Final Magnetic Moment22.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-1.845 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.098 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.61 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToMn3TeO6 + Fe2TeO6 + Li2TeO4 + Fe2O3 + Li2TeO3 |
Band Gap0.864 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [1] |
HallP 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 102.3 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 238.8 |
AlN (mp-661) | <0 0 1> | <0 1 0> | 186.6 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 62.4 |
AlN (mp-661) | <1 0 1> | <1 -1 0> | 315.1 |
AlN (mp-661) | <1 1 0> | <0 1 0> | 186.6 |
AlN (mp-661) | <1 1 1> | <1 -1 0> | 315.1 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 238.8 |
GaAs (mp-2534) | <1 0 0> | <0 1 1> | 287.7 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 238.8 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 204.7 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 272.9 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 238.8 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 187.3 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 136.4 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 238.8 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 272.9 |
SiO2 (mp-6930) | <1 0 0> | <1 -1 0> | 189.0 |
SiO2 (mp-6930) | <1 1 1> | <0 1 -1> | 209.9 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 204.7 |
KCl (mp-23193) | <1 1 0> | <1 0 -1> | 278.3 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 -1> | 279.9 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 170.6 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 307.0 |
DyScO3 (mp-31120) | <1 1 1> | <1 1 0> | 215.1 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 272.9 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 272.9 |
ZnSe (mp-1190) | <1 0 0> | <0 1 1> | 287.7 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 238.8 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 0> | 311.1 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 249.8 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 238.8 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 249.8 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 68.2 |
Te2W (mp-22693) | <1 0 0> | <1 0 1> | 290.7 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 312.2 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 136.4 |
YVO4 (mp-19133) | <1 1 0> | <1 0 0> | 62.4 |
Te2Mo (mp-602) | <0 0 1> | <1 0 -1> | 208.7 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 170.6 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 249.8 |
Te2Mo (mp-602) | <1 0 0> | <1 -1 0> | 315.1 |
Te2Mo (mp-602) | <1 1 0> | <1 0 0> | 187.3 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 1 0> | 311.1 |
GaSe (mp-1943) | <0 0 1> | <1 1 0> | 215.1 |
BN (mp-984) | <0 0 1> | <1 0 1> | 290.7 |
BN (mp-984) | <1 0 0> | <0 0 1> | 204.7 |
BN (mp-984) | <1 1 0> | <0 1 0> | 311.1 |
BN (mp-984) | <1 1 1> | <1 0 0> | 312.2 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 238.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Mg(MoO2)2 (mvc-6124) | 0.3887 | 0.192 | 3 |
Na4Ti5O12 (mp-760184) | 0.3856 | 0.036 | 3 |
Ca(WO2)2 (mvc-10243) | 0.3768 | 0.329 | 3 |
CaMn2O4 (mvc-10378) | 0.2397 | 0.079 | 3 |
Ca(WO2)2 (mvc-10486) | 0.3953 | 0.384 | 3 |
Li4Nb3Fe5O16 (mp-770110) | 0.2886 | 0.077 | 4 |
Li4Co3Sb5O16 (mp-770677) | 0.2705 | 0.057 | 4 |
Li4Fe3Sb5O16 (mp-769870) | 0.2618 | 0.047 | 4 |
Li4Co5Te3O16 (mp-781593) | 0.1938 | 0.096 | 4 |
Li4Ni3Sb5O16 (mp-774248) | 0.2502 | 0.081 | 4 |
Si3N4 (mp-641539) | 0.6623 | 0.288 | 2 |
P4Ru (mp-27173) | 0.6661 | 0.000 | 2 |
Ge3N4 (mp-641541) | 0.6226 | 0.208 | 2 |
Fe23O32 (mp-776135) | 0.6709 | 0.107 | 2 |
Fe3O4 (mp-650112) | 0.6773 | 0.057 | 2 |
Li4Fe2Co3Sb3O16 (mp-764902) | 0.2605 | 0.079 | 5 |
Li4Mn2Co3Te3O16 (mp-767658) | 0.1784 | 0.085 | 5 |
Li4Nb3Fe2Ni3O16 (mp-764250) | 0.2227 | 0.092 | 5 |
Li4Nb2Cr3Cu3O16 (mp-775290) | 0.2702 | 0.056 | 5 |
Li4Mn3Sn3(TeO8)2 (mp-775506) | 0.2685 | 0.054 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eVFe: 5.3 eV |
PseudopotentialsVASP PAW: Li_sv Mn_pv Fe_pv Te O |
Final Energy/Atom-6.0297 eV |
Corrected Energy-191.6301 eV
-191.6301 eV = -168.8328 eV (uncorrected energy) - 11.5607 eV (MP Advanced Correction) - 11.2366 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)