Final Magnetic Moment15.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.135 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.045 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.20 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCoPO4 + Co(PO3)3 + P2W2O11 + O2 |
Band Gap0.135 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinR3 [146] |
HallR 3 |
Point Group3 |
Crystal Systemtrigonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 0 1> | 263.0 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 328.8 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 197.3 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 197.3 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 65.8 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 65.8 |
SiO2 (mp-6930) | <1 1 0> | <1 0 0> | 192.1 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 263.0 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 65.8 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 197.3 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 197.3 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 197.3 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 263.0 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 263.0 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 197.3 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 263.0 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 263.0 |
BN (mp-984) | <0 0 1> | <0 0 1> | 65.8 |
BN (mp-984) | <1 1 0> | <0 0 1> | 65.8 |
LiGaO2 (mp-5854) | <0 1 1> | <0 0 1> | 131.5 |
LiGaO2 (mp-5854) | <1 1 0> | <0 0 1> | 197.3 |
Al (mp-134) | <1 1 1> | <0 0 1> | 197.3 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 328.8 |
TiO2 (mp-2657) | <1 1 1> | <0 0 1> | 197.3 |
Ge3(BiO3)4 (mp-23560) | <1 1 1> | <0 0 1> | 197.3 |
C (mp-66) | <1 1 1> | <0 0 1> | 65.8 |
LaF3 (mp-905) | <1 0 0> | <0 0 1> | 328.8 |
PbS (mp-21276) | <1 0 0> | <0 0 1> | 328.8 |
PbS (mp-21276) | <1 1 0> | <0 0 1> | 263.0 |
PbS (mp-21276) | <1 1 1> | <0 0 1> | 65.8 |
Ni (mp-23) | <1 0 0> | <0 0 1> | 328.8 |
Ni (mp-23) | <1 1 0> | <0 0 1> | 263.0 |
Ni (mp-23) | <1 1 1> | <0 0 1> | 65.8 |
PbSe (mp-2201) | <1 0 0> | <0 0 1> | 197.3 |
PbSe (mp-2201) | <1 1 1> | <0 0 1> | 65.8 |
MoSe2 (mp-1634) | <1 1 0> | <0 0 1> | 263.0 |
Si (mp-149) | <1 1 0> | <0 0 1> | 328.8 |
Si (mp-149) | <1 1 1> | <0 0 1> | 197.3 |
Au (mp-81) | <1 1 1> | <0 0 1> | 263.0 |
CdSe (mp-2691) | <1 0 0> | <0 0 1> | 197.3 |
CdSe (mp-2691) | <1 1 0> | <0 0 1> | 263.0 |
CdSe (mp-2691) | <1 1 1> | <0 0 1> | 65.8 |
WSe2 (mp-1821) | <1 1 0> | <0 0 1> | 263.0 |
WSe2 (mp-1821) | <1 1 1> | <0 0 1> | 263.0 |
ZrO2 (mp-2858) | <0 1 1> | <0 0 1> | 197.3 |
CaCO3 (mp-3953) | <0 0 1> | <0 0 1> | 65.8 |
CaCO3 (mp-3953) | <1 0 0> | <0 0 1> | 263.0 |
YAlO3 (mp-3792) | <1 0 0> | <0 0 1> | 328.8 |
YAlO3 (mp-3792) | <1 1 0> | <0 0 1> | 328.8 |
SiC (mp-8062) | <1 0 0> | <1 0 0> | 192.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ti2(PO4)3 (mp-774537) | 0.1742 | 0.013 | 3 |
Mo2(PO4)3 (mp-32055) | 0.1731 | 0.013 | 3 |
V2(PO4)3 (mp-540480) | 0.1764 | 0.027 | 3 |
Cr2(PO4)3 (mp-540211) | 0.1543 | 0.061 | 3 |
V2(PO4)3 (mp-32469) | 0.0966 | 0.015 | 3 |
Nb3Co(PO4)6 (mp-772332) | 0.0759 | 0.000 | 4 |
MnNb3(PO4)6 (mp-775218) | 0.0831 | 0.046 | 4 |
Ti3P6WO24 (mp-775198) | 0.0562 | 0.000 | 4 |
Fe3P6WO24 (mp-775004) | 0.0607 | 0.225 | 4 |
Ti3Cr(PO4)6 (mp-774416) | 0.0835 | 0.051 | 4 |
Cr5O12 (mp-773920) | 0.3195 | 0.000 | 2 |
Mo4O11 (mp-622101) | 0.6373 | 0.018 | 2 |
Nb2O5 (mp-776896) | 0.6117 | 0.059 | 2 |
Mo4O11 (mp-565865) | 0.6621 | 0.026 | 2 |
V5O12 (mp-778252) | 0.3750 | 0.024 | 2 |
VCrP2(O4F)2 (mp-765139) | 0.4274 | 0.041 | 5 |
CaTi2Fe2(PO4)6 (mvc-11942) | 0.4829 | 0.210 | 5 |
CsZr2Al(PO4)4 (mp-1019720) | 0.4836 | 0.000 | 5 |
MnVP2(O4F)2 (mp-777435) | 0.4580 | 0.002 | 5 |
VFeP2(O4F)2 (mp-778349) | 0.4405 | 0.038 | 5 |
Zr12Si2Bi2P16PbO72 (mp-693759) | 0.6959 | 0.009 | 6 |
LiTi3MnCr(PO4)6 (mp-772224) | 0.6179 | 0.001 | 6 |
NaLiTiAl(PO4)3 (mp-776520) | 0.7121 | 0.023 | 6 |
Na2LiTi3Al(PO4)6 (mp-769074) | 0.6398 | 0.011 | 6 |
Na2LiTi3Al(PO4)6 (mp-769073) | 0.6379 | 0.014 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesCo: 3.32 eVW: 6.2 eV |
PseudopotentialsVASP PAW: Co P W_pv O |
Final Energy/Atom-6.8023 eV |
Corrected Energy-258.1049 eV
-258.1049 eV = -231.2769 eV (uncorrected energy) - 16.8550 eV (MP Anion Correction) - 9.9730 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)