4 (mp-650112) | 0.3186 | 0.060 | 2 |
Li4V3Cr3(SbO8)2 (mp-777249) | 0.0775 | 0.037 | 5 |
Li2Cr2FeSbO8 (mp-861530) | 0.0786 | 4.856 | 5 |
Li4V3Cr3(WO8)2 (mp-772356) | 0.0757 | 0.006 | 5 |
Li4Cr3Cu3(SbO8)2 (mp-783908) | 0.1099 | 0.035 | 5 |
Li4Cr3Fe3(SbO8)2 (mp-771925) | 0.1172 | 6.495 | 5 |
Li3MnFeCo(PO4)3 (mp-764931) | 0.6468 | 0.017 | 6 |
Li3MnFeCo(PO4)3 (mp-764809) | 0.6373 | 0.014 | 6 |
Li3MnFeCo(PO4)3 (mp-764869) | 0.6408 | 0.032 | 6 |
Li3MnFeCo(PO4)3 (mp-764969) | 0.6428 | 0.057 | 6 |
Li3MnFeCo(PO4)3 (mp-764870) | 0.6432 | 0.466 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesCr: 3.7 eVW: 6.2 eV |
PseudopotentialsVASP PAW: Li_sv Cr_pv W_pv O |
Final Energy/Atom-7.2539 eV |
Corrected Energy-235.1245 eV
-235.1245 eV = -203.1079 eV (uncorrected energy) - 20.7800 eV (MP Advanced Correction) - 11.2366 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)