Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.418 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.127 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.96 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToSi2Ru |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP4/mmm [123] |
Hall-P 4 2 |
Point Group4/mmm |
Crystal Systemtetragonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 1 0> | 150.5 |
LaAlO3 (mp-2920) | <1 0 0> | <1 0 0> | 136.8 |
LaAlO3 (mp-2920) | <1 0 1> | <1 1 0> | 150.5 |
LaAlO3 (mp-2920) | <1 1 1> | <1 1 1> | 253.5 |
AlN (mp-661) | <0 0 1> | <1 1 0> | 150.5 |
AlN (mp-661) | <1 0 0> | <1 0 1> | 138.6 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 107.8 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 106.4 |
AlN (mp-661) | <1 1 1> | <1 1 0> | 86.0 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 141.0 |
CeO2 (mp-20194) | <1 1 0> | <1 0 0> | 167.3 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 33.2 |
GaAs (mp-2534) | <1 1 0> | <1 0 1> | 138.6 |
GaAs (mp-2534) | <1 1 1> | <1 1 0> | 172.0 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 41.5 |
BaF2 (mp-1029) | <1 1 0> | <1 0 0> | 228.1 |
BaF2 (mp-1029) | <1 1 1> | <1 0 0> | 136.8 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 41.5 |
KCl (mp-23193) | <1 1 0> | <1 0 0> | 228.1 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 124.4 |
GaN (mp-804) | <1 0 0> | <1 1 0> | 86.0 |
GaN (mp-804) | <1 0 1> | <1 1 1> | 115.2 |
GaN (mp-804) | <1 1 0> | <1 1 0> | 86.0 |
GaN (mp-804) | <1 1 1> | <1 1 0> | 86.0 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 215.7 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 132.7 |
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 306.9 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 1> | 138.6 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 165.9 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 66.4 |
DyScO3 (mp-31120) | <1 1 1> | <1 0 0> | 288.9 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 174.2 |
SiO2 (mp-6930) | <1 0 0> | <1 1 1> | 115.2 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 240.5 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 190.8 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 207.4 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 74.6 |
InAs (mp-20305) | <1 1 0> | <1 0 1> | 52.0 |
InAs (mp-20305) | <1 1 1> | <1 0 1> | 259.8 |
ZnSe (mp-1190) | <1 1 1> | <1 1 0> | 172.0 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 82.9 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 33.2 |
ZnSe (mp-1190) | <1 1 0> | <1 0 1> | 138.6 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 16.6 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 1> | 69.3 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 124.4 |
CdS (mp-672) | <1 1 0> | <1 0 1> | 190.5 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 207.4 |
CdS (mp-672) | <1 0 1> | <1 0 0> | 136.8 |
CdS (mp-672) | <1 1 1> | <0 0 1> | 207.4 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
318 | 62 | 89 | 0 | 0 | 0 |
62 | 318 | 89 | 0 | 0 | 0 |
89 | 89 | 412 | 0 | 0 | 0 |
0 | 0 | 0 | 65 | 0 | 0 |
0 | 0 | 0 | 0 | 65 | 0 |
0 | 0 | 0 | 0 | 0 | 86 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
3.4 | -0.5 | -0.6 | 0 | 0 | 0 |
-0.5 | 3.4 | -0.6 | 0 | 0 | 0 |
-0.6 | -0.6 | 2.7 | 0 | 0 | 0 |
0 | 0 | 0 | 15.3 | 0 | 0 |
0 | 0 | 0 | 0 | 15.3 | 0 |
0 | 0 | 0 | 0 | 0 | 11.7 |
Shear Modulus GV97 GPa |
Bulk Modulus KV169 GPa |
Shear Modulus GR87 GPa |
Bulk Modulus KR166 GPa |
Shear Modulus GVRH92 GPa |
Bulk Modulus KVRH168 GPa |
Elastic Anisotropy0.59 |
Poisson's Ratio0.27 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
MnCoSb (mp-1018803) | 0.7187 | 0.046 | 3 |
FeSi2 (mp-20738) | 0.1658 | 0.059 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Si Ru_pv |
Final Energy/Atom-7.1246 eV |
Corrected Energy-21.3739 eV
-21.3739 eV = -21.3739 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)