Final Magnetic Moment2.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-3.038 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.056 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.68 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi2VSiO5 + SiO2 |
Band Gap1.792 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinImma [74] |
Hall-I 2b 2 |
Point Groupmmm |
Crystal Systemorthorhombic |
sign indicates spin ↑ ↓
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <1 1 0> | 188.3 |
GaAs (mp-2534) | <1 1 0> | <0 1 0> | 234.7 |
SiO2 (mp-6930) | <1 0 0> | <1 0 1> | 167.5 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 318.8 |
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 159.4 |
DyScO3 (mp-31120) | <1 0 0> | <0 1 0> | 234.7 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 318.8 |
ZnSe (mp-1190) | <1 1 0> | <0 1 0> | 234.7 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 1> | 167.5 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 318.8 |
LiF (mp-1138) | <1 1 0> | <0 1 1> | 141.9 |
YVO4 (mp-19133) | <1 1 0> | <0 0 1> | 318.8 |
YVO4 (mp-19133) | <1 1 1> | <1 0 1> | 167.5 |
Ag (mp-124) | <1 1 0> | <1 0 0> | 147.3 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 239.1 |
LiNbO3 (mp-3731) | <1 0 1> | <0 1 0> | 234.7 |
SiC (mp-7631) | <1 0 0> | <0 0 1> | 318.8 |
C (mp-66) | <1 0 0> | <0 0 1> | 318.8 |
GdScO3 (mp-5690) | <1 0 0> | <0 1 1> | 141.9 |
LaF3 (mp-905) | <1 1 0> | <1 1 0> | 188.3 |
TbScO3 (mp-31119) | <1 0 0> | <0 1 1> | 141.9 |
Ni (mp-23) | <1 0 0> | <1 0 0> | 147.3 |
BaTiO3 (mp-5986) | <1 0 0> | <0 0 1> | 239.1 |
NdGaO3 (mp-3196) | <1 1 1> | <0 1 1> | 141.9 |
SiC (mp-11714) | <1 0 0> | <0 0 1> | 159.4 |
SiC (mp-11714) | <1 1 0> | <0 0 1> | 159.4 |
Au (mp-81) | <1 1 1> | <0 0 1> | 239.1 |
WS2 (mp-224) | <1 0 1> | <0 1 0> | 234.7 |
BN (mp-984) | <1 1 1> | <0 1 0> | 234.7 |
C (mp-48) | <1 1 1> | <0 1 0> | 234.7 |
WSe2 (mp-1821) | <1 0 0> | <1 0 0> | 147.3 |
Al (mp-134) | <1 1 1> | <1 0 1> | 167.5 |
ZrO2 (mp-2858) | <1 0 -1> | <0 0 1> | 318.8 |
Ge(Bi3O5)4 (mp-23352) | <1 1 0> | <1 0 0> | 147.3 |
LiGaO2 (mp-5854) | <0 0 1> | <1 0 1> | 167.5 |
LiTaO3 (mp-3666) | <1 0 1> | <0 1 0> | 234.7 |
CdWO4 (mp-19387) | <0 0 1> | <0 0 1> | 239.1 |
CdWO4 (mp-19387) | <1 0 1> | <0 0 1> | 318.8 |
TiO2 (mp-390) | <1 1 0> | <0 0 1> | 159.4 |
TiO2 (mp-390) | <1 1 1> | <0 0 1> | 159.4 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 318.8 |
GdScO3 (mp-5690) | <0 1 1> | <1 0 1> | 167.5 |
GdScO3 (mp-5690) | <1 1 0> | <0 0 1> | 318.8 |
TbScO3 (mp-31119) | <1 1 0> | <0 0 1> | 318.8 |
Ni (mp-23) | <1 1 0> | <0 0 1> | 239.1 |
NdGaO3 (mp-3196) | <1 0 0> | <0 0 1> | 318.8 |
NdGaO3 (mp-3196) | <1 1 0> | <0 0 1> | 318.8 |
Ga2O3 (mp-886) | <1 0 1> | <0 0 1> | 318.8 |
Au (mp-81) | <1 1 0> | <1 0 0> | 147.3 |
C (mp-48) | <1 1 0> | <0 1 0> | 234.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li2Cr(Si2O5)3 (mp-775340) | 0.2799 | 0.077 | 4 |
Li2Cr(PO3)5 (mp-704942) | 0.4657 | 0.044 | 4 |
LiSb3(P3O10)2 (mp-762248) | 0.4450 | 0.097 | 4 |
Li2Mn3P9O28 (mp-763668) | 0.4273 | 0.053 | 4 |
LiP2WO8 (mp-765954) | 0.4355 | 0.063 | 4 |
Cr19O48 (mp-850874) | 0.6814 | 0.095 | 2 |
Si2TeO7 (mvc-4099) | 0.5411 | 0.292 | 3 |
In2P2O7 (mp-17100) | 0.5518 | 0.000 | 3 |
Cr3(PO4)4 (mp-695952) | 0.5310 | 0.089 | 3 |
Mn3(PO4)4 (mp-697730) | 0.5634 | 0.092 | 3 |
Ni(PO3)3 (mp-699315) | 0.5435 | 0.071 | 3 |
KNa2Y(Si2O5)3 (mp-555155) | 0.5048 | 0.000 | 5 |
Na2AlB(As2O7)2 (mp-556195) | 0.5514 | 0.000 | 5 |
LiVCr(P2O7)2 (mp-765163) | 0.5716 | 0.009 | 5 |
LiVFe(P2O7)2 (mp-767272) | 0.5144 | 0.009 | 5 |
LiVCr(P2O7)2 (mp-767608) | 0.5151 | 0.009 | 5 |
CsAlBP2HO9 (mp-542129) | 0.7099 | 0.000 | 6 |
Li2MgCr3Se3(SO8)3 (mp-773983) | 0.6190 | 0.040 | 6 |
LiMgCr3Se2(SO6)4 (mp-769552) | 0.5972 | 0.001 | 6 |
NaInBP2HO9 (mp-757312) | 0.6902 | 0.013 | 6 |
RbAlBP2HO9 (mp-542130) | 0.6679 | 0.000 | 6 |
Ca2Al2FeSi4BHO16 (mp-540713) | 0.7106 | 0.002 | 7 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-points16 |
U ValuesV: 3.25 eV |
PseudopotentialsVASP PAW: Li_sv V_pv Si O |
Final Energy/Atom-7.5072 eV |
Corrected Energy-384.7789 eV
-384.7789 eV = -360.3462 eV (uncorrected energy) - 21.0687 eV (MP Anion Correction) - 3.3640 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)