Final Magnetic Moment13.032 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.040 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.065 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.70 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCoPO4 + Ni2P2O7 + O2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPm [6] |
HallP 2y |
Point Groupm |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 279.0 |
AlN (mp-661) | <0 0 1> | <0 1 0> | 142.2 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 111.6 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 55.8 |
AlN (mp-661) | <1 1 0> | <1 1 0> | 299.0 |
AlN (mp-661) | <1 1 1> | <1 0 1> | 193.5 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 306.9 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 251.1 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 195.3 |
SiO2 (mp-6930) | <1 0 1> | <0 1 0> | 142.2 |
SiO2 (mp-6930) | <1 1 0> | <1 0 1> | 193.5 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 1> | 322.4 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 55.8 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 167.4 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 195.3 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 251.1 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 334.8 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 139.5 |
LiF (mp-1138) | <1 1 1> | <1 0 0> | 57.8 |
Te2W (mp-22693) | <0 0 1> | <0 1 0> | 331.9 |
Te2W (mp-22693) | <0 1 1> | <1 1 0> | 299.0 |
TePb (mp-19717) | <1 1 0> | <0 1 0> | 189.6 |
Te2Mo (mp-602) | <1 0 0> | <0 1 0> | 331.9 |
Te2Mo (mp-602) | <1 0 1> | <0 1 0> | 331.9 |
Te2Mo (mp-602) | <1 1 0> | <0 0 1> | 195.3 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 167.4 |
Ag (mp-124) | <1 1 1> | <1 0 0> | 57.8 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 0 1> | 257.9 |
BN (mp-984) | <1 0 1> | <0 1 0> | 237.0 |
BN (mp-984) | <1 1 0> | <1 0 0> | 231.1 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 251.1 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 251.1 |
Al (mp-134) | <1 0 0> | <0 0 1> | 195.3 |
Al (mp-134) | <1 1 0> | <1 0 0> | 115.6 |
Al (mp-134) | <1 1 1> | <1 0 0> | 57.8 |
LiGaO2 (mp-5854) | <0 0 1> | <1 0 1> | 257.9 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 195.3 |
CdTe (mp-406) | <1 0 0> | <0 1 1> | 220.0 |
TeO2 (mp-2125) | <0 0 1> | <1 0 1> | 64.5 |
TeO2 (mp-2125) | <1 0 0> | <0 0 1> | 139.5 |
SiC (mp-7631) | <0 0 1> | <0 1 0> | 142.2 |
SiC (mp-7631) | <1 0 0> | <0 0 1> | 195.3 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 27.9 |
TiO2 (mp-2657) | <1 0 1> | <0 1 0> | 237.0 |
C (mp-66) | <1 1 0> | <0 1 0> | 142.2 |
C (mp-66) | <1 1 1> | <1 0 0> | 173.4 |
GdScO3 (mp-5690) | <0 0 1> | <1 0 1> | 64.5 |
GdScO3 (mp-5690) | <0 1 1> | <1 1 0> | 224.2 |
GdScO3 (mp-5690) | <1 1 0> | <0 0 1> | 334.8 |
Mg (mp-153) | <1 0 0> | <0 0 1> | 195.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
MnCrO4 (mp-780641) | 0.2370 | 0.104 | 3 |
Fe3(P2O7)2 (mvc-12221) | 0.3261 | 0.327 | 3 |
NiPO4 (mp-540008) | 0.2879 | 0.231 | 3 |
Fe3(P2O7)2 (mp-540486) | 0.3287 | 0.327 | 3 |
CrCoO4 (mp-766868) | 0.3152 | 0.244 | 3 |
FeCo(PO4)2 (mp-775299) | 0.1527 | 0.047 | 4 |
MnCo(PO4)2 (mp-775270) | 0.1373 | 0.051 | 4 |
MnFe(PO4)2 (mp-764401) | 0.1482 | 0.011 | 4 |
CoNi(PO4)2 (mp-766719) | 0.1092 | 0.157 | 4 |
Mn3Ni(PO4)4 (mp-771982) | 0.1028 | 0.027 | 4 |
FeO2 (mvc-11999) | 0.6866 | 0.720 | 2 |
CrO2 (mvc-11581) | 0.6240 | 0.166 | 2 |
VO2 (mp-777469) | 0.6987 | 0.038 | 2 |
VO2 (mvc-6918) | 0.6279 | 0.095 | 2 |
MoO2 (mvc-6944) | 0.6366 | 0.281 | 2 |
MnFeCo(PO4)3 (mp-764410) | 0.2265 | 0.028 | 5 |
MnFeCo(PO4)3 (mp-764392) | 0.2594 | 0.029 | 5 |
MnFeCo(PO4)3 (mp-763496) | 0.2384 | 0.028 | 5 |
MnFeCo(PO4)3 (mp-764415) | 0.2285 | 0.300 | 5 |
MnFeCo(PO4)3 (mp-763446) | 0.3139 | 0.333 | 5 |
Li4Mn3CrCo2(PO4)6 (mp-763479) | 0.7469 | 0.080 | 6 |
LiMgCr3Se2(SO6)4 (mp-769552) | 0.6233 | 0.257 | 6 |
Li2Mg2MnFe(PO4)4 (mp-849669) | 0.6720 | 0.008 | 6 |
NaLiMn2Fe4(PO4)6 (mp-777193) | 0.6845 | 0.018 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesCo: 3.32 eVNi: 6.2 eV |
PseudopotentialsVASP PAW: Co Ni_pv P O |
Final Energy/Atom-6.5776 eV |
Corrected Energy-176.8857 eV
-176.8857 eV = -157.8630 eV (uncorrected energy) - 11.2366 eV (MP Anion Correction) - 7.7860 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)