Final Magnetic Moment1.998 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.998 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.039 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.61 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi2CrO4 + SiO2 + Li2Si2O5 + Cr2O3 |
Band Gap1.255 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCmce [64] |
Hall-C 2bc 2 |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
GaAs (mp-2534) | <1 1 0> | <0 1 0> | 142.5 |
SiO2 (mp-6930) | <1 0 1> | <0 1 0> | 142.5 |
ZnSe (mp-1190) | <1 1 0> | <0 1 0> | 142.5 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 0> | 170.2 |
LiF (mp-1138) | <1 1 0> | <0 1 0> | 142.5 |
Al (mp-134) | <1 1 1> | <1 0 0> | 170.2 |
LiGaO2 (mp-5854) | <0 1 1> | <1 0 0> | 170.2 |
Ni (mp-23) | <1 1 1> | <1 0 0> | 170.2 |
Ge(Bi3O5)4 (mp-23352) | <1 1 0> | <0 1 0> | 142.5 |
BaTiO3 (mp-5986) | <1 1 1> | <1 0 0> | 170.2 |
CaCO3 (mp-3953) | <1 0 0> | <1 0 0> | 170.2 |
Ge (mp-32) | <1 1 0> | <0 1 0> | 142.5 |
Fe2O3 (mp-24972) | <1 0 0> | <0 1 0> | 142.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li2V5O12 (mp-776871) | 0.6744 | 0.016 | 3 |
V4Cr2O13 (mp-851269) | 0.6040 | 0.113 | 3 |
V5FeO12 (mp-777454) | 0.6626 | 0.069 | 3 |
V5CoO12 (mp-761587) | 0.6461 | 0.174 | 3 |
V4Fe2O13 (mp-565529) | 0.6691 | 0.000 | 3 |
LiFe(Si2O5)3 (mp-775750) | 0.4947 | 0.102 | 4 |
Li2Fe(Si2O5)3 (mp-775303) | 0.4331 | 0.126 | 4 |
Li2V(Si2O5)3 (mp-775292) | 0.1235 | 0.023 | 4 |
LiCr(Si2O5)3 (mp-853182) | 0.5169 | 0.088 | 4 |
LiV(Si2O5)3 (mp-775301) | 0.5115 | 0.048 | 4 |
Li3Ti3Fe(PO4)6 (mp-743728) | 0.6504 | 0.013 | 5 |
Li8Fe7Co(PO4)12 (mp-781112) | 0.6839 | 0.016 | 5 |
Li8CrFe7(PO4)12 (mp-849438) | 0.6900 | 0.598 | 5 |
Li8NbFe7(PO4)12 (mp-776163) | 0.6911 | 0.000 | 5 |
NaLiZr(Si2O5)3 (mp-15543) | 0.5137 | 0.000 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesCr: 3.7 eV |
PseudopotentialsVASP PAW: Li_sv Cr_pv Si O |
Final Energy/Atom-7.4853 eV |
Corrected Energy-768.7760 eV
-768.7760 eV = -718.5866 eV (uncorrected energy) - 42.1374 eV (MP Anion Correction) - 8.0520 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)