Final Magnetic Moment49.142 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.770 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.013 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.41 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToNaFe(SiO3)2 + SiO2 + Fe2O3 + O2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [1] |
HallP 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <0 1 1> | 156.7 |
DyScO3 (mp-31120) | <0 1 1> | <0 1 1> | 156.7 |
DyScO3 (mp-31120) | <1 1 1> | <0 1 -1> | 140.2 |
GdScO3 (mp-5690) | <1 1 1> | <0 1 -1> | 140.2 |
LiNbO3 (mp-3731) | <0 0 1> | <1 0 -1> | 141.2 |
LiGaO2 (mp-5854) | <0 1 1> | <0 1 0> | 218.8 |
GaP (mp-2490) | <1 1 0> | <0 1 0> | 218.8 |
TbScO3 (mp-31119) | <1 1 1> | <0 1 -1> | 140.2 |
LiTaO3 (mp-3666) | <0 0 1> | <1 0 -1> | 141.2 |
NdGaO3 (mp-3196) | <0 1 0> | <0 1 0> | 218.8 |
NdGaO3 (mp-3196) | <0 1 1> | <0 1 1> | 156.7 |
NdGaO3 (mp-3196) | <1 1 1> | <0 1 -1> | 140.2 |
TiO2 (mp-390) | <1 1 0> | <0 1 1> | 156.7 |
MgF2 (mp-1249) | <1 0 0> | <0 0 1> | 100.7 |
ZnO (mp-2133) | <1 0 0> | <0 1 1> | 156.7 |
SrTiO3 (mp-4651) | <1 0 0> | <0 1 0> | 218.8 |
SrTiO3 (mp-4651) | <1 1 1> | <0 1 -1> | 140.2 |
CaF2 (mp-2741) | <1 1 0> | <0 1 0> | 218.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
LaWN3 (mp-989633) | 0.5640 | 0.011 | 3 |
Cr3(P2O7)2 (mp-569271) | 0.5751 | 0.001 | 3 |
CdSiO3 (mp-776023) | 0.5558 | 0.027 | 3 |
P4W3O14 (mvc-1031) | 0.5252 | 0.315 | 3 |
MnSiO3 (mp-25041) | 0.5137 | 0.016 | 3 |
Na5Fe6(SiO3)12 (mp-767634) | 0.0680 | 0.021 | 4 |
NaFe2(SiO3)4 (mp-771678) | 0.1956 | 0.066 | 4 |
CaMn2(SiO3)4 (mvc-12762) | 0.3372 | 0.064 | 4 |
CaFe2(SiO3)4 (mvc-11952) | 0.3575 | 0.091 | 4 |
LiCoP2O7 (mp-31519) | 0.3686 | 0.075 | 4 |
MoO2 (mvc-6944) | 0.6833 | 0.387 | 2 |
NaLi7Fe8(SiO3)16 (mp-775490) | 0.4615 | 0.011 | 5 |
NaLiFe2(SiO3)4 (mp-853133) | 0.4192 | 0.198 | 5 |
NaLi3Fe4(SiO3)8 (mp-775132) | 0.4354 | 0.011 | 5 |
NaLi3Fe4(SiO3)8 (mp-775021) | 0.4246 | 0.011 | 5 |
Ca2Mg5Si8(O11F)2 (mp-557662) | 0.4656 | 0.000 | 5 |
Na2Ca6Mg7Fe(SiO3)16 (mp-745155) | 0.5163 | 0.031 | 6 |
NaCa3ScZn3(SiO3)8 (mp-693463) | 0.5094 | 0.029 | 6 |
NaCa2ScZn2(SiO3)6 (mp-534778) | 0.5043 | 0.025 | 6 |
KCa5Mg5Al(SiO3)12 (mp-534793) | 0.5156 | 0.033 | 6 |
Na5CaAl5Fe(SiO3)12 (mp-744927) | 0.4759 | 0.034 | 6 |
Ca2Al2FeSi4BHO16 (mp-540713) | 0.6320 | 0.068 | 7 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesFe: 5.3 eV |
PseudopotentialsVASP PAW: Na_pv Fe_pv Si O |
Final Energy/Atom-7.1375 eV |
Corrected Energy-776.0769 eV
-776.0769 eV = -706.6095 eV (uncorrected energy) - 42.1374 eV (MP Anion Correction) - 27.3300 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)